Abstract

Abstract To enhance the performance (i.e., mechanical properties and ionic conductivity) of pore-filling polymer electrolytes, titanium dioxide (TiO 2 ) nanoparticles are added to both a porous membrane and its included viscous electrolyte, poly(ethylene oxide- co -ethylene carbonate) copolymer (P(EO-EC)). A porous membrane with 10 wt.% TiO 2 shows better performance (e.g., homogeneous distribution, high uptake, and good mechanical properties) than the others studied and is therefore chosen as the matrix to prepare polymer electrolytes. A maximum conductivity of 5.1 × 10 −5 S cm −1 at 25 °C is obtained for a polymer electrolyte containing 1.5 wt.% TiO 2 in a viscous electrolyte, compared with 3.2 × 10 −5 S cm −1 for a polymer electrolyte without TiO 2 . The glass transition temperature, T g is lowered by the addition of TiO 2 (up to 1.5 wt.% in a viscous electrolyte) due to interaction between P(EO-EC) and TiO 2 , which weakens the interaction between oxide groups of the P(EO-EC) and lithium cations. The overall results indicate that the sample prepared with 10 wt.% TiO 2 for a porous membrane and 1.5 wt.% TiO 2 for a viscous electrolyte is a promising polymer electrolyte for rechargeable lithium batteries.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Supercapacitor Materials and Fabrication · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Jeon · J. Power Sources · 2005 · 143 · 21910.1016/j.jpowsour.2004.12.005 ↗
2. Jeon · J. Electrochem. Soc. · 2005 · 152 · A158310.1149/1.1939167 ↗
3. Xu · Chem. Mater. · 2001 · 13 · 57510.1021/cm000694a ↗
4. Ji · J. Power Sources · 2003 · 117 · 12410.1016/S0378-7753(03)00159-9 ↗
5. Jiang · J. Electrochem. Soc. · 2005 · 152 · A76710.1149/1.1865892 ↗
6. Ahn · J. Power Sources · 2003 · 119–121 · 42210.1016/S0378-7753(03)00264-7 ↗
7. Prosini · J. Power Sources · 1998 · 75 · 7310.1016/S0378-7753(98)00094-9 ↗
8. Appetecchi · J. Electrochem. Soc. · 2000 · 147 · 444810.1149/1.1394084 ↗
9. Borghini · J. Electrochem. Soc. · 1995 · 142 · 211810.1149/1.2044260 ↗
10. Sun · J. Electrochem. Soc. · 1999 · 146 · 167210.1149/1.1391824 ↗
11. Liao · J. Polym. Sci. Part B: Polym. Phys. · 2004 · 42 · 427210.1002/polb.20293 ↗
12. Yang · Nature · 1998 · 396 · 15210.1038/24132 ↗
13. Chung · J. Power Sources · 2001 · 97–98 · 64410.1016/S0378-7753(01)00748-0 ↗
14. Liu · J. Power Sources · 2004 · 129 · 30310.1016/j.jpowsour.2003.11.026 ↗
15. Zheng · Mater. Sci. Eng. · 2000 · B77 · 5510.1016/S0921-5107(00)00465-7 ↗
16. Kobayashi · Macromolecules · 1975 · 8 · 15810.1021/ma60044a013 ↗
17. Marand · J. Polym. Sci. Part B: Polym. Phys. · 1988 · 26 · 136110.1002/polb.1988.090260703 ↗
18. Kim · Polymer · 2002 · 43 · 395110.1016/S0032-3861(02)00215-X ↗
19. Morales · Electrochim. Acta · 1999 · 45 · 104910.1016/S0013-4686(99)00300-X ↗
20. Park · Solid State Ionics · 2003 · 159 · 11110.1016/S0167-2738(03)00025-0 ↗