journal article·2012-03

On the poisoning effect of O2 and N2 for the Zr0.9Ti0.1V2 hydrogen storage alloy

T.B. Zhang, X.W. Yang, J.S. Li, R. Hu, X.Y. Xue, H.Z. Fu

Publisher page

Abstract

Abstract Homogeneously annealed Zr 0.9 Ti 0.1 V 2 samples are firstly exposed to contamination gases of O 2 and N 2 for 30, 60 and 180 s at the ambient temperature, respectively. Hydrogen absorption properties are examined after poisoning and regeneration. The compositions and valence in the surface and sub-surface are investigated by X-ray photoelectron spectroscopy (XPS). The hydrogen absorption capacity of the alloy has been almost entirely degraded by the oxygen poisoning. After the regeneration, the oxygen-poisoned sample can hardly absorb hydrogen while the nitrogen-poisoned sample re-obtains the hydrogen absorption capacity with the value as 2.85 H A −1 (molar ratio of hydrogen to alloy). The activation temperature of the oxygen-poisoned sample is ∼100 K higher than the value of the un-poisoned one. With the help of ion etching, it is found the thickness of the passivated surface layer of the oxygen-poisoned sample was ∼58 nm. However, the thickness of the passivated surface layer of the un-poisoned sample is only ∼36 nm. That is the reason why the oxygen-poisoned sample cannot renew the hydrogen absorption capacity under the same regeneration conditions as in the un-poisoned one.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen Storage and Materials · Nuclear Materials and Properties · Fuel Cells and Related Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Block · J. Less-Common Met. · 1983 · 89 · 7710.1016/0022-5088(83)90251-5 ↗
2. Eisenberg · J. Less-Common Met. · 1983 · 89 · 5510.1016/0022-5088(83)90248-5 ↗
3. Goodell · J. Less-Common Met. · 1983 · 89 · 4510.1016/0022-5088(83)90247-3 ↗
4. Schweppe · J. Alloys Compd. · 1997 · 253–254 · 51110.1016/S0925-8388(96)03002-2 ↗
5. Sandrock · J. Less-Common Met. · 1980 · 73 · 16110.1016/0022-5088(80)90355-0 ↗
6. Sang · Chin. J. Rare Met. · 2001 · 25 · 178
7. Sang · J. Funct. Mater. · 1999 · 30 · 137
8. Hara · J. Nucl. Mater. · 2003 · 320 · 26510.1016/S0022-3115(03)00189-2 ↗
9. Sutara · Vacuum · 2001 · 61 · 13510.1016/S0042-207X(00)00469-3 ↗
10. Kandavel · Int. J. Hydrogen Energy · 2008 · 33 · 375410.1016/j.ijhydene.2008.04.042 ↗
11. Cui · Intermetallics · 2008 · 16 · 66210.1016/j.intermet.2008.02.009 ↗
12. Davidson · Int. J. Hydrogen Energy · 2001 · 26 · 21910.1016/S0360-3199(00)00069-0 ↗
13. Yang · Int. J. Hydrogen Energy · 2010 · 35 · 1198110.1016/j.ijhydene.2010.08.065 ↗
14. Reddy · J. Alloys Compd. · 2008 · 460 · 26810.1016/j.jallcom.2007.06.001 ↗
15. Cao · J. Power Sources · 2001 · 93 · 14110.1016/S0378-7753(00)00555-3 ↗
16. Park · J. Alloys Compd. · 1992 · 182 · 4310.1016/0925-8388(92)90572-Q ↗
17. Jain · Int. J. Hydrogen Energy · 2007 · 32 · 244510.1016/j.ijhydene.2006.12.005 ↗
18. Jurczyk · J. Alloys Compd. · 1999 · 285 · 25010.1016/S0925-8388(98)01045-7 ↗
19. Yang · Int. J. Hydrogen Energy · 2011 · 36 · 931810.1016/j.ijhydene.2011.05.009 ↗
20. Mani · J. Alloys Compd. · 2002 · 337 · 14810.1016/S0925-8388(01)01931-4 ↗
21. Li · J. Alloys Compd. · 2005 · 393 · 23110.1016/j.jallcom.2004.08.097 ↗
22. Wang · Rare Met. Mater. Eng. · 2011 · 40 · 487
23. Yang · Solid State Commun. · 2011 · 151 · 84210.1016/j.ssc.2011.03.017 ↗
24. Sutara · Vacuum · 2004 · 74 · 30510.1016/j.vacuum.2003.12.144 ↗
25. Matolin · Vacuum · 2003 · 71 · 31710.1016/S0042-207X(02)00756-X ↗
26. Sinha · J. Less-Common Met. · 1986 · 125 · 8510.1016/0022-5088(86)90082-2 ↗
27. Fabík · Surf. Sci. · 2004 · 566–568 · 124610.1016/j.susc.2004.06.138 ↗
28. Masek · J. Vac. Sci. Technol. A: Vac. Surf. Films · 2003 · 21 · 79710.1116/1.1562175 ↗
29. Matolín · Appl. Surf. Sci. · 2004 · 235 · 20210.1016/j.apsusc.2004.05.125 ↗
30. Li · Thin Solid Films · 2006 · 515 · 112110.1016/j.tsf.2006.07.052 ↗