journal article·2007-01

The influence of hydrogen sulfide on proton exchange membrane fuel cell anodes

Weiyu Shi, Baolian Yi, Ming Hou, Fenning Jing, Hongmei Yu, Pingwen Ming

Journal of Power Sources· Volume 164· Issue 1
Publisher page

Abstract

Abstract The effect of hydrogen sulfide on proton exchange membrane fuel cell (PEMFC) anodes was studied by cyclic voltammetry (CV), potential steps and electrochemical impedance spectroscopy (EIS). The severity of the effect of H 2 S varies depending on the H 2 S concentration, current density and the cell temperature. The anode humidification does not impact the poisoning rate much when the anode is exposed to H 2 S. The adsorption of H 2 S on the anode is dissociative and this dissociation can produce adsorbed sulfur. The dissociation potential of H 2 S was studied by potential steps, and the values of the dissociation potential are about 0.4 V at 90 °C, 0.5 V at 60 °C and 0.6 V at 30 °C, respectively. The adsorbed sulfur can be oxidized at a higher potential. During CV scans, two oxidation peaks for the adsorbed sulfur at 1.07 and 1.2 V were observed at 90 °C, however a single oxidation peak could be observed at 1.2 V at 60 °C and at 1.27 V at 30 °C. Application of EIS to a H 2 S|H 2 half-cell shows that the charge transfer resistance increases when the anode is exposed to H 2 S because of H 2 S adsorption.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Industrial Gas Emission Control

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Fuel Cell Handbook, fifth ed., US Department of Energy, West Virginia, 2000.
2. Loučka · J. Electroanal. Chem. · 1971 · 31 · 31910.1016/S0022-0728(71)80162-6 ↗
3. Najdeker · Electroanal. Chem. Interfacial Electrochem. · 1973 · 41 · 7910.1016/S0022-0728(73)80031-2 ↗
4. Contractor · J. Electroanal. Chem. · 1979 · 96 · 17510.1016/S0022-0728(79)80374-5 ↗
5. Uribe · 2001
6. Mohtadi · Electrochem. Solid-State Lett. · 2003 · 6 · A27210.1149/1.1621831 ↗
7. Mohtadi · Appl. Catal. B: Environ. · 2005 · 56 · 3710.1016/j.apcatb.2004.08.012 ↗
8. Chin · J. Electrochem. Soc. · 1986 · 133 · 244710.1149/1.2108447 ↗
9. Wagner · J. Appl. Electrochem. · 2002 · 32 · 85910.1023/A:1020551609230 ↗
10. Yang · J. Electrochem. Soc. · 2006 · 153 · A104310.1149/1.2189280 ↗
11. Mathieu · Appl. Catal. · 1984 · 9 · 36110.1016/0166-9834(84)80007-X ↗
12. Lu · J. Power Sources · 2003 · 124 · 8110.1016/S0378-7753(03)00616-5 ↗
13. Yuan · J. Power Sources · 2006 · 161 · 92010.1016/j.jpowsour.2006.05.003 ↗
14. Ciureanu · J. Phys. Chem. B · 1999 · 103 · 964510.1021/jp9918407 ↗