Cycling stability and degradation mechanism of LiMnPO4 based electrodes
Source abstract
Abstract
Abstract Long term stability of LiMnPO 4 particles with a crystallite size between ∼20 and 50 nm covered with a dense native carbon coating (14 wt.%) is demonstrated. More than 500 cycles at a rate of C/20, in the potential window of 2.7–4.5 V and a temperature of 55 °C were achieved. During most of the cycling the average capacity decay was less than 0.06% per cycle. After about 500 cycles a sudden capacity drop was observed. Degradation processes in various stages of cycling were thoroughly examined using a range of techniques. Severe surface film formation, manganese dissolution and degradation of Li x MnPO 4 accompanied by formation of Li 4 P 2 O 7 were clearly identified. The good long term stability seems to be due to dense, protective carbon coating. Decomposition is most likely initiated at local defects in the microstructure of pyrolytic carbon coating around LiMnPO 4 particles. In addition to known degradation mechanisms of LiMnPO 4 we observed pronounced gradual amorphization of the olivine crystallites during long-term cycling at 55 °C. Finally, changes in morphology of the carbon black additive after prolonged cycling are reported and commented.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. High-performance carbon-LiMnPO4 nanocomposite cathode for lithium batteries10.1002/adfm.201000469 ↗
2. Enhanced electrochemical performance of carbon–LiMn1−xFexPO4 nanocomposite cathode for lithium-ion batteries10.1016/j.jpowsour.2010.11.159 ↗
3. Highly porous LiMnPO4 in combination with an ionic liquid-based polymer gel electrolyte for lithium batteries10.1016/j.elecom.2011.07.005 ↗
4. Improved capacity retention in rechargeable 4 V lithium/lithium-manganese oxide (spinel) cells10.1016/0167-2738(94)90450-2 ↗
5. Electrochemical performance of nanocomposite LiMnPO4/C cathode materials for lithium batteries10.1016/j.elecom.2009.10.039 ↗
6. Synthesis and characterization of lithium manganese phosphate by a precipitation method10.1149/1.3265440 ↗
7. LiMnPO4 nanoplate grown via solid-state reaction in molten hydrocarbon for Li-ion battery cathode10.1021/nl1007085 ↗
8. LiMnPO4 as an advanced cathode material for rechargeable lithium batteries10.1149/1.3125765 ↗
9. Electrochemical activity of carbon blacks in LiPF6-based organic electrolytes10.1016/j.jpowsour.2013.07.033 ↗
10. The cathode-electrolyte interface in the Li-ion battery10.1016/j.electacta.2004.03.049 ↗
11. Toward understanding of electrical limitations (electronic, ionic) in LiMPO4 (M = Fe, Mn) electrode materials10.1149/1.1884787 ↗
12. Polyanionic (phosphates, silicates, sulfates) frameworks as electrode materials for rechargeable Li (or Na) batteries10.1021/cr3001862 ↗
13. The degradation mechanism of a composite LiMnPO4 cathode10.1149/2.018209jes ↗
14. Ageing mechanisms in lithium-ion batteries10.1016/j.jpowsour.2005.01.006 ↗
15. Huggins · 2009
16. Synthesis of nanometric LiMnPO4 via a two-step technique10.1021/cm203095d ↗
17. 2003
18. 2000
19. Mn(II) deposition on anodes and its effects on capacity fade in spinel lithium manganate-carbon systems10.1038/ncomms3437 ↗
20. Self-discharge of LiMn2O4/C Li-ion cells in their discharged state10.1149/1.1838235 ↗
21. Influence of manganese(II), cobalt(II), and nickel(II) additives in electrolyte on performance of graphite anode for lithium-ion batteries10.1016/S0013-4686(01)00847-7 ↗
22. Improved lithium manganese oxide spinel/graphite Li-ion cells for high-power applications10.1016/j.jpowsour.2003.11.007 ↗
23. Influence of carbon black and binder on Li-ion batteries10.1016/S0378-7753(01)00481-5 ↗
24. Interfacial impedance study of Li-ion composite cathodes during aging at elevated temperatures10.1149/1.2213568 ↗
25. Interfacial phenomena at a composite LiMnPO4 cathode10.1149/2.076207jes ↗
26. Interfacial side-reactions at a LiNi0.5Mn1.5O4 electrode in organic carbonate-based electrolytes10.1016/j.elecom.2013.04.007 ↗
27. The study of surface phenomena related to electrochemical lithium intercalation into LixMOy host materials (M = Ni, Mn)10.1149/1.1393357 ↗
28. New insights into the interactions between electrode materials and electrolyte solutions for advanced nonaqueous batteries10.1016/S0378-7753(99)00187-1 ↗
29. I. Exnar, T. Drezen, M. Zukalova, J. Miners, O. Frank, L. Kavan, U.S. Patent 2010/0178562 A1, 2010.10.1149/MA2010-03/1/413 ↗
30. Structure of rapidly quenched lithium phosphate glasses
31. Improved electrode performance of porous LiFePO4 using RuO2 as an oxidic nanoscale interconnect10.1002/adma.200700697 ↗
32. Structural changes in vanadium oxide-based cathodes during cycling in a lithium polymer electrolyte cell10.1016/0013-4686(92)80145-C ↗
33. The LixV2O5 system: an overview of the structure modifications induced by the lithium intercalation10.1016/0167-2738(94)90414-6 ↗
34. Electrochemically-driven solid-state amorphization in lithium-silicon alloys and implications for lithium storage10.1016/S1359-6454(02)00514-1 ↗
35. Deformation and stress in electrode materials for Li-ion batteries10.1016/j.pmatsci.2014.02.001 ↗
36. Phase diagram of Lix(MnyFe1−y)PO4 (0 ≤ x, y ≤ 1)10.1149/1.1401083 ↗
37. One-step low-temperature route for the preparation of electrochemically active LiMnPO4 powders10.1021/cm030347b ↗
38. Solid solution phases in the olivine-type LiMnPO4/MnPO4 system10.1149/1.3167389 ↗
39. Improving the performance of lithium manganese phosphate through divalent cation substitution10.1149/1.2971169 ↗
40. Phase stability study of Li1−xMnPO4 (0 ≤ x ≤ 1) cathode for Li rechargeable battery10.1149/1.3138705 ↗