journal article·2017-02

Increasing the durability of Li-ion batteries by means of manganese ion trapping materials with nitrogen functionalities

Anjan Banerjee, Baruch Ziv, Shalom Luski, Doron Aurbach, Ion C. Halalay

Publisher page

Abstract

Abstract Manganese dissolution from positive electrodes seriously reduces the useful life of Li-ion batteries, especially with positive electrode materials having spinel phases. We show herein that Mn ion trapping separators containing inexpensive mass-produced materials may dramatically increase the life of Li-ion batteries. LiMn2O4-graphite cells containing these materials and a LiPF6 based electrolyte solution display excellent capacity retention during cycling at both room and elevated temperatures, over baseline cells with plain separators. After 30 days of cycling at 55 °C and C/5 rate, LiMn2O4-graphite cells containing three different Mn-trapping materials with nitrogen functionalities retain between 75% and 125% more of the initial capacity than the baseline cells. Mn amounts in graphite negative electrodes from cells with the functional separators are 13–21 times lower than in baseline cells. LiMn2O4 lattice shrinkage in cells with functionalized separators is negligible compared to baseline cells, indicating major reductions in the loss of electrochemically active Li+ ions and increased stability of the LiMn2O4 crystal lattice.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Du Pasquier · J. Electrochem. Soc. · 1999 · 146 · 42810.1149/1.1391625 ↗
2. Amatucci · J. Power Sources · 1997 · 69 · 1110.1016/S0378-7753(97)02542-1 ↗
3. Lu · Nat. Comm. · 2014 · 5 · 569310.1038/ncomms6693 ↗
4. Mori · J. Power Sources · 1997 · 68 · 5910.1016/S0378-7753(97)02619-0 ↗
5. Aurbach · J. Phys. Chem. B · 1997 · 101 · 219510.1021/jp962815t ↗
7. Ein-Eli · Electrochem. Solid State Lett. · 1999 · 2 · 21210.1149/1.1390787 ↗
8. Aurbach · J. Power Sources · 2000 · 89 · 20610.1016/S0378-7753(00)00431-6 ↗
9. Verma · Electrochim. Acta · 2010 · 55 · 633210.1016/j.electacta.2010.05.072 ↗
10. Amatucci · Electrochim. Acta · 1999 · 45 · 25510.1016/S0013-4686(99)00209-1 ↗
11. Gummow · Solid State Ion. · 1994 · 69 · 5910.1016/0167-2738(94)90450-2 ↗
12. Wang · Solid State Ion. · 1999 · 120 · 9510.1016/S0167-2738(98)00554-2 ↗
13. Choi · J. Electrochem. Soc. · 2006 · 153 · A176010.1149/1.2219710 ↗
14. Li · Electrochim. Acta · 2006 · 51 · 387210.1016/j.electacta.2005.11.015 ↗
15. Jung · Adv. Mater. · 2010 · 22 · 217210.1002/adma.200903951 ↗
16. Yi · Ion. (Kiel) · 2009 · 15 · 77910.1007/s11581-009-0373-x ↗
17. Xu · Chem. Rev. · 2004 · 104 · 430310.1021/cr030203g ↗
18. Xu · Chem. Rev. · 2014 · 114 · 1150310.1021/cr500003w ↗
19. Amatucci · Electrochim. Acta · 1999 · 45 · 25510.1016/S0013-4686(99)00209-1 ↗
20. Ziv · J. Electrochem. Soc. · 2014 · 161 · A121310.1149/2.0091409jes ↗
21. Li · J. Power Sources · 2014 · 272 · 113410.1016/j.jpowsour.2014.04.073 ↗
22. Banerjee · J. Electrochem. Soc. · 2016 · 163 · A108310.1149/2.0081607jes ↗
23. Banerjee · Adv. Energy Mat. · 2016
24. Ochida · J. Electrochem. Soc. · 2013 · 160 · A41010.1149/2.021303jes ↗
25. Kim · Electrochem. Comm. · 2015 · 58 · 2510.1016/j.elecom.2015.05.019 ↗
26. Domi · J. Electrochem. Soc. · 2016 · 163 · A160710.1149/2.0601608jes ↗
27. Liu · Chem. Commun. · 2012 · 48 · 985810.1039/c2cc34529c ↗
28. Woo · J. Electrochem. Soc. · 2013 · 160 · A223410.1149/2.092311jes ↗
29. Kim · Adv. Energy Mat. · 2015 · 5
30. Miao · J. Power Sources · 2008 · 184 · 42010.1016/j.jpowsour.2008.03.045 ↗
31. Shilina · Anal. Chem. · 2016 · 88 · 444010.1021/acs.analchem.6b00204 ↗
32. Huang · J. Solid State Electrochem. · 2013 · 17 · 59110.1007/s10008-012-1891-4 ↗
33. Huang · J. Power Sources · 2012 · 216 · 21610.1016/j.jpowsour.2012.05.019 ↗