Electrochemical properties of cross-linked polymer electrolyte by electron beam irradiation and application to lithium ion batteries
Source abstract
Abstract
Abstract A polymer electrolyte was successfully fabricated for a room temperature operation lithium battery by cross-linking the mixture of oligomeric poly (ethylene glycol) dimethylether (PEGDME) and poly (ethylene glycol) diacrylate (PEGDA) with Li(CF3SO2)2N using electron beam irradiation. The maximum ionic conductivity achieved for the cross-linked solid polymer electrolyte (c-SPE) at room temperature was 2.1 × 10−4 S cm−1 and the lithium transport number of the electrolyte was around 0.2. The c-SPE showed no reaction heat with lithium metal up to 300 °C. The interface resistance of Li/c-SPE/Li at room temperature was about 45 Ω cm2, which is considerable lower than that of 210 Ω cm2 for Li/PEO10Li(CF3SO2)2N/Li. The electrochemical window of the polymer electrolyte was above 4 V (versus Li+/Li). The initial discharge capacity for the Li/SPE/LiFePO4-C cell was approximately 90 mAh g−1 for LiFePO4-C at 1/10 °C rate at room temperature and showed a good cyclability and a high coulombic efficiency of 99.2%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Fenton · Polymer · 1973 · 14 · 58910.1016/0032-3861(73)90146-8 ↗
2. Berthier · Solid State Ionics · 1983 · 11 · 9110.1016/0167-2738(83)90068-1 ↗
3. Armand · 1979
4. Fan · J. Electrochem. Soc. · 1997 · 144 · 39910.1149/1.1837423 ↗
5. Abraham · Chem. Mater. · 1997 · 9 · 197810.1021/cm970075a ↗
6. Choi · Solid State Ionics · 2007 · 178 · 123510.1016/j.ssi.2007.06.006 ↗
7. Kang · J. Power Sources · 2001 · 92 · 25510.1016/S0378-7753(00)00546-2 ↗
8. Maccallum · Solid State Ionics · 1984 · 11 · 30710.1016/0167-2738(84)90022-5 ↗
9. Kronfli · Br. Polym. J. · 1988 · 20 · 27510.1002/pi.4980200319 ↗
10. Collier · Clin. Orthop. Relat. Res. · 2003 · 414 · 28910.1097/01.blo.0000073343.50837.03 ↗
11. Uchiyama · Solid State Ionics · 2009 · 180 · 20510.1016/j.ssi.2008.11.015 ↗
12. Hanai · J. Power Sources · 2008 · 178 · 78910.1016/j.jpowsour.2007.10.004 ↗
13. Evans · Polymer · 1987 · 28 · 232410.1016/0032-3861(87)90394-6 ↗
14. Appetecchi · J. Electrochem. Soc. · 1998 · 145 · 412610.1149/1.1838925 ↗
15. Li · Solid State Ionics · 2003 · 159 · 9710.1016/S0167-2738(03)00004-3 ↗
16. Liu · J. Electrochem. Soc. · 2010 · 157 · A109210.1149/1.3473790 ↗
17. Kim · Solid State Ionics · 2002 · 149 · 2910.1016/S0167-2738(02)00130-3 ↗