journal article·2017-02

Fabrication and characterization of a tubular ceramic fuel cell based on BaZr0.1Ce0.7Y0.1Yb0.1O3-δ proton conducting electrolyte

Amir Reza Hanifi, Navjot Kaur Sandhu, Thomas H. Etsell, Jing-Li Luo, Partha Sarkar

Publisher page

Abstract

Abstract A proton conducting anode supported tubular fuel cell is fabricated in this research using the highly proton conductive BaZr 0.1 Ce 0.7 Y 0.1 Yb 0.1 O 3-δ (BZCYYb) electrolyte. The cell is in a Ni-BZCYYb/BZCYYb/LSCF-BZCYYb configuration consisting of a support, electrolyte and cathode with thicknesses of 680 μm, 25 μm and 90 μm, respectively. The cell delivers maximum power densities of 331, 362 and 416 mW/cm 2 at 600, 650 and 700 °C, respectively. AC impedance spectroscopy results show values of 0.94 Ω.cm 2 , 0.73 Ω.cm 2 , and 0.60 Ω.cm 2 for total resistance at the corresponding temperatures while the major resistance contributor is the ohmic resistance. The Ni-BZCYYb anode microstructure shows detachment of Ni and the BZCYYb in most regions as well as pores inside the Ni grains. Despite the low anode porosity (25%), the cell gives a very low concentration polarization value (0.05 Ω.cm 2 ) indicating that the fuel gas could readily diffuse into the microstructure. This might be attributed to water forming on the cathode side, which masks the necessity of having a high porosity anode. The cell fails when tested under CO:H 2 of 1:1 at 700 °C due to significant carbon (graphite) formation indicating that proton conductors based on barium cerates are not appropriate choices for application under hydrocarbon fuels.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Minh · J. Am. Ceram. Soc. · 1993 · 76 · 56310.1111/j.1151-2916.1993.tb03645.x ↗
2. Haile · Acta Mater. · 2003 · 51 · 598110.1016/j.actamat.2003.08.004 ↗
3. Steele · Nature · 2001 · 414 · 34510.1038/35104620 ↗
4. Tao · Adv. Mater. · 2006 · 18 · 158110.1002/adma.200502098 ↗
5. Fabbri · Adv. Mater. · 2012 · 24 · 19510.1002/adma.201103102 ↗
6. Schober · Solid State Ionics · 2003 · 162 · 27710.1016/S0167-2738(03)00241-8 ↗
7. Demin · Int. J. Hydrogen Energy · 2001 · 26 · 110310.1016/S0360-3199(01)00043-X ↗
8. Coors · J. Power Sources · 2003 · 118 · 15010.1016/S0378-7753(03)00072-7 ↗
9. Kreuer · Solid State Ionics · 1999 · 125 · 28510.1016/S0167-2738(99)00188-5 ↗
10. Manning · Solid State Ionics · 1997 · 100 · 110.1016/S0167-2738(97)00345-7 ↗
11. Xie · J. Alloys Compd. · 2009 · 472 · 55110.1016/j.jallcom.2008.05.036 ↗
12. Min · Ceram. Int. · 2014 · 40 · 151310.1016/j.ceramint.2013.07.036 ↗
13. Iwahara · Solid State Ionics · 2004 · 168 · 29910.1016/j.ssi.2003.03.001 ↗
14. Rainwater · Int. J. Hydrogen Energy · 2012 · 37 · 1834210.1016/j.ijhydene.2012.09.027 ↗
15. Norby · Solid State Ionics · 1999 · 125 · 110.1016/S0167-2738(99)00152-6 ↗
16. Kreuer · Ann. Rev. Mater. Res. · 2003 · 33 · 33310.1146/annurev.matsci.33.022802.091825 ↗
17. Babilo · J. Am. Ceram. Soc. · 2005 · 88 · 236210.1111/j.1551-2916.2005.00449.x ↗
18. Yamazaki · J. Mater. Chem. · 2010 · 20 · 815810.1039/c0jm02013c ↗
19. Park · Solid State Ionics · 2010 · 181 · 16310.1016/j.ssi.2009.06.015 ↗
20. Giannici · Solid State Ionics · 2007 · 178 · 58710.1016/j.ssi.2007.01.015 ↗
21. Coors · J. Am. Ceram. Soc. · 2002 · 85 · 263710.1111/j.1151-2916.2002.tb00507.x ↗
22. Sawant · Electrochim. Acta · 2014 · 120 · 8010.1016/j.electacta.2013.12.061 ↗
23. Liu · Int. J. Hydrogen Energy · 2011 · 36 · 1374110.1016/j.ijhydene.2011.07.087 ↗
24. Bhide · J. Electrochem. Soc. · 1999 · 146 · 203810.1149/1.1391888 ↗
25. Zakowsky · Solid State Ionics · 2005 · 176 · 301910.1016/j.ssi.2005.09.040 ↗
26. Murugaraj · Solid State Ionics · 1997 · 9810.1016/S0167-2738(97)00102-1 ↗
27. VahidMohammadi · J. Electrochem. Soc. · 2015 · 162 · F80310.1149/2.0021508jes ↗
28. Yang · Science · 2009 · 326 · 12610.1126/science.1174811 ↗
29. Suzuki · J. Power Sources · 2006 · 160 · 7310.1016/j.jpowsour.2006.01.037 ↗
30. Kendall · Int. J. Appl. Ceram. Technol. · 2010 · 7 · 110.1111/j.1744-7402.2008.02350.x ↗
31. Lawlor · J. Power Sources · 2009 · 193 · 38710.1016/j.jpowsour.2009.02.085 ↗
32. Hibino · J. Electrochem. Soc. · 2002 · 149 · A150310.1149/1.1513983 ↗
33. Adler · Solid State Ionics · 1998 · 111 · 12510.1016/S0167-2738(98)00179-9 ↗
34. Reitz · J. Power Sources · 2006 · 161 · 43710.1016/j.jpowsour.2006.04.019 ↗
35. Xin · J. Power Sources · 2006 · 160 · 122110.1016/j.jpowsour.2006.02.073 ↗
36. Zhao · J. Power Sources · 2011 · 196 · 68810.1016/j.jpowsour.2010.07.058 ↗
37. Choi · Int. J. Hydrogen Energy · 2014 · 39 · 1281210.1016/j.ijhydene.2014.06.018 ↗
38. Kuhn · J. Phys. Chem. C · 2008 · 112 · 1246810.1021/jp801521y ↗