Abstract

Abstract Carbon supported Pt and Pt–Ni (1:1) nanoparticles were prepared by reduction of metal precursors with NaBH 4 . XRD analysis indicated that only a small amount of Ni alloyed with Pt (Ni atomic fraction in the alloy about 0.05). The as-prepared catalysts were submitted to chronoamperometry (CA) measurements to evaluate their activity for the oxygen reduction reaction (ORR). CA measurements showed that the ORR activity of the as-prepared Ni-containing catalyst was higher than that of pure Pt. Then, their stability was studied by submitting these catalysts to durability tests involving either 30 h of constant potential (CP, 0.8 V vs. RHE) operation or repetitive potential cycling (RPC, 1000 cycles) between 0.5 and 1.0 V vs. RHE at 20 mV s −1 . After 30 h of CP operation at 0.8 V vs. RHE, loss of all non-alloyed Ni, partial dissolution of the Pt–Ni alloy and an increase of the crystallite size was observed for the Pt–Ni/C catalyst. The ORR activity of the Pt–Ni/C catalyst was almost stable, whereas the ORR activity of Pt/C slightly decreased with respect to the as-prepared catalyst. Loss of all non-alloyed and part of alloyed Ni was observed for the Pt–Ni/C catalyst following repetitive potential cycling. Conversely to the results of 30 h of CP operation at 0.8 V vs. RHE, after RPC the ORR activity of Pt–Ni/C was lower than that of both as-prepared Pt–Ni/C and cycled Pt/C. This result was explained in terms of Pt surface enrichment and crystallite size increase for the Pt–Ni/C catalyst.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials · Conducting polymers and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Polymer electrolyte fuel cells
2. Jalan · J. Electrochem. Soc. · 1983 · 130 · 229910.1149/1.2119574 ↗
3. Beard · J. Electrochem. Soc. · 1986 · 133 · 183910.1149/1.2109033 ↗
4. Paffett · J. Electrochem. Soc. · 1988 · 135 · 143110.1149/1.2096016 ↗
5. Beard · J. Electrochem. Soc. · 1990 · 137 · 336810.1149/1.2086223 ↗
6. Mukerjee · J. Electroanal. Chem. · 1993 · 357 · 20110.1016/0022-0728(93)80380-Z ↗
7. Watanabe · J. Electrochem. Soc. · 1994 · 141 · 265910.1149/1.2059162 ↗
8. Toda · J. Electrochem. Soc. · 1999 · 146 · 375010.1149/1.1392544 ↗
9. Min · Electrochim. Acta · 2000 · 45 · 421110.1016/S0013-4686(00)00553-3 ↗
10. Paulus · J. Phys. Chem. B · 2002 · 106 · 418110.1021/jp013442l ↗
11. Antolini · Electrochim. Acta · 2002 · 48 · 26310.1016/S0013-4686(02)00644-8 ↗
12. Mukerjee · J. Electrochem. Soc. · 1995 · 142 · 140910.1149/1.2048590 ↗
13. Stamenkovic · J. Phys. Chem. B · 2002 · 106 · 1197010.1021/jp021182h ↗
14. Stamenkovic · J. Electroanal. Chem. · 2003 · 554–555 · 19110.1016/S0022-0728(03)00177-3 ↗
15. Drillet · Electrochim. Acta · 2002 · 47 · 198310.1016/S0013-4686(02)00027-0 ↗
16. Wakabayashi · J. Phys. Chem. B · 2005 · 109 · 583610.1021/jp046204+ ↗
17. Yang · J. Phys. Chem. B · 2004 · 108 · 1102410.1021/jp049034+ ↗
18. Antolini · J. Power Sources · 2006 · 160 · 95710.1016/j.jpowsour.2006.03.006 ↗
19. Colon-Mercado · Electrochem. Commun. · 2004 · 6 · 79510.1016/j.elecom.2004.05.028 ↗
20. Zignani · J. Power Sources · 2008 · 182 · 8310.1016/j.jpowsour.2008.03.061 ↗
21. Antolini · Mater. Chem. Phys. · 2003 · 78 · 56310.1016/S0254-0584(02)00389-9 ↗
22. McBreen · Langmuir · 1987 · 3 · 42810.1021/la00075a027 ↗
23. Tolentino · J. Synchrotron Radiat. · 1998 · 5 · 52110.1107/S0909049597015264 ↗
24. Ressler · J. Phys. IV · 1997 · C2 · 269
25. Pandya · J. Electrochem. Soc. · 1990 · 137 · 38310.1149/1.2086450 ↗
26. van Zon · J. Chem. Phys. · 1985 · 82 · 574210.1063/1.448563 ↗
27. Antolini · Appl. Catal. B · 2006 · 63 · 13710.1016/j.apcatb.2005.09.014 ↗
28. Endo · Electrochim. Acta · 2004 · 49 · 250310.1016/j.electacta.2004.01.025 ↗
29. Antolini · Electrochem. Solid State Lett. · 2005 · 8 · A22610.1149/1.1870632 ↗
30. Antolini · J. Power Sources · 2006 · 155 · 16110.1016/j.jpowsour.2005.05.009 ↗
31. Mukerjee · J. Phys. Chem. · 1995 · 99 · 457710.1021/j100013a032 ↗
32. Mukerjee · J. Electroanal. Chem. · 1998 · 448 · 16310.1016/S0022-0728(97)00018-1 ↗
33. Antolini · Int. J. Hydrogen Energy · 2005 · 30 · 121310.1016/j.ijhydene.2005.05.001 ↗
34. Borup · J. Power Sources · 2006 · 163 · 7610.1016/j.jpowsour.2006.03.009 ↗
35. Han · Electrochem. Commun. · 2007 · 9 · 31710.1016/j.elecom.2006.09.027 ↗
36. Triaca · J. Appl. Electrochem. · 1990 · 20 · 34710.1007/BF01076040 ↗
37. Burke · Electrochim. Acta · 1990 · 36 · 96710.1016/0013-4686(90)90029-Y ↗
38. Burke · Electrochim. Acta · 1991 · 37 · 4310.1016/0013-4686(92)80010-J ↗
39. Burke · J. Electroanal. Chem. · 1982 · 137 · 17510.1016/0022-0728(82)85078-X ↗
40. Kinoshita · J. Electroanal. Chem. Interfacial Electrochem. · 1973 · 48 · 15710.1016/S0022-0728(73)80257-8 ↗
41. Burke · J. Electroanal. Chem. · 1980 · 112 · 24710.1016/S0022-0728(80)80406-2 ↗
42. Hu · Electrochim. Acta · 1999 · 44 · 272710.1016/S0013-4686(98)00400-9 ↗