Effects of precursor, synthesis time and synthesis temperature on the physical and electrochemical properties of Li(Ni1−x−yCoxMny)O2 cathode materials
Source abstract
Abstract
Abstract The effects of the synthesis temperature, the synthesis time and the nature of the transition-metal hydroxide precursors on the physical and electrochemical properties of Li(Ni 1− x − y Co x Mn y )O 2 synthesized using solid-state reactions are studied. Higher synthesis temperature results in larger primary and secondary particle sizes, a lower tap density and a broader secondary particle size distribution. Increase in reaction time improves the crystallinity and the cyclability. A smaller primary particle size of the precursor leads to a larger primary particle size of Li(Ni 1− x − y Co x Mn y )O 2 . Li(Ni 1− x − y Co x Mn y )O 2 with a better crystallinity, a well-defined layered structure and a better cation ordering exhibits a higher capacity, a better cycling performance and rate capability. The optimized synthesis conditions for precursors NCMOH111-α and NCMOH424-a is 950 °C for 12 h and 950 °C for 9 h, respectively. NCM111-α-950-12h delivers a discharge capacity of 165.5 mAh g −1 during the initial cycle at a rate of 0.1C with a columbic efficiency of 87%, a 3C rate capability of 91.25% and a 1C capacity retention rate of 98.25% after 40 cycles.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Extraction and Separation Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Chen · J. Power Sources · 2003 · 119–121 · 18410.1016/S0378-7753(03)00176-9 ↗
2. Ohzuku · Chem. Lett. · 2001 · 64210.1246/cl.2001.642 ↗
3. Koyama · J. Power Sources · 2003 · 119–121 · 64410.1016/S0378-7753(03)00194-0 ↗
4. Sun · Nat. Mater. · 2009 · 8 · 32010.1038/nmat2418 ↗
5. Patoux · Electrochem. Commun. · 2004 · 6 · 76710.1016/j.elecom.2004.05.024 ↗
6. Belharouak · J. Power Sources · 2003 · 123 · 24710.1016/S0378-7753(03)00529-9 ↗
7. Zhang · J. Power Sources · 2010 · 195 · 129210.1016/j.jpowsour.2009.09.029 ↗
8. Luo · J. Power Sources · 2006 · 158 · 65410.1016/j.jpowsour.2005.09.047 ↗
9. Deng · Electrochim. Acta · 2008 · 53 · 244110.1016/j.electacta.2007.10.025 ↗
10. Zhang · Electrochim. Acta · 2007 · 52 · 733710.1016/j.electacta.2007.06.015 ↗
11. Wu · Electrochim. Acta · 2012 · 75 · 39310.1016/j.electacta.2012.05.035 ↗
12. Dahn · Solid State Ionics · 1990 · 44 · 8710.1016/0167-2738(90)90049-W ↗
13. Reimers · Solid State Ionics · 1993 · 61 · 33510.1016/0167-2738(93)90401-N ↗
14. Moshtev · J. Power Sources · 1995 · 54 · 32910.1016/0378-7753(94)02094-J ↗
15. Yoshio · J. Power Sources · 1998 · 74 · 4610.1016/S0378-7753(98)00011-1 ↗
16. Wang · Solid State Ionics · 2004 · 175 · 23910.1016/j.ssi.2004.09.043 ↗
17. Kim · J. Electrochem. Soc. · 2003 · 150 · A53810.1149/1.1559063 ↗
18. Kim · Electrochim. Acta · 2004 · 49 · 93710.1016/j.electacta.2003.10.005 ↗
19. Hu · Chin. J. Nonferrous Met. · 2008 · 18 · 1721
20. Guo · Trans. Nonferrous Met. Soc. China · 2005 · 15 · 1185