Study on the reversible capacity loss of layered oxide cathode during low-temperature operation
Source abstract
Abstract
In this study, commercial Li(Ni1/3Co1/3Mn1/3)O2/graphite (NCM/C) lithium-ion batteries were cycled at −10 °C under different current rates ranging from 0.2 C to 1C. Electrochemical measurements and post-mortem analysis were performed to identify the root causes of the degradation in the electrochemical performance of the cells. The results reveal that apart from the increase of lithium plating on the anode, there is a considerable and abnormal capacity loss on the NCM cathode with the increase in current rate. The different degradation mechanisms including the loss of lithium inventory (LLI) and the specific capacity loss of NCM material (LAM) during cycling at −10 °C were analyzed quantitatively. It is shown that the evolution trend of LLI with the increase in current rate (8.6%, 35.0%, 55.8% for 0.2 C, 0.5 C and 1 C respectively) corresponds closely to that of the capacity loss of the full-cells (8.6%, 45.5%, 63.6% for 0.2 C, 0.5 C and 1 C, respectively), which is different to the trend of LAM (7.2%, 8.8%, 22.3% for 0.2 C, 0.5 C and 1 C, respectively). Further analysis by XRD and HR-TEM clearly indicates that the crystallinity of the hexagonal layered structure of NCM was greatly impaired after low-temperature cycling at −10 °C, and spinel phase can be observed among the layered structure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Palacin · Science · 2016 · 351 · 125329210.1126/science.1253292 ↗
2. Jaguemont · Appl. Energ · 2016 · 164 · 9910.1016/j.apenergy.2015.11.034 ↗
3. Sides · Adv. Mater. · 2005 · 17 · 12510.1002/adma.200400517 ↗
4. Senyshyn · J. Power Sources · 2015 · 282 · 23510.1016/j.jpowsour.2015.02.008 ↗
5. Smart · J. Electrochem. Soc. · 2010 · 157 · 136110.1149/1.3501236 ↗
6. Waldmann · J. Power Sources · 2014 · 262 · 12910.1016/j.jpowsour.2014.03.112 ↗
7. Broussely · J. Power Sources · 2005 · 146 · 9010.1016/j.jpowsour.2005.03.172 ↗
8. Vetter · J. Power Sources · 2005 · 147 · 26910.1016/j.jpowsour.2005.01.006 ↗
9. Suresh · J. Appl. Electrochem. · 2002 · 32 · 26710.1023/A:1015565404343 ↗
10. Zhang · Electrochim. Acta · 2002 · 48 · 24110.1016/S0013-4686(02)00620-5 ↗
11. Li · J. Power Sources · 2015 · 281 · 6910.1016/j.jpowsour.2015.01.173 ↗
12. Zhang · Electrochem. Commun. · 2002 · 4 · 92810.1016/S1388-2481(02)00490-3 ↗
13. Yaqub · J. Mater. Sci. · 2014 · 49 · 770710.1007/s10853-014-8479-6 ↗
14. Harris · Chem. Phys. Lett. · 2010 · 485 · 26510.1016/j.cplett.2009.12.033 ↗
15. Iriyama · J. Electrochem. Soc. · 2006 · 153 · 82110.1149/1.2178647 ↗
16. Monroe · J. Electrochem. Soc. · 2003 · 150 · 137710.1149/1.1606686 ↗
17. Monroe · J. Electrochem. Soc. · 2004 · 151 · 88010.1149/1.1710893 ↗
18. Rosso · Electrochim. Acta · 2006 · 51 · 533410.1016/j.electacta.2006.02.004 ↗
19. Plichta · J. Power Sources · 2001 · 94 · 16010.1016/S0378-7753(00)00578-4 ↗
20. Agubra · Materials · 2013 · 6 · 131010.3390/ma6041310 ↗
21. Gunawardhana · Electrochem. Commun. · 2011 · 13 · 111610.1016/j.elecom.2011.07.014 ↗
22. Smart · J. Electrochem. Soc. · 2011 · 158 · 37910.1149/1.3544439 ↗
23. Birkenmaier · J. Electrochem. Soc. · 2015 · 162 · 264610.1149/2.0451514jes ↗
24. Uhlmann · J. Power Sources · 2015 · 279 · 42810.1016/j.jpowsour.2015.01.046 ↗
25. Zhang · Electrochim. Acta · 2004 · 49 · 105710.1016/j.electacta.2003.10.016 ↗
26. Legrand · J. Power Sources · 2014 · 245 · 20810.1016/j.jpowsour.2013.06.130 ↗
27. Petzl · J. Power Sources · 2015 · 275 · 79910.1016/j.jpowsour.2014.11.065 ↗
28. Petzl · J. Power Sources · 2014 · 254 · 8010.1016/j.jpowsour.2013.12.060 ↗
29. Tippmann · J. Power Sources · 2014 · 252 · 30510.1016/j.jpowsour.2013.12.022 ↗
30. Smart · J. Power Sources · 2003 · 119–121 · 34910.1016/S0378-7753(03)00154-X ↗
31. Plichta · J. Power Sources · 2000 · 88 · 19210.1016/S0378-7753(00)00367-0 ↗
32. Shiao · J. Power Sources · 2000 · 87 · 16710.1016/S0378-7753(99)00470-X ↗
33. Ji · J. Electrochem. Soc. · 2013 · 160 · 63610.1149/2.047304jes ↗
34. Dubarry · J. Power Sources · 2011 · 196 · 1033610.1016/j.jpowsour.2011.08.078 ↗
35. Dubarry · J. Power Sources · 2009 · 194 · 54110.1016/j.jpowsour.2009.05.036 ↗
36. Dubarry · J. Power Sources · 2011 · 196 · 1032810.1016/j.jpowsour.2011.08.077 ↗
37. Dubarry · J. Power Sources · 2011 · 196 · 342010.1016/j.jpowsour.2010.07.029 ↗
38. Park · J. Power Sources · 2008 · 178 · 82610.1016/j.jpowsour.2007.08.034 ↗
39. Stiaszny · J. Power Sources · 2014 · 251 · 43910.1016/j.jpowsour.2013.11.080 ↗
40. Liu · J. Power Sources · 2014 · 261 · 28510.1016/j.jpowsour.2014.03.083 ↗
41. Ecker · J. Power Sources · 2014 · 248 · 83910.1016/j.jpowsour.2013.09.143 ↗
42. Han · J. Power Sources · 2014 · 251 · 3810.1016/j.jpowsour.2013.11.029 ↗
43. Liu · J. Power Sources · 2014 · 269 · 92010.1016/j.jpowsour.2014.07.051 ↗
44. Gomez · J. Power Sources · 2011 · 196 · 482610.1016/j.jpowsour.2010.12.107 ↗
45. Zhou · Solid State Ion. · 2013 · 249–250 · 13410.1016/j.ssi.2013.07.024 ↗
46. Li · ACS Appl. Mater. Interfaces · 2014 · 6 · 507510.1021/am500215b ↗
47. Zheng · J. Alloy Compd. · 2015 · 644 · 60710.1016/j.jallcom.2015.04.173 ↗
48. Hu · J. Power Sources · 2015 · 277 · 19310.1016/j.jpowsour.2014.12.015 ↗
49. Jung · Adv. Energy Mater. · 2014 · 4 · 130078710.1002/aenm.201300787 ↗
50. Reichert · J. Power Sources · 2013 · 239 · 4510.1016/j.jpowsour.2013.03.053 ↗
51. Hong · J. Mater. Chem. · 2010 · 20 · 1017910.1039/c0jm01971b ↗