journal article·2011-09

Effects of chromium poisoning on the long-term oxygen exchange kinetics of the solid oxide fuel cell cathode materials La0.6Sr0.4CoO3 and Nd2NiO4

Min Yang, Edith Bucher, Werner Sitte

Journal of Power Sources· Volume 196· Issue 17
Publisher page

Abstract

Abstract The influence of chromium poisoning on the long-term stability of the oxygen exchange kinetics of the promising IT-SOFC cathode materials La 0.6 Sr 0.4 CoO 3−δ (LSC) and Nd 2 NiO 4+δ (NDN) is investigated in-situ by dc-conductivity relaxation experiments. The as-prepared LSC and NDN samples show high chemical oxygen surface exchange coefficients k chem . After the deposition of a 10 nm thick Cr-layer onto the surface, k chem of LSC decreases to 50% of the initial value. Additional chromium deposition of 20 nm on LSC leads to a further decrease of k chem to 27% of the initial value. In contrast, the effect of a 10 nm thick Cr-layer on k chem of NDN is negligible. Even with additional 20 nm of chromium and a total testing time of 1750 h, the nickelate retains a k chem of 60% of the initial value. X-ray photoelectron spectroscopy (XPS) of the degraded. LSC shows a significantly altered surface cation composition with Sr-enrichment down to 30 nm depth while XPS analysis of the degraded NDN reveals a thin surface zone of approximately 30 nm containing nickel and chromium. In contrast to LSC, the changes in the surface composition of NDN due to Cr-poisoning ultimately had only a minor influence on the surface exchange properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Teraoka · Mater. Res. Bull. · 1988 · 23 · 5110.1016/0025-5408(88)90224-3 ↗
2. Mizusaki · Solid State Ionics · 1992 · 52 · 7910.1016/0167-2738(92)90093-5 ↗
3. Tai · Solid State Ionics · 1995 · 76 · 25910.1016/0167-2738(94)00244-M ↗
4. Tai · Solid State Ionics · 1995 · 76 · 27310.1016/0167-2738(94)00245-N ↗
5. Sun · J. Solid State Electrochem. · 2010 · 14 · 112510.1007/s10008-009-0932-0 ↗
6. Tarancón · J. Mater. Chem. · 2010 · 20 · 379910.1039/b922430k ↗
7. Peters · J. Electrochem. Soc. · 2008 · 155 · B73010.1149/1.2909552 ↗
8. Januschewsky · Adv. Funct. Mater. · 2009 · 19 · 315110.1002/adfm.200900362 ↗
9. Heel · J. Power Sources · 2010 · 195 · 670910.1016/j.jpowsour.2010.04.006 ↗
10. Bucher · J. Electrochem. Soc. · 2008 · 155 · B121810.1149/1.2981024 ↗
11. Yokokawa · J. Alloys Compd. · 2008 · 452 · 4110.1016/j.jallcom.2006.12.150 ↗
12. Dieterle · J. Mater. Sci. · 2008 · 43 · 313510.1007/s10853-008-2502-8 ↗
13. Hjalmarsson · Solid State Ionics · 2008 · 179 · 142210.1016/j.ssi.2007.11.010 ↗
14. E. Bucher, W. Sitte, Solid State Ionics, in press, doi:10.1016/j.ssi.2010.01.006.10.1016/j.ssi.2010.01.006 ↗
15. Mauvy · J. Eur. Ceram. Soc. · 2005 · 25 · 266910.1016/j.jeurceramsoc.2005.03.120 ↗
16. Zhao · Solid State Ionics · 2008 · 179 · 200010.1016/j.ssi.2008.06.019 ↗
17. Egger · 2009 · 2547
18. Greenblatt · Curr. Opin. Solid State Mater. Sci. · 1997 · 2 · 17410.1016/S1359-0286(97)80062-9 ↗
19. Tamura · Physica C · 1996 · 258 · 6110.1016/0921-4534(95)00798-9 ↗
20. Boehm · Solid State Ionics · 2005 · 176 · 271710.1016/j.ssi.2005.06.033 ↗
21. Naumovich · Solid State Sci. · 2005 · 7 · 135310.1016/j.solidstatesciences.2005.08.005 ↗
22. Lalanne · J. Power Sources · 2008 · 185 · 121810.1016/j.jpowsour.2008.06.072 ↗
23. Haanappel · J. Fuel Cell Sci. Technol. · 2009 · 6 · 0410161
24. Komatsu · J. Power Sources · 2008 · 176 · 13210.1016/j.jpowsour.2007.10.068 ↗
25. Jiang · Solid State Ionics · 2008 · 179 · 145910.1016/j.ssi.2008.01.006 ↗
26. Yokokawa · 2009 · 923
27. Menzler · 2009 · 566
28. Schuler · 2010 · 7111
29. Montero · J. Power Sources · 2008 · 184 · 17210.1016/j.jpowsour.2008.05.081 ↗
30. Jablonski · J. Power Sources · 2008 · 180 · 43310.1016/j.jpowsour.2008.02.010 ↗
31. Kim · Curr. Appl. Phys. · 2010 · 10 · S8610.1016/j.cap.2009.11.049 ↗
32. D. Chatterjee, S. Biswas, Int. J. Hydrogen Energy, in press, doi:10.1016/j.ijhydene.2010.04.114.10.1016/j.ijhydene.2010.04.114 ↗
33. Q.X. Fu, D. Sebold, F. Tietz, H.P. Buchkremer, Solid State Ionics, in press, doi:10.1016/j.ssi.2010.03.010.10.1016/j.ssi.2010.03.010 ↗
34. Douy · Int. J. Inorg. Mater. · 2001 · 3 · 69910.1016/S1466-6049(01)00188-X ↗
35. Preis · Solid State Ionics · 2004 · 175 · 39310.1016/j.ssi.2003.12.045 ↗
36. Bucher · Solid State Ionics · 2008 · 179 · 103210.1016/j.ssi.2008.01.089 ↗
37. Finsterbusch · Solid State Ionics · 2010 · 181 · 64010.1016/j.ssi.2010.03.007 ↗
38. Yang · 2010 · 10151
39. Egger · J. Electrochem. Soc. · 2010 · 157 · B153710.1149/1.3481420 ↗
40. Marcos · J. Catal. · 1987 · 105 · 9510.1016/0021-9517(87)90011-X ↗
41. van der Heide · Surf. Interface Anal. · 2002 · 33 · 41410.1002/sia.1227 ↗
42. Simner · Electrochem. Solid-State Lett. · 2006 · 9 · A47810.1149/1.2266160 ↗
43. Fearn · Solid State Ionics · 2008 · 179 · 81110.1016/j.ssi.2008.01.020 ↗
44. Oh · 2009 · 2871
45. Jiang · J. Electrochem. Soc. · 2006 · 153 · A12710.1149/1.2136077 ↗
46. Konysheva · J. Electrochem. Soc. · 2006 · 153 · A76510.1149/1.2172563 ↗
47. Yokokawa · Solid State Ionics · 2006 · 177 · 319310.1016/j.ssi.2006.07.055 ↗
48. Komatsu · Electrochem. Solid-State Lett. · 2006 · 9 · A910.1149/1.2130309 ↗