Abstract

An understanding of the solid electrolyte interphase (SEI) that forms on the lithium-metal surface is essential to the further development of rechargeable lithium-metal batteries. Currently, the formation of dendrites during cycling, which can lead to catastrophic failure of the cell, has mostly halted research on these power sources. The discovery of ionic liquids as electrolytes has rekindled the possibility of safe, rechargeable, lithium-metal batteries. The current limitation of ionic liquid electrolytes, however, is that when compared with conventional non-aqueous electrolytes the device rate capability is limited. Recently, we have shown that the addition of a zwitterion such as N-methyl-N-(butyl sulfonate) pyrrolidinium resulted in enhancement of the achievable current densities by 100%. It was also found that the resistance of the SEI layer in the presence of a zwitterion is 50% lower. In this study, a detailed chemical and electrochemical analysis of the SEI that forms in both the presence and absence of a zwitterion has been conducted. Clear differences in the chemical nature and also the thickness of the SEI are observed and these may account for the enhancement of operating current densities.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Ionic liquids properties and applications · Advancements in Battery Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Munichandraiah · J. Power Sources · 1998 · 72 · 20310.1016/S0378-7753(97)02771-7 ↗
2. Yamaki · 1999 · 339
3. Brummer · 1980 · 123
4. Yamaki · J. Appl. Electrochem. · 1997 · 28 · 13510.1023/A:1003270406759 ↗
5. Peled · J. Electrochem. Soc. · 1979 · 126 · 204710.1149/1.2128859 ↗
6. Aurbach · J. Power Sources · 2000 · 89 · 20610.1016/S0378-7753(00)00431-6 ↗
7. Peled · 2003
8. Peled · 1999 · 419
9. Owen · Chem. Soc. Rev. · 1997 · 26 · 25910.1039/cs9972600259 ↗
10. Howlett · J. Power Sources · 2003 · 114 · 27710.1016/S0378-7753(02)00603-1 ↗
11. Shin · Electrochem. Commun. · 2003 · 5 · 101610.1016/j.elecom.2003.09.017 ↗
12. Sakaebe · Electrochem. Commun. · 2003 · 5 · 59410.1016/S1388-2481(03)00137-1 ↗
13. Katayama · Electrochemistry (Tokyo Jpn.) · 2003 · 71 · 103310.5796/electrochemistry.71.1033 ↗
14. Rogers · Science · 2003 · 302 · 79210.1126/science.1090313 ↗
15. Endres · 2003 · 289
16. Seddon · Nat. Mater. · 2003 · 2 · 36310.1038/nmat907 ↗
17. Carter · Chem. Commun. · 2004 · 6 · 63010.1039/b313068a ↗
18. Welton · Chem. Rev. · 1999 · 99 · 207110.1021/cr980032t ↗
19. Zein El Abedin · 2003
20. Howlett · Electrochem. Solid-State Lett. · 2004 · 7 · A9710.1149/1.1664051 ↗
21. Howlett · Z. Phys. Chem. (Muenchen, Germany) · 2006 · 220 · 148310.1524/zpch.2006.220.10.1483 ↗
22. Tiyapiboonchaiya · Nat. Mater. · 2004 · 3 · 2910.1038/nmat1044 ↗
23. Byrne · Adv. Mater. (Weinheim, Germany) · 2005 · 17 · 249710.1002/adma.200500595 ↗
24. Howlett · J. Electrochem. Soc. · 2006 · 153 · A59510.1149/1.2164726 ↗
25. Byrne · J. Mater. Chem. · 2004 · 14 · 12710.1039/b309358a ↗
26. Meyer · Electrochem. Solid-State Lett. · 2005 · 8 · A14510.1149/1.1854117 ↗
27. Eshkenazi · Solid State Ionics · 2004 · 170 · 8310.1016/S0167-2738(03)00107-3 ↗
28. Castriota · J. Phys. Chem. A · 2005 · 109 · 9210.1021/jp046030w ↗
29. MacFarlane · J. Phys. Chem. B. · 1999 · 103 · 416410.1021/jp984145s ↗