journal article·2009-04

High-temperature mechanical properties of a glass sealant for solid oxide fuel cell

Hsiu-Tao Chang, Chih-Kuang Lin, Chien-Kuo Liu

Journal of Power Sources· Volume 189· Issue 2
Publisher page

Abstract

Abstract The high-temperature mechanical properties of a newly developed silicate-based glass sealant, designated as GC-9, have been studied for use in planar solid oxide fuel cell (pSOFC). Four-point bending tests were conducted at room temperature, 550 °C, 600 °C, 650 °C, 700 °C and 750 °C to investigate the variation of flexural strength, elastic modulus, and stress relaxation with temperature for the given glass sealant. Weibull statistic analysis was applied to describe the fracture strength data. The results indicated that the flexural strength was increased with temperature when the testing temperature was below the glass transition temperature (Tg, 668 °C). This was presumably caused by a crack healing effect taking place at high temperatures for glasses. However, with a further increase of temperature to a level higher than Tg, significant stress relaxation was observed to cause extremely large deformation without breaking the specimen. When the controlled displacement rate was increased by an order of magnitude, the stress relaxation effect at 750 °C became less effective. However, the mechanical stiffness of the given glass was significantly reduced at a temperature higher than Tg.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Advanced ceramic materials synthesis · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Eichler · J. Eur. Ceram. Soc. · 1999 · 19 · 110110.1016/S0955-2219(98)00382-3 ↗
2. Ley · J. Mater. Res. · 1996 · 11 · 148910.1557/JMR.1996.0185 ↗
3. Lara · J. Non-Cryst. Solids · 2004 · 348 · 14910.1016/j.jnoncrysol.2004.08.140 ↗
4. Meinhardt · J. Power Sources · 2008 · 182 · 18810.1016/j.jpowsour.2008.03.079 ↗
5. Lessing · J. Mater. Sci. · 2007 · 42 · 346510.1007/s10853-006-0409-9 ↗
6. Fergus · J. Power Sources · 2005 · 147 · 4610.1016/j.jpowsour.2005.05.002 ↗
7. Larsen · J. Mater. Sci. · 1998 · 33 · 249910.1023/A:1004332614379 ↗
8. Larsen · J. Non-Cryst. Solids · 1999 · 244 · 1610.1016/S0022-3093(98)00848-5 ↗
9. Lahl · J. Mater. Sci. · 2000 · 35 · 308910.1023/A:1004851418274 ↗
10. Sohn · J. Non-Cryst. Solids · 2001 · 282 · 22110.1016/S0022-3093(01)00344-1 ↗
11. Sohn · J. Non-Cryst. Solids · 2002 · 297 · 10310.1016/S0022-3093(01)01042-0 ↗
12. Zheng · J. Power Sources · 2004 · 128 · 16510.1016/j.jpowsour.2003.10.005 ↗
13. Sohn · J. Am. Ceram. Soc. · 2004 · 87 · 25410.1111/j.1551-2916.2004.00254.x ↗
14. Choi · Ceram. Eng. Sci. Proc. · 2005 · 26 · 27510.1002/9780470291221.ch33 ↗
15. Nguyen · J. Am. Ceram. Soc. · 2006 · 89 · 135810.1111/j.1551-2916.2005.00874.x ↗
16. Pascual · J. Power Sources · 2007 · 169 · 4010.1016/j.jpowsour.2007.01.040 ↗
17. Nielsen · J. Eur. Ceram. Soc. · 2007 · 27 · 181710.1016/j.jeurceramsoc.2006.05.046 ↗
18. Chou · J. Power Sources · 2007 · 168 · 42610.1016/j.jpowsour.2007.03.039 ↗
19. Chou · J. Power Sources · 2007 · 170 · 39510.1016/j.jpowsour.2007.03.060 ↗
20. Smeacetto · J. Eur. Ceram. Soc. · 2008 · 28 · 6110.1016/j.jeurceramsoc.2007.05.006 ↗
21. Haanappel · J. Power Sources · 2005 · 141 · 10210.1016/j.jpowsour.2004.08.053 ↗
22. Montross · Br. Ceram. Trans. · 2002 · 101 · 8510.1179/096797802225003956 ↗
23. Lin · J. Power Sources · 2007 · 164 · 23810.1016/j.jpowsour.2006.10.089 ↗
24. Yakabe · J. Power Sources · 2004 · 131 · 27810.1016/j.jpowsour.2003.12.057 ↗
25. Haanappel · J. Power Sources · 2005 · 150 · 8610.1016/j.jpowsour.2005.02.015 ↗
26. Chou · J. Power Sources · 2005 · 152 · 16810.1016/j.jpowsour.2005.03.213 ↗
27. Batfalsky · J. Power Sources · 2006 · 155 · 12810.1016/j.jpowsour.2005.05.046 ↗
28. Yang · J. Electrochem. Soc. · 2003 · 150 · A109510.1149/1.1590325 ↗
29. Yang · J. Mater. Eng. Perform. · 2004 · 13 · 32710.1361/10599490419298 ↗
30. Chou · J. Power Sources · 2006 · 157 · 26010.1016/j.jpowsour.2005.07.027 ↗
31. Choi · Mater. Sci. Eng. A · 2007 · 460–461 · 50910.1016/j.msea.2007.01.084 ↗
32. Liu · J. Power Sources · 2008 · 185 · 119310.1016/j.jpowsour.2008.07.017 ↗
33. Liu · 2007
34. Liu · 2007
35. Liu · 2008
36. ASTM Standard C1211 · 2005 · vol.15.01
37. Richerson · 1992
38. Hibbeler · 2004
39. Rouxel · J. Non-Cryst. Solids · 2000 · 271 · 22410.1016/S0022-3093(00)00109-5 ↗
40. Hrma · J. Non-Cryst. Solids · 1988 · 102 · 8810.1016/0022-3093(88)90116-0 ↗
41. Singh · Int. J. Appl. Ceram. Technol. · 2007 · 4 · 13410.1111/j.1744-7402.2007.02128.x ↗
42. Kese · J. Eur. Ceram. Soc. · 2006 · 26 · 101310.1016/j.jeurceramsoc.2004.12.018 ↗
43. Ono · Fatigue Fract. Eng. Mater. Struct. · 2007 · 30 · 110.1111/j.1460-2695.2006.01092.x ↗
44. Cassidy · J. Am. Ceram. Soc. · 1969 · 53 · 16110.1111/j.1151-2916.1970.tb12060.x ↗