Abstract
Silicon lithiation induces a high material expansion which leads to significant swelling and mechanical pressure at the anode and cell level. In this study, the effect of the various mechanical constrains on the swelling behaviour of pouch cell and cylindrical cell (18650) with high performance silicon carbon graphite (Si–C/G) anode material was evaluated. In case of 18650 cells, strain gauges were used to evaluate the strains and pressure generated from anode swelling during cycling process; in addition, individual cell components thickness change was captured at 8 different states of charge (SOC) during a cycle by in situ 3D imaging with X-Ray micro computed-tomography (voxel size 1.6 μm) combined with a specific image treatment. For bi-layer pouch cells, operando swelling was measured using an in-house high precision (<0.1 μm) compression set-up with simultaneous pressure and thickness recording as well as dynamic pressure regulation system. Combining these unique experimental techniques and the modelling of Si–C/G active material swelling in function of the SOC we were able to provide insights in porosity changes of anodes for the two cell formats.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Semiconductor materials and devices · Advancements in Semiconductor Devices and Circuit Design
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Performance and cost of materials for lithium-based rechargeable automotive batteries10.1038/s41560-018-0107-2 ↗
2. Lithium-ion batteries - current state of the art and anticipated developments
3. Si-alloy negative electrodes for Li-ion batteries10.1016/j.coelec.2018.02.002 ↗
4. Challenges and recent progress in the development of Si anodes for lithium-ion battery10.1002/aenm.201700715 ↗
5. Colossal reversible volume changes in lithium alloys10.1149/1.1388178 ↗
6. Reaction of Li with alloy thin films studied by in situ AFM
7. Volume, pressure and thickness evolution of Li-ion pouch cells with silicon-composite negative electrodes10.1149/2.1691712jes ↗
8. Operando pressure measurements reveal solid electrolyte interphase growth to rank Li-ion cell performance10.1016/j.joule.2018.12.009 ↗
9. Effects of mechanical compression on the aging and the expansion behavior of Si/C-Composite|NMC811 in different lithium-ion battery cell formats10.1149/2.1121915jes ↗
10. Analysis of the effect of applying external mechanical pressure on next generation silicon alloy lithium-ion cells10.1016/j.electacta.2019.03.138 ↗
11. Impact of electrochemical and mechanical interactions on lithium-ion battery performance investigated by operando dilatometry10.1016/j.jpowsour.2021.229457 ↗
12. Impact of silicon/graphite composite electrode porosity on the cycle life of 18650 lithium-ion cell10.1021/acsaem.0c01999 ↗
13. Quantifying microstructural dynamics and electrochemical activity of graphite and silicon-graphite lithium ion battery anodes10.1038/ncomms12909 ↗
14. In-situ X-ray tomographic study of the morphological changes of a Si/C paper anode for Li-ion batteries10.1016/j.jpowsour.2017.03.044 ↗
15. Strain-induced lithium losses in the solid electrolyte interphase on silicon electrodes10.1021/acsami.7b06647 ↗
16. Deformation and stress in electrode materials for Li-ion batteries10.1016/j.pmatsci.2014.02.001 ↗
17. Simultaneous operando measurements of the local temperature, state of charge, and strain inside a commercial lithium-ion battery pouch cell10.1149/2.1251807jes ↗
18. Dynamics of the morphological degradation of Si-based anodes for Li-ion batteries characterized by in situ synchrotron X-ray tomography10.1002/aenm.201803947 ↗
19. A facile and very effective method to enhance the mechanical strength and the cyclability of Si-based electrodes for Li-ion batteries10.1002/aenm.201701787 ↗
20. Fiji: an open-source platform for biological-image analysis10.1038/nmeth.2019 ↗
21. Phase diagram of Li„C610.1103/PhysRevB.44.9170 ↗
22. Study of lithiation mechanisms in silicon electrodes by Auger Electron Spectroscopy10.1039/c3ta10212b ↗
23. Reversible cycling of crystalline silicon powder10.1149/1.2402112 ↗
24. Structural changes in silicon anodes during lithium insertion/extraction10.1149/1.1652421 ↗
25. Multiscale multiphase lithiation and delithiation mechanisms in a composite electrode unraveled by simultaneous operando small-angle and wide-angle X-ray scattering10.1021/acsnano.9b05055 ↗
26. Operando quantification of (De)Lithiation behavior of silicon–graphite blended electrodes for lithium-ion batteries10.1002/aenm.201803380 ↗
27. Study of the influence of mechanical pressure on the performance and aging of Lithium-ion battery cells10.1016/j.jpowsour.2019.227148 ↗
28. Comparison of the structural and electrochemical properties of layered Li[NixCoyMnz]O2 (x = 1/3, 0.5, 0.6, 0.7, 0.8 and 0.85) cathode material for lithium-ion batteries10.1016/j.jpowsour.2013.01.063 ↗
29. Oxygen release and its effect on the cycling stability of LiNixMnyCozO2 (NMC) cathode materials for Li-ion batteries10.1149/2.0021707jes ↗
30. In situ XRD and electrochemical study of the reaction of lithium with amorphous silicon10.1149/1.1739217 ↗
31. Between Scylla and charybdis: balancing among structural stability and energy density of layered NCM cathode materials for advanced lithium-ion batteries10.1021/acs.jpcc.7b06363 ↗
32. Solid electrolyte interphase on native oxide-terminated silicon anodes for Li-ion batteries10.1016/j.joule.2018.12.013 ↗
33. Comparing anode and cathode electrode/electrolyte interface composition and morphology using soft and hard X-ray photoelectron spectroscopy10.1016/j.electacta.2013.03.010 ↗
34. Electrochemical SPM investigation of the solid electrolyte interphase film formed on Hopg electrodes10.1016/S1388-2481(00)00056-4 ↗
35. Evaluating the solid electrolyte interphase formed on silicon electrodes: a comparison of ex situ X-ray photoelectron spectroscopy and in situ neutron reflectometry10.1039/C6CP00978F ↗
36. Monitoring the morphological changes of Si-based electrodes by X-ray computed tomography: a 4D-multiscale approach
37. In situ investigation of the volume change in Li-ion cell with charging and discharging: satellite power applications10.1149/1.1635827 ↗
38. High-precision monitoring of volume change of commercial lithium-ion batteries by using strain gauges10.3390/su12020557 ↗
39. The development of jelly roll deformation in 18650 lithium-ion batteries at low state of charge10.1149/1945-7111/aba96d ↗
40. An innovative process for ultra‐thick electrodes elaboration: toward low‐cost and high‐energy batteries10.1002/ente.201900025 ↗
41. Modeling charge polarization voltage for large lithium-ion batteries in electric vehicles
42. Real-time stress measurements in lithium-ion battery negative-electrodes10.1016/j.jpowsour.2012.01.036 ↗
43. Electrochemical-mechanical coupled modeling and parameterization of swelling and ionic transport in lithium-ion batteries10.1016/j.jpowsour.2017.12.044 ↗
44. A mechanical aging mechanism in lithium-ion batteries10.1149/2.1001410jes ↗
45. Probing lithium-ion batteries' state-of-charge using ultrasonic transmission – concept and laboratory testing10.1016/j.jpowsour.2017.01.090 ↗