Silicon/graphite composites as an anode material for lithium ion batteries
Source abstract
Abstract
Mixed silicon–graphite composites have been prepared by means of mechanical milling process. Their micro-heterogeneous structure is considered responsible for electrode failures. A fingerprint of this process is seen by cycling the carbonaceous component of the composite in an electrolyte containing small amount of propylene–carbonate (PC). Local voltage drops close to 0 V (versus Li metal) resulted in local electrode mechanical deterioration. In the presence of silicon particles such local disorders would lead to a loose interparticle contact (zones called dead spots). Deterioration pattern of the mixed composite electrode may be considered as a set of ‘dead spots’ spreading across the electrode as the cycling proceeds. Hence, a careful optimization is necessary in order to fabricate composite electrode giving minimum local disorders and having satisfactory cycling performance.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Graphene research and applications · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. Toyoguchi · 1983 · 205
2. Toyoguchi · 1986 · 113
3. 1988 · 659
4. Takehara · J. Power Sources · 1989 · 26 · 25710.1016/0378-7753(89)80034-5 ↗
5. Nishio · 1999
6. Yamaki · 1999
7. Nagaura · Prog. Batteries Solar Cells · 1990 · 9 · 209
8. Nagaura · Prog. Batteries Solar Cells · 1991 · 10 · 218
9. Huggins · Ionics · 2000 · 6 · 5710.1007/BF02375547 ↗
10. Yoshio · J. Electrochem. Soc. · 2002 · 149 · A159810.1149/1.1518988 ↗
11. Yang · Electrochem. Commun. · 2002 · 4 · 89310.1016/S1388-2481(02)00483-6 ↗
12. Dimov · 2003
13. Dimov · J. Power Sources · 2004 · 136 · 10810.1016/j.jpowsour.2004.05.012 ↗