In situ and ex situ studies of anomalous eutectic formation in undercooled Ni–Sn alloys
Source abstract
Abstract
Abstract Anomalous eutectic formation in undercooled Ni–Sn alloys was investigated by in situ X-ray diffraction and ex situ remelting and annealing experiments. Dynamic recrystallization and partial remelting of primary solids followed by repeated nucleation and growth of eutectic grains in the mushy zone were revealed by time-resolved X-ray diffraction. Ex situ experiments demonstrated that partial remelting of near-equilibrium solidified alloys of eutectic or near-eutectic composition can convert regular lamellar eutectic into anomalous eutectic, whereas high-temperature annealing of splat-quenched alloys of similar composition can convert eutectic or two-phase dendrites into anomalous eutectic. It is concluded that compared to ripening in solid-states, partial remelting of eutectic or two-phase dendrites in a mushy zone provides a more realistic mechanism for anomalous eutectic formation in undercooled solidification of Ni–Sn eutectic alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Solidification and crystal growth phenomena · Shape Memory Alloy Transformations · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Undercooling in silver–copper eutectic alloys
2. Structure of undercooled Ni–Sn eutectic10.1007/BF02900268 ↗
3. Growth mechanisms in undercooled eutectics10.1007/BF02813283 ↗
4. High undercooling and rapid solidification of Ni–32.5% Sn eutectic alloy10.1016/0956-7151(91)90212-J ↗
5. Dendritic and eutectic solidification of undercooled Co–Sb alloys10.1016/0956-7151(93)90200-C ↗
6. Solidification of undercooled Ni32.5 wt% Sn eutectic alloy10.1007/BF00356210 ↗
7. Rapid solidification of undercooled eutectic and monotectic alloys10.1016/0921-5093(93)90244-9 ↗
8. Rapid dendritic and eutectic solidification of undercooled CoMo alloys10.1016/0921-5093(94)90821-4 ↗
9. Microtexture and macrotexture formation in the containerless solidification of undercooled Ni–18.7 at.% Sn eutectic melts10.1016/j.actamat.2004.10.029 ↗
10. Effect of undercooling on the microstructure of Ni–35 at. pct Mo (eutectic) and Ni–38 at. pct Mo (hypereutectic) alloys10.1007/BF02649470 ↗
11. Mechanism of formation of the anomalous eutectic structure in rapidly solidified Ni–Si, Co–Sb and Ni–Al–Ti alloys10.1016/S1359-6454(97)00339-X ↗
12. Structural evidence for the transition from coupled to decoupled growth in the solidification of undercooled Ni–Sn eutectic melt10.1007/s11661-007-9198-2 ↗
13. Mechanism of anomalous eutectic formation in the solidification of undercooled Ni–Sn eutectic alloy10.1557/JMR.2008.0259 ↗
14. New evidence for dual origin of anomalous eutectic structures in undercooled Ni–Sn alloys: in-situ observations and EBSD characterization10.1016/j.actamat.2011.03.016 ↗
15. The origin of anomalous eutectic structures in undercooled Ag–Cu alloy10.1016/j.actamat.2013.08.001 ↗
16. Remelting induced anomalous eutectic formation during solidification of deeply undercooled eutectic alloy melts10.1016/j.actamat.2015.05.014 ↗
17. Investigation of the origin of anomalous eutectic formation by remelting thin-gauge samples of an Ag–Cu eutectic alloy10.1016/j.scriptamat.2019.08.034 ↗
18. In situ observation of remelting induced anomalous eutectic structure formation in an undercooled Ni–18.7 at.% Sn eutectic alloy10.1016/j.scriptamat.2019.10.019 ↗
19. Microstructural characteristics of Ni–Sb eutectic alloys under substantial undercooling and containerless solidification conditions10.1007/s11661-002-0223-1 ↗
20. Phase selection and re-melting-induced anomalous eutectics in undercooled Ni–38 wt% Si alloys10.1007/s10853-016-0312-y ↗
21. Formation of anomalous eutectic microstructure in Au–Sn eutectic alloy prepared by melt mixing
22. Metastable solidification of hypereutectic Co2Si–CoSi composition: microstructural studies and in-situ observations10.1016/j.actamat.2017.09.037 ↗
23. High-energy synchrotron X-ray diffraction and its application to in situ structural phase-transition studies in complex sample environments10.1007/s11837-011-0218-8 ↗
24. On the metastable miscibility gap in liquid Cu–Cr alloys10.1007/s10853-009-3511-y ↗
25. In situ high-energy X-ray diffraction studies of melting, solidification and solid-state transformation of Ni3Sn10.1557/adv.2020.22 ↗
26. Structural evolution of undercooled Ni‒Cu alloys10.1016/S0022-0248(98)00399-6 ↗
27. Experimental study of grain refinement mechanism in undercooled Ni‒15at.% Cu alloy10.1557/JMR.2010.0257 ↗
28. Solid fraction in dendritic solidification of a liquid
29. Modeling of free eutectic growth and competitive solidification in undercooled near-eutectic alloys based on in situ measurements10.1007/s10853-014-8585-5 ↗
30. Herlach · 2007
31. Reexamination of the solidification behavior of undercooled Ni–Sn eutectic melts10.1016/S1359-6454(02)00146-5 ↗
32. Physical mechanism of grain refinement in solidification of undercooled melts10.1103/PhysRevLett.73.1380 ↗