Abstract To examine the impact of charge protocol and temperature on Li-ion cell degradation, commercial 18650 Li-ion cells with NCA/C chemistry are cycled deeply1000 times at either 25 °C or 60 °C using two different charge termination protocols: (a) potential-limited constant-current (CC) without a constant potential dwell, or (b) constant-current constant-voltage (CC-CV). Analyses indicate that the cells that experienced the CC CV charge protocol show a lower degradation rate than those cycled using the potential-limited/CC charge protocol at both temperatures. Additionally, the cells that used the potential-limited/CC charge protocol exhibit a much higher capacity degradation rate at 25 °C than at 60 °C. Electron microscopy and surface chemistry analyses show a thick secondary solid-electrolyte interphase (SEI) is formed on the anode surface for the cell using the potential-limited CC charge protocol at 25 °C, while this does not occur in the cells with potential-limited CC charge protocol at 60 °C. Based on the electrochemical data, this thick secondary SEI shows large resistance and makes higher rate cycling difficult. This secondary SEI is thought to be a key contributor to the fast capacity degradation rate of the cells using the CC charge protocol at 25 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Swain · Separ. Purif. Technol. · 2017 · 172 · 38810.1016/j.seppur.2016.08.031 ↗
2. Lv · ACS Sustain. Chem. Eng. · 2018 · 6 · 150410.1021/acssuschemeng.7b03811 ↗
3. Song · RSC Adv. · 2017 · 7 · 478310.1039/C6RA27210J ↗
4. Dunn · Environ. Sci. Technol. · 2012 · 46 · 1270410.1021/es302420z ↗
5. Wang · Energy Technol-Ger · 2018 · 6 · 242910.1002/ente.201800315 ↗
6. Vetter · J. Power Sources · 2005 · 147 · 26910.1016/j.jpowsour.2005.01.006 ↗
7. Kabir · Int. J. Energy Res. · 2017 · 41 · 196310.1002/er.3762 ↗
8. Waldmann · J. Power Sources · 2018 · 384 · 10710.1016/j.jpowsour.2018.02.063 ↗
9. Liu · RSC Adv. · 2016 · 6 · 8868310.1039/C6RA19482F ↗
10. Li · J. Power Sources · 2014 · 254 · 16810.1016/j.jpowsour.2013.12.099 ↗
11. Waldmann · Electrochim. Acta · 2015 · 178 · 52510.1016/j.electacta.2015.08.056 ↗
12. Petzl · J. Power Sources · 2015 · 275 · 79910.1016/j.jpowsour.2014.11.065 ↗
13. Burns · J. Electrochem. Soc. · 2015 · 162 · A95910.1149/2.0621506jes ↗
14. Waldmann · J. Electrochem. Soc. · 2016 · 163 · A123210.1149/2.0591607jes ↗
15. Lu · J. Electrochem. Soc. · 2013 · 160 · A313810.1149/2.022305jes ↗
16. Browning · J. Power Sources · 2013 · 239 · 34110.1016/j.jpowsour.2013.03.118 ↗
17. Li · Chem. Soc. Rev. · 2017 · 6 · 300610.1039/C6CS00875E ↗
18. Xiong · J. Electrochem. Soc. · 2016 · 163 · A54610.1149/2.0951603jes ↗
19. Norberg · Electrochem. Commun. · 2013 · 34 · 2910.1016/j.elecom.2013.04.007 ↗
20. MahootcheianAsl · Electrochem. Commun. · 2013 · 32 · 110.1016/j.elecom.2013.03.031 ↗
21. Xiong · J. Electrochem. Soc. · 2016 · 163 · A306910.1149/2.1031614jes ↗
22. Xiong · J. Electrochem. Soc. · 2017 · 164 · A34010.1149/2.1091702jes ↗
23. Li · J. Electrochem. Soc. · 2013 · 160 · A152410.1149/2.051309jes ↗
24. Joshi · J. Electrochem. Soc. · 2014 · 161 · A191510.1149/2.0861412jes ↗
25. Gilbert · J. Electrochem. Soc. · 2017 · 164 · A38910.1149/2.1111702jes ↗
26. Pieczonka · J. Phys. Chem. C · 2013 · 117 · 1594710.1021/jp405158m ↗
27. Burns · J. Electrochem. Soc. · 2013 · 160 · A145110.1149/2.060309jes ↗
28. Krueger · J. Electrochem. Soc. · 2013 · 160 · A54210.1149/2.022304jes ↗
29. Zhang · J. Power Sources · 2006 · 161 · 138510.1016/j.jpowsour.2006.06.040 ↗
30. Waldmann · J. Power Sources · 2014 · 262 · 12910.1016/j.jpowsour.2014.03.112 ↗
31. Pinson · J. Electrochem. Soc. · 2013 · 160 · A24310.1149/2.044302jes ↗
32. Sloop · J. Power Sources · 2003 · 119 · 33010.1016/S0378-7753(03)00149-6 ↗
33. Guéguen · J. Electrochem. Soc. · 2016 · 163 · A109510.1149/2.0981606jes ↗
34. Wagner · ACS Appl. Mater. Interfaces · 2016 · 8 · 3087110.1021/acsami.6b09164 ↗
35. Andersson · J. Electrochem. Soc. · 2002 · 149 · A135810.1149/1.1505636 ↗
36. Yang · J. Power Sources · 2017 · 360 · 2810.1016/j.jpowsour.2017.05.110 ↗