Abstract
Abstract Optimization of sintering temperature for NiO–Fe 2 O 3 composite oxide substrate was studied in order to obtain a dense substrate with smooth surface. By in situ reduction, the substrate was changed to a porous Ni–Fe alloy metal. The volumetric shrinkage and porosity of the substrate were also studied systematically with the Ni–Fe substrate reduced at different temperatures. A Sr and Mg-doped LaGaO 3 (LSGM) thin film was prepared on dense substrate by the pulsed laser deposition (PLD) method. The LSGM film with stoichiometric composition was successfully prepared under optimal deposition parameters and a target composition. Sm 0.5 Sr 0.5 CoO 3 (SSC55) cathode was prepared by the slurry coating method on the deposited film. Prepared SOFC single cell shows high power density and the maximum power density (MPD) achieved was 1.79, 0.82 and 0.29 W cm −2 at 973, 873 and 773 K, respectively. After thermal cycle from 973 to 298 K, the cell shows almost theoretical open circuit potential (1.1 V) and the power density of 1.62 W cm −2 , which is almost the same as that at first cycles. Therefore, the Ni–Fe porous metal support made by the selective reduction is highly promising as a metal anode substrate for SOFC using LaGaO 3 thin film.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Singhal · Solid State Ionics · 2002 · 152–153 · 40510.1016/S0167-2738(02)00349-1 ↗
2. Minh · Solid State Ionics · 2004 · 174 · 27110.1016/j.ssi.2004.07.042 ↗
3. Yamamoto · Electrochim. Acta · 2000 · 45 · 242310.1016/S0013-4686(00)00330-3 ↗
4. Zhu · Mater. Sci. Eng. A · 2003 · 362 · 22810.1016/S0921-5093(03)00620-8 ↗
5. Ishihara · J. Am. Chem. Soc. · 1994 · 116 · 380110.1021/ja00088a016 ↗
6. Ishihara · Chem. Commun. · 1996 · 8 · 92910.1039/cc9960000929 ↗
7. Ishihara · J. Electrochem. Soc. · 1998 · 145 · 317710.1149/1.1838783 ↗
8. Yan · Electrochem. Solid-State Lett. · 2005 · 8 · A38910.1149/1.1943568 ↗
9. Ishihara · Electrochim. Acta · 2006 · 52 · 164510.1016/j.electacta.2006.03.103 ↗
10. Chen · Solid State Ionics · 1994 · 70–71 · 10110.1016/0167-2738(94)90293-3 ↗
11. de Souza · Solid State Ionics · 1997 · 98 · 5710.1016/S0167-2738(96)00525-5 ↗
12. Lunot · 1998 · 834
13. 1999 · 333
14. Bai · Solid State Ionics · 1998 · 113–115 · 25910.1016/S0167-2738(98)00290-2 ↗
15. Phase Diagram, American Ceramic Society, Fig. 5421.