Abstract
Abstract Surface morphology changes of LiMn 2 O 4 thin film positive electrodes in lithium-ion batteries after repeated potential cycling or storage at elevated temperatures were observed by in situ atomic force microscopy (AFM) to elucidate the origin of capacity fading of LiMn 2 O 4 . After repeated potential cycling in the overall potential range from 3.50 to 4.30 V at elevated temperatures, the entire thin film surface was covered with small round-shaped particles accompanied by capacity fading of the electrode, while no significant changes were observed at 25 °C. The discharge capacity decreased more significantly when cycled in the lower potential range (3.81–4.07 V) than when cycled in the higher potential range (4.04–4.30 V). After storage at elevated temperatures at a depth of discharge (DOD) of 75%, which is located in the lower potential range, similar surface morphology changes were observed. In addition, discharge capacity markedly decreased, and the crystallinity of the LiMn 2 O 4 thin film was lowered after storage. Hence, the observed changes in morphology at elevated temperatures are closely related to capacity fading of the LiMn 2 O 4 thin film. The loss of crystallinity was caused by the formation of small particles on the LiMn 2 O 4 surface, which would be accelerated on the LiMn 2 O 4 surface in contact with an electrolyte solution through some kind of dissolution/precipitation reaction.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Supercapacitor Materials and Fabrication
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Winter · Adv. Mater. · 1998 · 10 · 72510.1002/(SICI)1521-4095(199807)10:10<725::AID-ADMA725>3.0.CO;2-Z ↗
2. Inaba · Langumir · 1996 · 12 · 153510.1021/la950848e ↗
3. Aurbach · J. Power Sources · 2000 · 89 · 20610.1016/S0378-7753(00)00431-6 ↗
4. Ohzuku · J. Electrochem. Soc. · 1990 · 137 · 76910.1149/1.2086552 ↗
5. Yamada · Electrochem. Commun. · 2003 · 5 · 50210.1016/S1388-2481(03)00113-9 ↗
6. Gummow · Solid State Ionics · 1994 · 69 · 5910.1016/0167-2738(94)90450-2 ↗
7. Thackeray · Electrochem. Solid-State Lett. · 1998 · 1 · 710.1149/1.1390617 ↗
8. Xia · J. Electrochem. Soc. · 1997 · 144 · 259310.1149/1.1837870 ↗
9. Inaba · J. Power Sources · 1999 · 81/82 · 55410.1016/S0378-7753(99)00215-3 ↗
10. Doi · J. Electrochem. Soc. · 2008 · 155 · A2010.1149/1.2799076 ↗
11. Jeong · J. Electrochem. Soc. · 2001 · 148 · A98910.1149/1.1387981 ↗
12. Inaba · Langmuir · 2004 · 20 · 134810.1021/la035857z ↗
13. Saitoh · J. Electrochem. Soc. · 2004 · 151 · A1710.1149/1.1630038 ↗
14. Takahashi · J. Power Sources · 2004 · 136 · 11510.1016/j.jpowsour.2004.05.014 ↗
15. Shin · Chem. Mater. · 2003 · 15 · 295410.1021/cm0341787 ↗
16. Yazami · J. Power Sources · 2006 · 153 · 25110.1016/j.jpowsour.2005.10.012 ↗
17. Manthiram · Electrochem. Solid-State Lett. · 2007 · 10 · A22810.1149/1.2754387 ↗
18. Yamane · J. Electrochem. Soc. · 2002 · 149 · A151410.1149/1.1515278 ↗
19. Li · Solid State Ionics · 2000 · 130 · 22110.1016/S0167-2738(00)00665-2 ↗
20. Li · Solid State Ionics · 2002 · 146 · 5510.1016/S0167-2738(01)01002-5 ↗