Local impact of humidification on degradation in polymer electrolyte fuel cells
Source abstract
Abstract
Abstract The water level in a polymer electrolyte membrane fuel cell (PEMFC) affects the durability as is seen from the degradation processes during operation a PEMFC with fully- and nonhumidified gas streams as analyzed using an in-situ segmented cell for local current density measurements during a 300 h test operating under constant conditions and using ex situ SEM/EDX and XPS post-test analysis of specific regions. The impact of the RH on spatial distribution of the degradation process results from different water distribution giving different chemical environments. Under nonhumidified gas streams, the cathode inlet region exhibits increased degradation, whereas with fully humidified gases the bottom of the cell had the higher performance losses. The degradation and the degree of reversibility produced by Pt dissolution, PTFE defluorination, and contaminants such as silicon (Si) and nickel (Ni) were locally evaluated.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advancements in Solid Oxide Fuel Cells
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (83)
Show source-provided references
1. Kurtz · 2015
2. U.S. Department of Energy (DOE) · 2013
3. Evaluation of reversible and irreversible degradation rates of polymer electrolyte membrane fuel cells tested in automotive conditions10.1016/j.jpowsour.2016.07.049 ↗
4. Effect of relative humidity on oxygen reduction kinetics in a PEMFC10.1149/1.1897368 ↗
5. Operating proton exchange membrane fuel cells without external humidification of the reactant gases10.1149/1.1837893 ↗
6. Large-scale current fluctuations in PEM fuel cells operating with reduced feed stream humidification10.1016/j.jpowsour.2003.09.067 ↗
7. PEMFC operation failure under severe dehydration10.1016/j.ijhydene.2011.11.059 ↗
8. Performance equations of proton exchange membrane fuel cells with feeds of varying degrees of humidification10.1016/j.electacta.2011.12.079 ↗
9. Operation of a proton-exchange membrane fuel cell under non-humidified conditions using thin cast Nafion membranes with different gas-diffusion media10.1016/j.jpowsour.2005.06.023 ↗
10. Electrochemical analysis of polymer electrolyte membrane fuel cell operated with dry-air feed10.1016/j.jpowsour.2009.04.027 ↗
11. An experimental study on water transport through the membrane of a PEFC operating in the dead-end mode10.1016/j.ijhydene.2009.07.010 ↗
12. The dynamic response of PEM fuel cells to changes in load10.1016/j.ces.2004.10.033 ↗
13. Oscillations of PEM fuel cells at low cathode humidification10.1016/j.jelechem.2010.04.005 ↗
14. Oscillation of PEFC under low cathode humidification: effect of gravitation and bipolar plate design10.1149/05801.0209ecst ↗
15. Experimental study on water transport coefficient in proton exchange membrane fuel cell10.1016/j.jpowsour.2009.01.038 ↗
16. Aging mechanisms and lifetime of PEFC and DMFC10.1016/j.jpowsour.2003.09.033 ↗
17. Degradation study of MEA for PEMFCs under low humidity conditions10.1149/1.1739314 ↗
18. Lifetime behavior of a PEM fuel cell with low humidification of feed stream10.1039/B412600A ↗
19. In situ analysis of performance degradation of a PEMFC under nonsaturated humidification10.1149/1.1854781 ↗
20. Mechanical endurance of polymer electrolyte membrane and PEM fuel cell durability10.1002/polb.20863 ↗
21. Membrane degradation at catalyst layer edges in PEMFC MEAs10.1149/1.2789791 ↗
22. Membrane degradation in polymer electrolyte fuel cells under low humidification conditions
23. Durability of perfluorosulfonic acid and hydrocarbon membranes: effect of humidity and temperature10.1149/1.2806798 ↗
24. The effect of relative humidity on membrane degradation rates and mechanisms in proton exchange membrane fuel cells10.1149/1.2811696 ↗
25. Mechanisms of membrane degradation
26. Dissolution and migration of platinum after long-term operation of a polymer electrolyte fuel cell under various conditions10.1016/j.jpowsour.2008.05.062 ↗
27. Degradation of polymer-electrolyte membranes in fuel cells10.1149/1.3095466 ↗
28. Membrane degradation behavior during open-circuit voltage hold test10.1149/1.2741129 ↗
29. Degradation of perfluorinated membranes having intentionally formed Pt-Band10.1149/1.2982012 ↗
30. Membrane degradation mechanism during open-circuit voltage hold test10.1016/j.jpowsour.2008.03.078 ↗
31. The effect of platinum in a Nafion membrane on the durability of the membrane under fuel cell conditions10.1016/j.jpowsour.2010.02.043 ↗
32. Nafion degradation in PEFCs from end plate iron contamination10.1016/S0013-4686(03)00026-4 ↗
33. Durability of perfluorinated ionomer membrane against hydrogen peroxide10.1016/j.jpowsour.2005.10.043 ↗
34. Gas crossover and membrane degradation in polymer electrolyte fuel cells10.1016/j.electacta.2006.03.008 ↗
35. Effects of operating parameters on hydrogen crossover rate through Nafion® membranes in polymer electrolyte membrane fuel cells10.1016/j.renene.2013.01.046 ↗
36. Gas permeation through water-swollen hydrogel membranes10.1016/j.memsci.2007.10.032 ↗
37. Surface-oxide growth at platinum electrodes in aqueous H2SO4
38. Simulation of anodic Pt oxide growth10.1016/S0022-0728(96)04813-9 ↗
39. A surface-electrochemical basis for the direct logarithmic growth law for initial stages of extension of anodic oxide films formed at noble metals10.1063/1.459319 ↗
40. Effect of voltage on platinum dissolution10.1149/1.2180536 ↗
41. Dissolution mechanism of platinum in sulfuric acid solution10.1149/2.017212jes ↗
42. Kinetic model of platinum dissolution in PEMFCs10.1149/1.1613669 ↗
43. Investigation of platinum oxidation in PEM fuel cells at various relative humidities10.1149/1.2372230 ↗
44. The effect of humidity and oxygen partial pressure on degradation of Pt/C catalyst in PEM fuel cell10.1016/j.electacta.2008.10.008 ↗
45. Hydrogen peroxide formation rates in a PEMFC anode and cathode10.1149/1.2801980 ↗
46. Effect of elevated temperature and reduced relative humidity on ORR kinetics for PEM fuel cells10.1149/1.1984351 ↗
47. Analysis of the influence of temperature and gas humidity on the performance stability of polymer electrolyte membrane fuel cells10.1149/2.0071603jes ↗
48. Measurement of the distributions of local current density and local ionic resistance of PEFC
49. Evaluation of a 2.5 kWel automotive low temperature PEM fuel cell stack with extended operating temperature range up to 120°C10.1016/j.jpowsour.2015.10.056 ↗
50. Segmented cells as tool for development of fuel cells and error prevention/prediagnostic in fuel cell stacks10.1016/j.jpowsour.2007.03.055 ↗
51. Self-humidifying polymer electrolyte membranes for fuel cells10.1149/1.1837307 ↗
52. Polymer electrolyte membranes incorporated with nanometer-size particles of Pt and/or metal-oxides: experimental analysis of the self-humidification and suppression of gas-crossover in fuel cells10.1021/jp973477e ↗
53. Preparation of highly dispersed SiO2 and Pt particles in Nafion®112 for self-humidifying electrolyte membranes in fuel cells10.1016/j.electacta.2005.11.012 ↗
54. An ultrathin self-humidifying membrane for PEM fuel cell application: fabrication, characterization, and experimental analysis10.1021/jp061955s ↗
55. Investigation of PEMFC operation above 100 °C employing perfluorosulfonic acid silicon oxide composite membranes10.1016/S0378-7753(02)00086-1 ↗
56. Function and characterization of metal oxide-nafion composite membranes for elevated-temperature H 2/O 2 PEM fuel cells10.1021/cm051781b ↗
57. Water-retention effect of composite membranes with different types of nanometer silicon dioxide10.1149/1.2976793 ↗
58. Pt/SiO2 catalyst as an addition to Nafion/PTFE self-humidifying composite membrane10.1016/j.jpowsour.2006.03.068 ↗
59. Advanced mesostructured hybrid silica-nafion membranes for high-performance PEM fuel cell10.1021/cm070929j ↗
60. Effect of SiO2 on the dynamics of proton conducting [Nafion/(SiO2)X] composite membranes: a solid-state 19F NMR study10.1039/c0cp02316g ↗
61. Degradation of sealings for PEFC test cells during fuel cell operation10.1016/j.jpowsour.2003.09.017 ↗
62. Performance and lifetime analysis of the kW-class PEMFC stack10.1016/S0378-7753(01)01032-1 ↗
63. Degradation of silicone rubber under compression in a simulated PEM fuel cell environment10.1016/j.jpowsour.2007.05.026 ↗
64. Degradation characteristics of elastomeric gasket materials in a simulated PEM fuel cell environment10.1007/s11665-008-9233-5 ↗
65. Durability testing of silicone materials for PEMFC use10.5254/rct.13.88931 ↗
66. XPS investigation of the PTFE induced hydrophobic properties of electrodes for low temperature fuel cells10.1016/j.apsusc.2005.02.007 ↗
67. Beamson · 1992
68. The effect of humidity on the degradation of Nafion membrane10.1016/j.polymdegradstab.2009.05.016 ↗
69. Effect of diphenyl siloxane on the catalytic activity of Pt on carbon10.1149/1.2787870 ↗
70. Oxygen reduction kinetics at platinum electrodes covered with perfluorinated ionomer in the presence of impurity cations Fe3+, Ni2+ and Cu2+10.1039/b002566f ↗
71. The effect of impurity cations on the oxygen reduction kinetics at platinum electrodes covered with perfluorinated ionomer10.1021/jp010822y ↗
72. Impact of metal cations on the electrocatalytic properties of Pt/C nanoparticles at multiple phase interfaces10.1039/c2cp42191g ↗
73. Cationic contamination effects on polymer electrolyte membrane fuel cell performance10.1149/1.3610986 ↗
74. The effect of impurity cations on the transport characteristics of perfluorosulfonated ionomer membranes10.1021/jp983762d ↗
75. Performance impact of cationic contaminants
76. Ion and water transport characteristics of perfluorosulfonated ionomer membranes with H+ and alkali metal cations10.1021/jp013195l ↗
77. Contaminant absorption and conductivity in polymer electrolyte membranes10.1016/j.jpowsour.2005.01.064 ↗
78. In situ metal ion contamination and the effects on proton exchange membrane fuel cell performance10.1016/j.jpowsour.2011.01.086 ↗
79. Baldwin · 1989
80. Advanced materials for improved PEMFC performance and life10.1016/j.jpowsour.2004.01.023 ↗
81. Review: durability and degradation issues of PEM fuel cell components10.1002/fuce.200700053 ↗
82. XPS analysis of the degradation of Nafion10.1007/s002160051454 ↗
83. Applications of ESCA to polymer chemistry