Effect of H2O2 on Nafion® properties and conductivity at fuel cell conditions
Source abstract
Abstract
Abstract During PEM fuel cell operation, formation of H 2 O 2 and material corrosion occurs, generating trace amounts of metal cations (i.e., Fe 2+ , Pt 2+ ) and subsequently initiating the deterioration of cell components and, in particular, PFSA membranes (e.g., Nafion). However, most previous studies of this have been performed using conditions not relevant to fuel cell environments, and very few investigations have studied the effect of Nafion decomposition on conductivity, one of the most crucial factors governing PEMFC performance. In this study, a quantitative examination of properties and conductivities of degraded Nafion membranes at conditions relevant to fuel cell environments (30–100%RH and 80 °C) was performed. Nafion membranes were pre-ion-exchanged with small amounts of Fe 2+ ions prior to H 2 O 2 exposure. The degradation degree (defined as loss of ion-exchange capacity, weight, and fluoride content), water uptake, and conductivity of H 2 O 2 -exposed membranes were found to strongly depend on Fe content and H 2 O 2 treatment time. SEM cross-sections showed that the degradation initially took place in the center of the membrane, while FTIR analysis revealed that Nafion degradation preferentially proceeds at the sulfonic end group and at the ether linkage located in the pendant side chain and that the H-bond of water is weakened after prolonged H 2 O 2 exposure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Membrane-based Ion Separation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Zhang · J. Power Sources · 2009 · 194 · 58810.1016/j.jpowsour.2009.06.073 ↗
2. Li · Ind. Eng. Chem. Res. · 2001 · 40 · 478910.1021/ie010467y ↗
3. Chen · J. Power Sources · 2007 · 169 · 28810.1016/j.jpowsour.2007.03.037 ↗
4. Tang · J. Power Sources · 2007 · 170 · 8510.1016/j.jpowsour.2007.03.061 ↗
5. Marrony · J. Power Sources · 2008 · 182 · 46910.1016/j.jpowsour.2008.02.096 ↗
6. Yoda · Electrochim. Acta · 2007 · 52 · 599710.1016/j.electacta.2007.03.049 ↗
7. Darling · J. Electrochem. Soc. · 2005 · 152 · A24210.1149/1.1836156 ↗
8. Guilminot · J. Electrochem. Soc. · 2007 · 154 · B110610.1149/1.2775218 ↗
9. Guilminot · J. Electrochem. Soc. · 2007 · 154 · B9610.1149/1.2388863 ↗
10. Ramaswamy · Electrochim. Acta · 2008 · 53 · 327910.1016/j.electacta.2007.11.010 ↗
11. Shao · J. Power Sources · 2007 · 171 · 55810.1016/j.jpowsour.2007.07.004 ↗
12. Aoki · Electrochem. Commun. · 2006 · 8 · 150910.1016/j.elecom.2006.07.017 ↗
13. Qiao · J. Electrochem. Soc. · 2006 · 153 · A96710.1149/1.2186768 ↗
14. Vishal · J. Electrochem. Soc. · 2007 · 154 · B65210.1149/1.2734869 ↗
15. Xie · Polymer · 2007 · 48 · 549710.1016/j.polymer.2007.07.043 ↗
16. Young · J. Electrochem. Soc. · 2010 · 157 · B42510.1149/1.3281899 ↗
17. Zhou · Macromolecules · 2007 · 40 · 869510.1021/ma071603z ↗
18. Endoh · Electrochem. Solid-State Lett. · 2004 · 7 · A20910.1149/1.1739314 ↗
19. Jung · J. Power Sources · 2007 · 170 · 28110.1016/j.jpowsour.2007.03.084 ↗
20. Curtin · J. Power Sources · 2004 · 131 · 4110.1016/j.jpowsour.2004.01.023 ↗
21. Healy · Fuel Cells · 2005 · 5 · 30210.1002/fuce.200400050 ↗
22. Schiraldi · Polym. Rev. · 2006 · 46 · 315
23. Chen · Electrochim. Acta · 2009 · 54 · 398410.1016/j.electacta.2009.02.021 ↗
24. Kundu · Polym. Degrad. Stab. · 2008 · 93 · 21410.1016/j.polymdegradstab.2007.10.001 ↗
25. Maletzky · Chemosphere · 1999 · 38 · 231510.1016/S0045-6535(98)00450-0 ↗
26. Pozio · Electrochim. Acta · 2003 · 48 · 154310.1016/S0013-4686(03)00026-4 ↗
27. Schiraldi · J. Macromol. Sci. Pol. Rev. · 2006 · 46 · 31510.1080/15583720600796458 ↗
28. Hongsirikarn · J. Power Sources · 2010 · 195 · 3010.1016/j.jpowsour.2009.07.013 ↗
29. Hongsirikarn · J. Power Sources · 2010 · 195 · 721310.1016/j.jpowsour.2010.05.005 ↗
30. Hongsirikarn · J. Power Sources · 2010 · 195 · 341610.1016/j.jpowsour.2009.12.023 ↗
31. Hongsirikarn · J. Power Sources · 2011 · 196 · 64410.1016/j.jpowsour.2010.07.080 ↗
32. Okada · J. Phys. Chem. B · 1999 · 103 · 331510.1021/jp983762d ↗
33. Okada · J. Electroanal. Chem. · 1998 · 442 · 13710.1016/S0022-0728(97)00499-3 ↗
34. Okada · J. Phys. Chem. B · 2002 · 106 · 126710.1021/jp013195l ↗
35. Wang · Int. J. Hydrogen Energy · 2008 · 33 · 228310.1016/j.ijhydene.2008.01.052 ↗
36. Iojoiu · J. Electrochem. Soc. · 2007 · 154 · B111510.1149/1.2775282 ↗
37. Yu · Phys. Chem. Chem. Phys. · 2003 · 5 · 61110.1039/b209020a ↗
38. Fernandes · J. Power Sources · 2009 · 193 · 54710.1016/j.jpowsour.2009.04.038 ↗
39. Inaba · Electrochem. Solid-State Lett. · 2004 · 7 · A47410.1149/1.1814595 ↗
40. Teranishi · Electrochem. Solid State Lett. · 2006 · 9 · A47510.1149/1.2266163 ↗
41. Huang · Chem. Phys. Lett. · 2003 · 371 · 8010.1016/S0009-2614(03)00259-8 ↗
42. Mittal · Electrochem. Solid-State Lett. · 2006 · 9 · A29910.1149/1.2192696 ↗
43. Okada · J. Electrochem. Soc. · 1997 · 144 · 274410.1149/1.1837890 ↗
44. Chen · Polym. Degrad. Stab. · 2009 · 94 · 143610.1016/j.polymdegradstab.2009.05.016 ↗
45. Sethuraman · J. Electrochem. Soc. · 2008 · 155 · B11910.1149/1.2806798 ↗
46. Bosnjakovic · J. Phys. Chem. B. · 2004 · 108 · 433210.1021/jp037519c ↗
47. Ghassemzadeh · J. Power Sources · 2009 · 186 · 33410.1016/j.jpowsour.2008.10.004 ↗
48. Wind · J. Power Sources · 2002 · 105 · 25610.1016/S0378-7753(01)00950-8 ↗
49. Kinumoto · J. Power Sources · 2006 · 158 · 122210.1016/j.jpowsour.2005.10.043 ↗
50. Halseid · J. Electrochem. Soc. · 2004 · 151 · A38110.1149/1.1641035 ↗
51. Mauritz · Chem. Rev. · 2004 · 104 · 453510.1021/cr0207123 ↗
52. Gonzáalez-Lafont · Int. J. Quantum Chem. · 1986 · 29 · 137310.1002/qua.560290532 ↗
53. Bosnjakovic · J. Phys. Chem. B · 2004 · 108 · 433210.1021/jp037519c ↗
54. Malik · Ind. Eng. Chem. Res. · 2009 · 48 · 696110.1021/ie900681n ↗
55. Kreuer · Electrochim. Acta · 1998 · 43 · 128110.1016/S0013-4686(97)10031-7 ↗
56. Lott · Electrochem. Solid State Lett. · 2005 · 8 · A51310.1149/1.2017768 ↗
57. Springer · J. Electrochem. Soc. · 1991 · 138 · 233410.1149/1.2085971 ↗