Performance and testing of glass-ceramic sealant used to join anode-supported-electrolyte to Crofer22APU in planar solid oxide fuel cells
Source abstract
Abstract
Abstract This work describes the performance and testing of a glass-ceramic sealant used to join the ceramic electrolyte (anode-supported-electrolyte (ASE)) to the metallic interconnect (Crofer22APU) in planar SOFC stacks. The designed glass-ceramic sealant is a barium and boron free silica-based glass, which crystallizes by means of the heat-treatment after being deposited on substrates by the slurry technique. Joined ASE/glass-ceramic seal/Crofer22APU samples were tested for 500 h in H2–3H2O atmosphere at the fuel cell operating temperature of 800 °C. Moreover, the joined ASE/glass-ceramic seal/Crofer22APU samples were submitted to three thermal cycles each of 120 h duration, in order to evaluate the thermomechanical stability of the sealant. The microstructures and elemental distribution at Crofer22APU/glass-ceramic and ASE/glass-ceramic interfaces were investigated. SEM micrograph observations of joined samples that underwent cyclic thermal tests and exposure for 500 h in H2–3H2O atmosphere showed that the adhesion between the glass-ceramic and Crofer22APU at either interface was very good and no microstructural changes were detected at the interfacial boundaries. The study showed that the use of the glass-ceramic was successful in preventing strong adverse corrosion effects at the Crofer22APU/glass-ceramic sealant interface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Steele · Nature · 2001 · 414 · 34510.1038/35104620 ↗
2. Singh · J. Appl. Ceram. Technol. · 2007 · 4 · 13410.1111/j.1744-7402.2007.02128.x ↗
3. Antepara · J. Power Sources · 2005 · 151 · 10310.1016/j.jpowsour.2005.02.084 ↗
4. Fergus · J. Power Sources · 2005 · 147 · 4610.1016/j.jpowsour.2005.05.002 ↗
5. Jordan · Am. Ceram. Soc. Bull. · 2008 · 87 · 26
6. Weil · JOM · 2006 · 36
7. Singh · J. Mater. Eng. Perform. · 2006 · 15 · 42210.1361/105994906X117224 ↗
8. Singh · J. Appl. Ceram. Technol. · 2007 · 4 · 11910.1111/j.1744-7402.2007.02126.x ↗
9. Kim · Int. J. Hydrogen Energy · 2007 · 32 · 365510.1016/j.ijhydene.2006.08.054 ↗
10. Shiru · J. Power Sources · 2007 · 168 · 44710.1016/j.jpowsour.2007.03.014 ↗
11. Chou · J. Power Sources · 2007 · 168 · 42610.1016/j.jpowsour.2007.03.039 ↗
12. Chou · J. Power Sources · 2007 · 170 · 39510.1016/j.jpowsour.2007.03.060 ↗
13. Brochu · J. Eur. Ceram. Soc. · 2006 · 26 · 330710.1016/j.jeurceramsoc.2005.08.002 ↗
14. Smeacetto · J. Eur. Ceram. Soc. · 2008 · 28 · 61110.1016/j.jeurceramsoc.2007.07.008 ↗
15. Gosh · J. Eur. Ceram. Soc. · 2008 · 28 · 6910.1016/j.jeurceramsoc.2007.05.008 ↗
16. Meinhardt · J. Power Sources · 2008 · 182 · 18810.1016/j.jpowsour.2008.03.079 ↗
17. Kumar · Int. J. Hydrogen Energy · 2008 · 33 · 43410.1016/j.ijhydene.2007.07.049 ↗
18. Piao · J. Rare Earths · 2007 · 25 · 43410.1016/S1002-0721(07)60451-7 ↗
19. Gross · Fuel Cells Bull. · 2006 · 9 · 1210.1016/S1464-2859(06)71320-7 ↗
20. Yang · J. Electrochem. Soc. · 2003 · 150 · A109510.1149/1.1590325 ↗
21. Larsen · J. Non-Cryst. Solids · 1999 · 244 · 1610.1016/S0022-3093(98)00848-5 ↗
22. Smeacetto · J. Eur. Ceram. Soc. · 2008 · 28 · 6110.1016/j.jeurceramsoc.2007.05.006 ↗
23. Smeacetto · J. Eur. Ceram. Soc. · 2008 · 28 · 252110.1016/j.jeurceramsoc.2008.03.035 ↗
24. Yang · J. Electrochem. Soc. · 2004 · 151 · B66910.1149/1.1810393 ↗
25. Ogasawara · J. Electrochem. Soc. · 2007 · 154 · B65710.1149/1.2735919 ↗
26. Nielsen · J. Eur. Ceram. Soc. · 2007 · 27 · 181710.1016/j.jeurceramsoc.2006.05.046 ↗
27. Turkdogan · 1980
28. Essuman · Oxid. Met. · 2008 · 69 · 14310.1007/s11085-007-9090-x ↗