journal article·2023-01

Flash sintering with concurrent crystallization of Li1.5Al0.5Ge1.5(PO4)3 glass

João V. Campos, Isabela R. Lavagnini, Vinicius M. Zallocco, Eduardo B. Ferreira, Eliria M.J.A. Pallone, Ana C.M. Rodrigues

Acta Materialia· Volume 244
Publisher page

Abstract

Single-phase Li 1.5Al 0.5Ge 1.5(PO 4) 3 NaSICON (Na superionic conductor) glass-ceramic is obtained via a new route using flash-sinter crystallization. Green compacts of glass powder are sinter-crystallized in a few seconds. The results suggest that controlling the current increase during the flash event is needed to avoid overheating, which could cause the melting of the samples. A processing map for the flash sinter-crystallization of Li 1.5Al 0.5Ge 1.5(PO 4) 3 is developed and presented based on the current density and holding time at the steady state. The samples fabricated by flash sinter-crystallization are compared with those conventionally heated. Using this novel technique, single-phase glass-ceramics are obtained with total ionic conductivity at room temperature surpassing that of glass-ceramics prepared by conventional heating (2.26 10 −4 S cm −1 and 1.36 10 −4 S cm −1, respectively).
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Microwave Dielectric Ceramics Synthesis · Advancements in Battery Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (67)

Show source-provided references
1. Origin of fast ion diffusion in superionic conductors10.1038/ncomms15893 ↗
2. First principles study on electrochemical and chemical stability of solid electrolyte–electrode interfaces in all-solid-state Li-ion batteries10.1039/C5TA08574H ↗
3. Promises and Challenges of Next-Generation "beyond Li-ion" Batteries for Electric Vehicles and Grid Decarbonization10.1021/acs.chemrev.0c00767 ↗
4. Progress and prospective of solid-state lithium batteries10.1016/j.actamat.2012.10.034 ↗
5. Stable LATP/LAGP double-layer solid electrolyte prepared via a simple dry-pressing method for solid state lithium ion batteries10.1039/C6RA19415J ↗
6. Methods for Lithium Ion NASICON Preparation: From Solid-State Synthesis to Highly Conductive Glass-Ceramics10.1021/acs.jpcc.0c07385 ↗
7. Synthesis and Properties of NaSICON-type LATP and LAGP Solid Electrolytes10.1002/cssc.201900725 ↗
8. Correlation between micro-structural properties and ionic conductivity of Li1.5Al0.5Ge1.5(PO4)3 ceramics10.1016/j.jpowsour.2011.03.065 ↗
9. Solid state lithium ionic conducting thin film Li1.4Al 0.4Ge1.6(PO4)3 prepared by tape casting10.1016/j.jallcom.2013.12.100 ↗
10. Preparation and Electrochemical Properties of Li 1+x Al x Ge 2-x (PO 4) 3 Synthesized by a Sol-Gel Method10.1149/2.080207jes ↗
11. Preparation of Li1.5Al0.5Ge1.5(PO4)3 solid electrolytes via the co-precipitation method10.1080/21870764.2019.1693680 ↗
12. Determination of crystallization kinetics parameters of a Li1.5Al0.5Ge1.5(PO4)3 (LAGP) glass by differential scanning calorimetry10.1590/S1516-14392013005000055 ↗
13. Controlled crystallization and ionic conductivity of a nanostructured LiAlGePO4 glass–ceramic10.1016/j.jnoncrysol.2009.07.012 ↗
14. Glass-to-Crystal Transition in Li 1+ x Al x Ge 2– x (PO 4) 3 : Structural Aspects Studied by Solid State NMR10.1021/jp502265h ↗
15. Fast Li+ ion conducting glass-ceramics in the system Li2O-Al2O3-GeO2-P2O510.1016/S0167-2738(97)00434-7 ↗
16. A bright future for glass-ceramics
17. Updated definition of glass-ceramics10.1016/j.jnoncrysol.2018.01.033 ↗
18. Flash Sintering of Nanograin Zirconia in <5 s at 850°C10.1111/j.1551-2916.2010.04089.x ↗
19. Alternating current field flash sintering 99% relative density ZnO ceramics at room temperature10.1016/j.scriptamat.2019.09.026 ↗
20. Water-assisted flash sintering: Flashing ZnO at room temperature to achieve ∼ 98% density in seconds10.1016/j.scriptamat.2017.08.032 ↗
21. Densification of La0.6Sr0.4Co0.2Fe 0.8O3 ceramic by flash sintering at temperature less than 100°C10.1007/s10853-014-8357-2 ↗
22. Flash sintering of ZnO ceramics at 50 °C under an AC field10.1016/j.ceramint.2019.08.142 ↗
23. Modeling of the temperature distribution of flash sintered zirconia10.2109/jcersj2.119.144 ↗
24. Microstructural evolution of 3YSZ flash-sintered with current ramp control10.1111/jace.17037 ↗
25. Flash Sintering using Controlled Current Ramp10.1016/j.jeurceramsoc.2018.04.003 ↗
26. Flash sintering with current rate: A different approach
27. Electric field-assisted ultrafast synthesis of nanopowders: a novel and cost-efficient approach10.1039/C6RA18734J ↗
28. Beyond flash sintering: How the flash event could change ceramics and glass processing10.1016/j.scriptamat.2020.05.065 ↗
29. Reactive flash sintering of the entropy-stabilized oxide Mg0.2Ni0.2Co0.2Cu0.2Zn0.2O10.1016/j.scriptamat.2020.02.006 ↗
30. Reactive flash sintering of the complex oxide Li0.5La0.5TiO3 starting from an amorphous precursor powder10.1016/j.scriptamat.2019.09.037 ↗
31. Phase evolution during reactive flash sintering of Li6.25Al0.25La3Zr2O12 starting from a chemically prepared powder10.1016/j.jeurceramsoc.2021.02.054 ↗
32. On the synchronicity of flash sintering and phase transformation10.1111/jace.16335 ↗
33. Effects of powder dispersion on reactive flash sintering of 8 mol% yttria-stabilized zirconia and MgAl2O4 composites10.1016/j.scriptamat.2020.08.009 ↗
34. The influence of the processing parameters on the reactive flash sintering of ZrO 2 -CeO 2
35. Reactive flash sintering of ceramics: a review
36. Rapid synthesis of Li 4 Ti 5 O 12 as lithium-ion battery anode by reactive flash sintering10.1111/jace.18086 ↗
37. Viscous flow flash sintering of porous silica glass10.1016/j.jnoncrysol.2017.09.024 ↗
38. Electrode-dependent Joule heating in soda lime silicate glass during flash processes10.1016/j.scriptamat.2020.03.005 ↗
39. DC-electro softening in soda lime silicate glass: An electro-thermal analysis10.1016/j.scriptamat.2018.03.028 ↗
40. C. Mclaren, W. Heffner, R. Tessarollo, R. Raj, H. Jain, Electric field-induced softening of alkali silicate glasses, 184101 (2015) 1–6. 10.1063/1.4934945.10.1063/1.4934945 ↗
41. Development of highly inhomogeneous temperature profile within electrically heated alkali silicate glasses10.1038/s41598-019-39431-8 ↗
42. Solid-state field-assisted ion exchange of Ag in lithium aluminum silicate glass-ceramics: A superfast processing route toward stronger materials with antimicrobial properties10.1016/j.jeurceramsoc.2021.11.035 ↗
43. Lithium Ion-Conducting Glass-Ceramics of Li 1.5 Al 0.5 Ge 1.5 (PO 4) 3 -xLi 2 O (x=0.0-0.20) with Good Electrical and Electrochemical Properties10.1111/j.1551-2916.2007.01827.x ↗
44. Flash sintering of ionic conductors: The need of a reversible electrochemical reaction10.1016/j.jeurceramsoc.2015.12.005 ↗
45. Flash sintering of cationic conductive ceramics: A way to build multilayer systems10.1111/jace.17787 ↗
46. Development of an instrumented and automated flash sintering setup for enhanced process monitoring and parameter control10.1016/j.jeurceramsoc.2018.09.002 ↗
47. On the Arrhenius-like behavior of conductivity during flash sintering of 3 mol% yttria stabilized zirconia ceramics10.1016/j.scriptamat.2021.114093 ↗
48. Flash sintering with current rate: A different approach10.1111/jace.16037 ↗
49. Microstructure evaluation of 3YSZ sintered by Two-Step Flash Sintering10.1016/j.ceramint.2021.04.174 ↗
50. Thermophysical Properties of Lithium Aluminum Germanium Phosphate with Different Compositions10.1007/s10765-020-2607-0 ↗
51. Flash sintering scaling-up challenges: Influence of the sample size on the microstructure and onset temperature of the flash event10.1016/j.scriptamat.2020.04.022 ↗
52. A thermal perspective of flash sintering: The effect of AC current ramp rate on microstructure evolution10.1016/j.jeurceramsoc.2020.11.040 ↗
53. GSAS-II : the genesis of a modern open-source all purpose crystallography software package10.1107/S0021889813003531 ↗
54. Influence of the Field and the Current Limit on Flash Sintering at Isothermal Furnace Temperatures10.1111/jace.12472 ↗
55. Flash sintering of tricalcium phosphate (TCP) bioceramics10.1016/j.jeurceramsoc.2017.08.004 ↗
56. Modelling the particle contact influence on the Joule heating and temperature distribution during FLASH sintering10.1016/j.jeurceramsoc.2019.12.015 ↗
57. Flash sintering incubation kinetics10.1038/s41524-020-00359-7 ↗
58. Correlating Transport and Structural Properties in Li 1+ x Al x Ge 2– x (PO 4) 3 (LAGP) Prepared from Aqueous Solution10.1021/acsami.8b00842 ↗
59. Structural evolution of NASICON-type Li 1+x Al x Ge 2−x (PO 4) 3 using in situ synchrotron X-ray powder diffraction10.1039/C6TA00402D ↗
60. Flash sintering of ceramics10.1016/j.jeurceramsoc.2018.08.048 ↗
61. Viscosity and liquidus-based predictor of glass-forming ability of oxide glasses10.1111/jace.16732 ↗
62. Crystallization of glass-forming liquids: Maxima of nucleation, growth, and overall crystallization rates10.1016/j.jnoncrysol.2015.08.023 ↗
63. Electrochemical stability of a NASICON solid electrolyte from the lithium aluminum germanium phosphate (LAGP) series10.1016/j.ssi.2022.115888 ↗
64. Glass-ceramics in Li1+xAlxGe2-x(PO4)3 system: The effect of Al2O3 addition on microstructure, structure and electrical properties10.1016/j.jallcom.2020.155281 ↗
65. Lithium Ion Diffusion Mechanism and Associated Defect Behaviors in Crystalline Li 1+ x Al x Ge 2– x (PO 4) 3 Solid-State Electrolytes10.1021/acs.jpcc.9b08390 ↗
66. NMR studies of Li mobility in NASICON-type glass-ceramic ionic conductors with optimized microstructure10.1039/C8TA11686E ↗
67. High lithium ion conducting solid electrolytes based on NASICON Li 1+x Al x M 2−x (PO 4) 3 materials (M = Ti, Ge and 0 ≤ x ≤ 0.5)10.1016/j.jeurceramsoc.2014.11.023 ↗