The study of electrochemical properties and lithium deposition of graphite at low temperature
Source abstract
Abstract
Abstract The electrochemical properties of graphite with various degrees of graphitization, contents of rhombohedral phase, and surface areas were electrochemically investigated at 25 °C and −5 °C. The degree of graphitization and the amount of rhombohedral phase affected the samples’ lithium intercalation/deintercalation and surface deposition. The reductions of electrolyte conductivity and lithium ion diffusion in the graphite interlayer at −5 °C lowered the graphite's capacity. Lithium deposition also occurred on the graphite's surface. Highly graphitized samples were affected greatly by temperature, showing large capacity loss at low temperature. Increased rhombohedral phase facilitated lithium deposition on the graphite's surface as lithium ions did not insert into the graphite interlayers and accumulated at its edged planes. Increasing the pathways for lithium ion intercalation could facilitate lithium intercalation and reduce lithium deposition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Graphene research and applications · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Noel · J. Power Sources · 1998 · 72 · 5310.1016/S0378-7753(97)02675-X ↗
2. Dahn · Electrochim. Acta · 1993 · 38 · 117910.1016/0013-4686(93)80048-5 ↗
3. Smart · J. Electrochem. Soc. · 1999 · 146 · 48610.1149/1.1391633 ↗
4. Shiao · J. Power Sources · 2000 · 87 · 16710.1016/S0378-7753(99)00470-X ↗
5. Plichta · J. Power Sourecs · 2000 · 88 · 19210.1016/S0378-7753(00)00367-0 ↗
6. Plichta · J. Power Sources · 2001 · 94 · 16010.1016/S0378-7753(00)00578-4 ↗
7. Herreyre · J. Power Sources · 2001 · 97–98 · 57610.1016/S0378-7753(01)00670-X ↗
8. Huang · J. Electrochem. Soc. · 2000 · 147 · 48610.1149/1.1393221 ↗
9. Lin · Electrochem. Solid-State Lett. · 2001 · 4 · A7110.1149/1.1368736 ↗
10. Zhang · J. Power Sources · 2002 · 110 · 217
11. Zhang · Electrochim. Acta · 2002 · 48 · 24110.1016/S0013-4686(02)00620-5 ↗
12. Honbo · J. Power Sources · 2009 · 189 · 33710.1016/j.jpowsour.2008.08.048 ↗
13. Reynier · J. Power Sources · 2009 · 189 · 60210.1016/j.jpowsour.2008.09.088 ↗
14. Park · J. Power Sources · 2008 · 189 · 60210.1016/j.jpowsour.2008.09.088 ↗
15. Franklin · Acta Crystallogr. · 1951 · 4 · 23510.1107/S0365110X51000842 ↗
16. Guerard · Carbon · 1975 · 13 · 33710.1016/0008-6223(75)90040-8 ↗
17. Ohzuku · J. Electrochem. Soc. · 1993 · 140 · 249010.1149/1.2220849 ↗
18. Dahn · Phys. Rev. B · 1991 · 44 · 917010.1103/PhysRevB.44.9170 ↗
19. Hardwick · Electrochim. Acta · 2007 · 52 · 488410.1016/j.electacta.2006.12.081 ↗
20. Wang · J. Power Sources · 1998 · 76 · 110.1016/S0378-7753(98)00114-1 ↗
21. Shi · J. Power Sources · 1997 · 68 · 29110.1016/S0378-7753(96)02562-1 ↗
22. Cao · J. Electrochem. Soc. · 2000 · 147 · 357910.1149/1.1393942 ↗
23. Dahn · Electrochim. Acta · 1993 · 38 · 117910.1016/0013-4686(93)80048-5 ↗
24. Qiu · Solid State Ionics · 1999 · 121 · 7310.1016/S0167-2738(98)00531-1 ↗
25. Shi · J. Electrochem. Soc. · 1996 · 143 · 346610.1149/1.1837238 ↗
26. Hardwick · Solid State Ionics · 2006 · 177 · 280110.1016/j.ssi.2006.03.032 ↗
27. Kohs · J. Power Sources · 2003 · 119–121 · 52810.1016/S0378-7753(03)00278-7 ↗
28. Spahr · J. Power Sources · 2006 · 153 · 30010.1016/j.jpowsour.2005.05.032 ↗
29. Winter · J. Electrochem. Soc. · 1998 · 145 · 42810.1149/1.1838281 ↗
30. Sphar · J. Power Sourecs · 2003 · 119–121 · 543
31. Yazami · J. Power Sources · 1993 · 43–44 · 59
32. Yamaguchi · J. Power Sources · 2001 · 97–98 · 15910.1016/S0378-7753(01)00739-X ↗
33. Mabuvhi · J. Electrochem. Soc. · 1995 · 142 · 104110.1149/1.2044128 ↗
34. Yoshio · 2009