Micro-tubular solid oxide fuel cells with graded anodes fabricated with a phase inversion method

Ling Zhao, Xiaozhen Zhang, Beibei He, Beibei Liu, Changrong Xia

Journal of Power Sources· Volume 196· Issue 3
Publisher page

Abstract

Abstract Micro-tubular proton-conducting solid oxide fuel cells (SOFCs) are developed with thin film BaZr 0.1 Ce 0.7 Y 0.1 Yb 0.1 O 3− δ (BZCYYb) electrolytes supported on Ni-BZCYYb anodes. The substrates, NiO-BZCYYb hollow fibers, are prepared by an immersion induced phase inversion technique. The resulted fibers have a special asymmetrical structure consisting of a sponge-like layer and a finger-like porous layer, which is propitious to serving as the anode supports for micro-tubular SOFCs. The fibers are characterized in terms of porosity, mechanical strength, and electrical conductivity regarding their sintering temperatures. To make a single cell, a dense BZCYYb electrolyte membrane about 20 μm thick is deposited on the hollow fiber by a suspension-coating process and a porous Sm 0.5 Sr 0.5 CoO 3 (SSC)-BZCYYb cathode is subsequently fabricated by a slurry coating technique. The micro-tubular proton-conducting SOFC generates a peak power density of 254 mW cm −2 at 650 °C when humidified hydrogen is used as the fuel and ambient air as the oxidant.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Catalysis and Oxidation Reactions · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Steele · Nature · 2001 · 414 · 34510.1038/35104620 ↗
2. Huang · Science · 2006 · 312 · 25410.1126/science.1125877 ↗
3. Zhan · Science · 2005 · 308 · 84410.1126/science.1109213 ↗
4. Sammes · J. Power Sources · 2005 · 145 · 42810.1016/j.jpowsour.2005.01.079 ↗
5. Akkaya · Int. J. Energy Res. · 2007 · 31 · 7910.1002/er.1238 ↗
6. Jia · Environ. Energy Eng. · 2008 · 54 · 554
7. Singhal · 2003
8. Droushiotis · Solid State Ionics · 2009 · 180 · 109110.1016/j.ssi.2009.04.004 ↗
9. Funahashi · J. Power Sources · 2007 · 163 · 73110.1016/j.jpowsour.2006.10.002 ↗
10. Suzuki · J. Alloys Compd. · 2008 · 451 · 63210.1016/j.jallcom.2007.04.149 ↗
11. Yang · J. Power Sources · 2009 · 187 · 9010.1016/j.jpowsour.2008.10.069 ↗
12. Wei · J. Membr. Sci. · 2008 · 320 · 19110.1016/j.memsci.2008.04.003 ↗
13. Jin · J. Membr. Sci. · 2009 · 341 · 23310.1016/j.memsci.2009.06.012 ↗
14. Yang · J. Power Sources · 2008 · 183 · 1410.1016/j.jpowsour.2008.05.006 ↗
15. Kreuer · Annu. Rev. Mater. Res. · 2003 · 33 · 33310.1146/annurev.matsci.33.022802.091825 ↗
16. Hirabayashi · Solid State Ionics · 2005 · 176 · 88110.1016/j.ssi.2004.12.007 ↗
17. Zhao · J. Power Sources · 2009 · 194 · 83510.1016/j.jpowsour.2009.06.010 ↗
18. Zhao · J. Power Sources · 2009 · 194 · 29110.1016/j.jpowsour.2009.05.001 ↗
19. Xia · Solid State Ionics · 2002 · 149 · 1110.1016/S0167-2738(02)00131-5 ↗
20. Yang · Adv. Mater. · 2008 · 20 · 328010.1002/adma.200702762 ↗
21. Tan · J. Membr. Sci. · 2007 · 302 · 10910.1016/j.memsci.2007.06.033 ↗
22. Blanco · J. Membr. Sci. · 2006 · 283 · 2710.1016/j.memsci.2006.06.011 ↗
23. Mok · J. Membr. Sci. · 1995 · 100 · 18310.1016/0376-7388(94)00134-K ↗
24. Droushiotis · Solid State Ionics · 2000 · 180 · 109110.1016/j.ssi.2009.04.004 ↗
25. Brown · J. Electrochem. Soc. · 2000 · 147 · 47510.1149/1.1393220 ↗
26. Roy · J. Power Sources · 2009 · 188 · 22010.1016/j.jpowsour.2008.11.076 ↗
27. Zhang · J. Alloys Compd. · 2010 · 494 · 36610.1016/j.jallcom.2010.01.048 ↗
28. Suzuki · Solid State Ionics · 2008 · 180 · 54610.1016/j.ssi.2008.09.023 ↗
29. Yang · J. Power Sources · 2010 · 195 · 47110.1016/j.jpowsour.2009.07.057 ↗
30. Yang · Science · 2009 · 326 · 12610.1126/science.1174811 ↗
31. Zhang · J. Power Sources · 2007 · 170 · 5510.1016/j.jpowsour.2007.03.080 ↗
32. Suzuki · Science · 2009 · 325 · 85210.1126/science.1176404 ↗