Nanocomposite electrolytes with fumed silica in poly(methyl methacrylate): thermal, rheological and conductivity studies
Source abstract
Abstract
Abstract Composite polymer electrolytes (CPEs), were prepared by adding hydrophilic fumed silica in different proportions upto 5 wt.% to gel polymeric electrolyte (GPE) comprising liquid electrolyte (1 M LiClO 4 in propylene carbonate) immobilized with 15 wt.% poly(methyl methacrylate) (PMMA). The effect of fumed silica content in the CPEs on the ionic conductivity and viscosity over a wide temperature range was investigated. The resultant CPEs showed room temperature conductivity ( σ 25 ) as high as 3.8 mS cm −1 along with viscosity value of 3700 P for 2 wt.% SiO 2 addition. Fumed silica addition both to the liquid electrolyte and to the GPE exhibits similar conductivity behaviour and this suggests a passive role of PMMA. The shear thinning behaviour, pointing towards easy processablity, high thermal stability and low volatility, makes these CPEs potential candidates as solid-like electrolytes for electrochemical devices.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advanced battery technologies research · Fuel Cells and Related Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Abraham · 1993
2. Swierczynski · Chem. Mater. · 2001 · 13 · 156010.1021/cm001178n ↗
3. Song · J. Power Sources · 1999 · 77 · 18310.1016/S0378-7753(98)00193-1 ↗
4. Appetechi · Electrochem. Commun. · 2001 · 3 · 28110.1016/S1388-2481(01)00137-0 ↗
5. Deepa · Electrochim. Acta · 2004 · 49 · 37310.1016/j.electacta.2003.08.020 ↗
6. Ahmad · Ionics · 2003 · 5–6 · 43910.1007/BF02376598 ↗
7. Agnihotry · Electrochim. Acta · 2004 · 49 · 234310.1016/j.electacta.2004.01.015 ↗
8. Yarovoy · Solid State Ionics · 1999 · 118 · 30110.1016/S0167-2738(98)00442-1 ↗
9. Zhou · J. Electrochem. Soc. · 2002 · 149 · 112110.1149/1.1496483 ↗
10. Walls · J. Electrochem. Soc. · 2003 · 150 · E16510.1149/1.1544635 ↗
11. Walls · Electrochim. Acta · 2003 · 48 · 207110.1016/S0013-4686(03)00187-7 ↗
12. Adehar · Electrochim. Acta · 2003 · 48 · 209910.1016/S0013-4686(03)00191-9 ↗
13. Yeager · J. Phys. Chem. · 1973 · 77 · 240710.1021/j100639a008 ↗
14. Battisti · J. Phys. Chem. · 1993 · 97 · 582610.1021/j100124a007 ↗
15. Fritz · J. Power Sources · 1993 · 41 · 25310.1016/0378-7753(93)80043-O ↗
16. Technical Bulletins, Cabot Sanmar Ltd., India, 1999.
17. Fritz · J. Power Sources · 1992 · 37 · 31510.1016/0378-7753(92)85015-3 ↗
18. Deepa · Solid State Ionics · 2002 · 152–153 · 25310.1016/S0167-2738(02)00307-7 ↗
19. Bohnke · J. Electrochem. Soc. · 1992 · 139 · 186210.1149/1.2069512 ↗
20. Cazzanelli · Electrochim. Acta · 1995 · 40 · 237910.1016/0013-4686(95)00198-N ↗
21. Stallworth · Electrochim. Acta · 1995 · 40 · 213710.1016/0013-4686(95)00153-6 ↗
22. Johansson · J. Phys. Chem. B · 2003 · 107 · 1262210.1021/jp035138t ↗
23. Raghavan · Chem. Mater. · 1998 · 10 · 24410.1021/cm970406j ↗
24. Aymonier · Chem. Mater. · 2003 · 15 · 487410.1021/cm031049h ↗
25. Holland · Polymer · 2001 · 42 · 482510.1016/S0032-3861(00)00923-X ↗
26. Grillone · J. Electrochem. Soc. · 1999 · 146 · 2710.1149/1.1391559 ↗