Eliminating micro-porous layer from gas diffusion electrode for use in high temperature polymer electrolyte membrane fuel cell
Source abstract
Abstract
Abstract In this work, we report a simple strategy to improve the performance of high temperature polymer electrolyte membrane fuel cell (HT-PEMFC) by eliminating the micro-porous layer (MPL) from its gas diffusion electrodes (GDEs). Due to the absence of liquid water and the general use of high amount of catalyst, the MPL in a HT-PEMFC system works limitedly. Contrarily, the elimination of the MPL leads to an interlaced micropore/macropore composited structure in the catalyst layer (CL), which favors gas transport and catalyst utilization, resulting in a greatly improved single cell performance. At the normal working voltage (0.6 V), the current density of the GDE eliminated MPL reaches 0.29 A cm−2, and a maximum power density of 0.54 W cm−2 at 0.36 V is obtained, which are comparable to the best results yet reported for the HT-PEMFCs with similar Pt loading and operated using air. Furthermore, the MPL-free GDE maintains an excellent durability during a preliminary 1400 h HT-PEMFC operation, owing to its structure advantages, indicating the feasibility of this electrode for practical applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced battery technologies research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Li · Prog. Polym. Sci. · 2009 · 34 · 44910.1016/j.progpolymsci.2008.12.003 ↗
2. Bose · Prog. Polym. Sci. · 2011 · 36 · 81310.1016/j.progpolymsci.2011.01.003 ↗
3. Quartarone · Energy Environ. Sci. · 2012 · 5 · 643610.1039/c2ee03055a ↗
4. Lobato · Appl. Catal. B · 2009 · 91 · 26910.1016/j.apcatb.2009.05.035 ↗
5. Orfanidi · Appl. Catal. B · 2011 · 106 · 37910.1016/j.apcatb.2011.05.043 ↗
6. Stassi · Appl. Catal. B · 2013 · 142–143 · 1510.1016/j.apcatb.2013.05.008 ↗
7. Kaserer · J. Phys. Chem. C · 2013 · 117 · 621010.1021/jp311924q ↗
8. Stephens · Energy Environ. Sci. · 2012 · 5 · 674410.1039/c2ee03590a ↗
9. Su · J. Power Sources · 2014 · 246 · 6310.1016/j.jpowsour.2013.07.062 ↗
10. Su · Int. J. Hydrogen Energy · 2013 · 38 · 1137010.1016/j.ijhydene.2013.06.107 ↗
11. Su · J. Power Sources · 2013 · 242 · 51010.1016/j.jpowsour.2013.05.128 ↗
12. He · Nano Energy · 2012 · 1 · 82810.1016/j.nanoen.2012.06.003 ↗
13. Chun · Renew. Energy · 2012 · 48 · 3510.1016/j.renene.2012.04.011 ↗
14. Chun · Int. J. Hydrogen Energy · 2010 · 35 · 1114810.1016/j.ijhydene.2010.07.056 ↗
15. Chun · Int. J. Hydrogen Energy · 2011 · 36 · 842210.1016/j.ijhydene.2011.04.038 ↗
16. Cindrella · J. Power Sources · 2009 · 194 · 14610.1016/j.jpowsour.2009.04.005 ↗
17. Ji · J. Electrochem. Soc. · 2010 · 157 · B175310.1149/1.3491359 ↗
18. Kim · Int. J. Hydrogen Energy · 2010 · 35 · 863110.1016/j.ijhydene.2010.05.123 ↗
19. Latorrata · Solid State Ionics · 2012 · 216 · 7310.1016/j.ssi.2012.03.030 ↗
20. Maidhily · Int. J. Hydrogen Energy · 2011 · 36 · 1235210.1016/j.ijhydene.2011.06.084 ↗
21. Park · J. Power Sources · 2006 · 163 · 35710.1016/j.jpowsour.2006.09.020 ↗
22. Park · J. Power Sources · 2008 · 177 · 45710.1016/j.jpowsour.2007.11.055 ↗
23. Pasaogullari · Electrochim. Acta · 2004 · 49 · 435910.1016/j.electacta.2004.04.027 ↗
24. Ramasamy · Int. J. Hydrogen Energy · 2008 · 33 · 335110.1016/j.ijhydene.2008.03.053 ↗
25. Tang · J. Power Sources · 2007 · 166 · 4110.1016/j.jpowsour.2007.01.021 ↗
26. Wang · J. Power Sources · 2006 · 162 · 47410.1016/j.jpowsour.2006.06.064 ↗
27. Wang · Electrochim. Acta · 2006 · 51 · 490910.1016/j.electacta.2006.01.048 ↗
28. Weng · Int. J. Hydrogen Energy · 2011 · 36 · 1370810.1016/j.ijhydene.2011.07.141 ↗
29. Wu · Int. J. Hydrogen Energy · 2010 · 35 · 758810.1016/j.ijhydene.2010.04.126 ↗
30. Lobato · J. Appl. Electrochem. · 2008 · 38 · 79310.1007/s10800-008-9512-8 ↗
31. Lobato · Fuel Cells · 2010 · 10 · 77010.1002/fuce.200900175 ↗
32. Kongstein · Energy · 2007 · 32 · 41810.1016/j.energy.2006.07.009 ↗
33. Seland · J. Power Sources · 2006 · 160 · 2710.1016/j.jpowsour.2006.01.047 ↗
34. Schmidt · J. Power Sources · 2008 · 176 · 42810.1016/j.jpowsour.2007.08.055 ↗
35. Hsueh · J. Electrochem. Soc. · 1984 · 131 · 82310.1149/1.2115707 ↗
36. Holst-Olesen · J. Power Sources · 2014 · 272 · 107210.1016/j.jpowsour.2014.09.035 ↗
37. Su · Electrocatalysis · 2014 · 5 · 36110.1007/s12678-014-0202-5 ↗
38. Millington · J. Power Sources · 2011 · 196 · 850010.1016/j.jpowsour.2011.06.024 ↗
39. Uchida · J. Electrochem. Soc. · 1995 · 142 · 414310.1149/1.2048477 ↗
40. Kim · Nat. Commun. · 2013 · 4 · 247310.1038/ncomms3473 ↗
41. Lee · J. Power Sources · 2004 · 131 · 20010.1016/j.jpowsour.2003.12.039 ↗
42. Zhang · J. Power Sources · 2007 · 172 · 16310.1016/j.jpowsour.2007.07.047 ↗
43. Yoon · Int. J. Hydrogen Energy · 2003 · 28 · 65710.1016/S0360-3199(02)00156-8 ↗
44. Prasanna · J. Power Sources · 2004 · 137 · 110.1016/j.jpowsour.2004.05.034 ↗
45. Yu · Fuel Cells · 2008 · 8 · 16510.1002/fuce.200800024 ↗
46. Oono · J. Power Sources · 2013 · 241 · 8710.1016/j.jpowsour.2013.03.122 ↗