Three-dimensional cubic ordered mesoporous carbon (CMK-8) as highly efficient stable Pd electro-catalyst support for formic acid oxidation
Source abstract
Abstract
Abstract In this work, Pd nanoparticles were supported on two types of three-dimensional cubic highly ordered mesoporous carbon (CMK-8) by the sodium borohydride reduction method and the activity of the Pd/CMK-8 electro-catalysts towards formic acid oxidation was evaluated and compared with that of commercial Pd/C (E-TEK) catalyst. The catalysts were characterized by transmission electron microscopy (TEM), X-ray diffraction (XRD), cyclic voltammetry, and chronoamperometry. Cyclic voltammetry revealed Pd/CMK-8 with larger pores as being the most electroactive with a mass specific activity (mA mgPd−1) of 486.4 that exceeded not only that of the Pd/C (E-TEK) (386.5 mA mgPd−1) but also that of recently reported Pd/CNT (200 mA mgPd−1), Pd/Graphene (210 mA mgPd−1) and Pd/Vulcan XC 72 (193 mA mgPd−1). As demonstrated with chronoamperometry, the larger pore Pd/CMK-8 also proved to be the most stable catalyst. This exceptional performance can be ascribed to the very high surface area and Ia3d symmetry that yields a relatively isotropic graphitized structure with a high conductivity. In addition, the open framework of the 3-D bicontinous channels and highly ordered mesopores allows for an advanced mass transfer characteristics. The results show that CMK-8 support would significantly improve the power output and stability of Pd-based electro-catalysts for formic acid oxidation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · Catalytic Processes in Materials Science · Covalent Organic Framework Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Feng · J. Power Sources · 2011 · 196 · 246910.1016/j.jpowsour.2010.11.073 ↗
2. Gago · J. Power Sources · 2011 · 196 · 132410.1016/j.jpowsour.2010.08.109 ↗
3. Zhou · J. Power Sources · 2011 · 196 · 111810.1016/j.jpowsour.2010.08.053 ↗
4. Bai · J. Alloy Compd. · 2011 · 509 · 102910.1016/j.jallcom.2010.09.165 ↗
5. Masud · Electrochem. Commun. · 2011 · 13 · 8610.1016/j.elecom.2010.11.020 ↗
6. Mamuru · J. Mater. Chem. · 2010 · 20 · 1070510.1039/c0jm02210a ↗
7. Ge · Electrochim. Acta · 2010 · 55 · 913210.1016/j.electacta.2010.09.002 ↗
8. Maiyalagan · Mater. Sci. Forum · 2010 · 657 · 14310.4028/www.scientific.net/MSF.657.143 ↗
9. Xia · J. Electrochem. Soc. · 1993 · 140 · 255910.1149/1.2220862 ↗
10. Maiyalagan · Catal. Commun. · 2009 · 10 · 43310.1016/j.catcom.2008.10.011 ↗
11. Rice · J. Power Sources · 2003 · 115 · 22910.1016/S0378-7753(03)00026-0 ↗
12. Yu · J. Power Sources · 2008 · 182 · 12410.1016/j.jpowsour.2008.03.075 ↗
13. Lu · J. Phys. Chem. B · 1999 · 103 · 970010.1021/jp992297x ↗
14. Maiyalagan · J. Solid State Electrochem. · 2009 · 13 · 156110.1007/s10008-008-0730-0 ↗
15. Maiyalagan · J. Power Sources · 2010 · 195 · 524610.1016/j.jpowsour.2010.03.022 ↗
16. Maiyalagan · Int. J. Hydrogen Energy · 2009 · 34 · 287410.1016/j.ijhydene.2009.01.069 ↗
17. Zhang · Energy Environ. Sci. · 2010 · 3 · 128610.1039/c0ee00139b ↗
18. Lee · J. Appl. Electrochem. · 2006 · 36 · 50710.1007/s10800-006-9120-4 ↗
19. Shao · J. Mater. Chem. · 2009 · 19 · 4610.1039/B808370C ↗
20. Maiyalagan · Appl. Catal. B Environ. · 2008 · 89 · 28610.1016/j.apcatb.2007.11.033 ↗
21. Maiyalagan · Electrochem. Commun. · 2005 · 7 · 90510.1016/j.elecom.2005.07.007 ↗
22. Shao · Appl. Catal. B · 2008 · 79 · 8910.1016/j.apcatb.2007.09.047 ↗
23. Ji · Nat. Mat. · 2010 · 2 · 286
24. Kong · Appl. Surf. Sci. · 2010 · 256 · 668810.1016/j.apsusc.2010.04.071 ↗
25. Salgado · J. Power Sources · 2010 · 195 · 402210.1016/j.jpowsour.2010.01.001 ↗
26. Antolini · Appl. Catal. B · 2009 · 88 · 110.1016/j.apcata.2009.05.045 ↗
27. Joo · Nature · 2001 · 412 · 16910.1038/35084046 ↗
28. Sun · J.Electroanal.Chem. · 2009 · 633 · 110.1016/j.jelechem.2009.04.013 ↗
29. Kim · J. Am. Chem. Soc. · 2005 · 127 · 760110.1021/ja042601m ↗
30. Jun · J. Am. Chem. Soc. · 2000 · 122 · 1071210.1021/ja002261e ↗
31. Wan · Chem. Mater. · 2008 · 20 · 93210.1021/cm7024125 ↗
32. Maiyalagan · J. Phys. Chem.C · 2012 · 116 · 263010.1021/jp210266n ↗
33. Radmilovic · J. Catal. · 1995 · 15 · 9810.1006/jcat.1995.1151 ↗
34. Antolini · J. Alloys Compd. · 2001 · 315 · 11810.1016/S0925-8388(00)01260-3 ↗
35. Chen · Fuel Cells · 2010 · 10 · 117110.1002/fuce.201000046 ↗
36. Suo · Electrochim. Acta · 2009 · 55 · 21010.1016/j.electacta.2009.08.039 ↗
37. Lee · J. Power Sources · 2010 · 195 · 589610.1016/j.jpowsour.2009.12.013 ↗
38. Acosta · J. Power Sources · 2010 · 195 · 46110.1016/j.jpowsour.2009.08.014 ↗
39. Duncan · Electrochim. Acta · 2007 · 52 · 619510.1016/j.electacta.2007.03.068 ↗
40. Soreta · Langmuir · 2010 · 26 · 1229310.1021/la101398g ↗
41. Park · Electrochim. Acta · 2010 · 55 · 433910.1016/j.electacta.2010.01.093 ↗
42. Liu · J. Power Sources · 2006 · 161 · 83110.1016/j.jpowsour.2006.05.052 ↗
43. Lu · J. Phys. Chem. C · 2010 · 114 · 2119010.1021/jp107768n ↗
44. Yang · J. Mater. Chem. · 2011 · 21 · 338410.1039/c0jm03361h ↗
45. Winjobi · Electrochim. Acta · 2010 · 55 · 421710.1016/j.electacta.2010.02.062 ↗