Comprehensive calorimetry of the thermally-induced failure of a lithium ion battery
Source abstract
Abstract
Abstract A lithium ion battery (LIB) subjected to external heat may fail irreversibly. Manifestations of this failure include venting of potentially combustible gases and aerosols followed by a rapid self-heating accompanied by ejection of the battery materials. It is important to be able to quantify the dynamics and energetics of this process to ensure safety of the energy storage systems utilizing LIBs. Here we report on development of a new experimental technique for the measurement of energetics of a thermally-induced battery failure. This technique, Copper Slug Battery Calorimetry (CSBC), was employed to investigate a widely utilized LIB of 2200 mAh capacity at various states of charge (SOC). It was shown that this techniques yields time and temperature resolved data on the rate of heat production inside the failing battery. The total energy generated inside the battery was found to increase with increasing SOC to the maximum value of 34.0 ± 1.8 kJ. To capture the energetics of flaming combustion of the materials ejected from the battery, CSBC was coupled with a cone calorimeter, which measures heat released in a non-premixed flame. The maximum amount of energy released by the battery through flaming combustion of ejected materials was found to be 97.5 ± 12.4 kJ.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Technologies Research · Advanced Battery Materials and Technologies · Advancements in Battery Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Thermal runaway caused fire and explosion of lithium ion battery10.1016/j.jpowsour.2012.02.038 ↗
2. Safety mechanisms in lithium-ion batteries10.1016/j.jpowsour.2005.12.002 ↗
3. Membranes in lithium ion batteries10.3390/membranes2030367 ↗
4. Investigations of the exothermic reactions of natural graphite anode for Li-ion batteries during thermal runaway10.1149/1.1836126 ↗
5. On safety of lithium-ion cells10.1016/S0378-7753(99)00135-4 ↗
6. DSC investigation of exothermic reactions occurring at elevated temperatures in lithium-ion anodes containing PVDF-based binders10.1016/j.jpowsour.2004.03.074 ↗
7. Thermal stability and phase transformation of electrochemically charged/discharged LiMnPO4 cathode for Li-ion batteries10.1039/c1ee01501j ↗
8. Differential scanning calorimetry study of the reactivity of carbon anodes in plastic Li-ion batteries10.1149/1.1838287 ↗
9. Roth · 2004
10. Thermal stability studies of Li-ion cells and components10.1149/1.1392458 ↗
11. Thermal abuse performance of high-power 18650 Li-ion cells10.1016/j.jpowsour.2003.09.068 ↗
12. Thermal runaway features of 18650 lithium-ion batteries for LiFePO4 cathode material by DSC and VSP210.1007/s10973-012-2573-2 ↗
13. Role of the cathode and anode in heat generation of Li-ion cells as a function of state of charge10.1016/j.jpowsour.2004.05.053 ↗
14. Comparative thermal stability of carbon intercalation anodes and lithium metal anodes for rechargeable lithium batteries10.1016/0378-7753(94)02076-F ↗
15. Simulation of abuse tolerance of lithium-ion battery packs10.1016/j.jpowsour.2006.10.013 ↗
16. Thermal characterization of a high-power lithium-ion battery: potentiometric and calorimetric measurement of entropy changes10.1016/j.energy.2013.09.028 ↗
17. Diagnostic examination of thermally abused high-power lithium-ion cells10.1016/j.jpowsour.2006.04.088 ↗
18. Accelerating rate calorimetry study on the thermal stability of lithium intercalated graphite in electrolyte. I. Experimental10.1149/1.1391893 ↗
19. Thermal explosion hazards on 18650 lithium ion batteries with a VSP2 adiabatic calorimeter
20. Thermal runaway potential of LiCoO2 and Li (Ni1/3Co1/3Mn1/3) O2 batteries determined with adiabatic calorimetry methodology10.1016/j.apenergy.2012.05.064 ↗
21. Self-reactive rating of thermal runaway hazards on 18650 lithium-ion batteries10.1007/s10973-011-1452-6 ↗
22. Micro calorimeter study on the thermal stability of lithium-ion battery electrolytes10.1016/j.jlp.2006.02.002 ↗
23. Effects of solvents and salt on the thermal stability of lithiated graphite used in lithium ion battery10.1016/j.jhazmat.2009.01.125 ↗
24. Thermal behavior of lithiated graphite with electrolyte in lithium-ion batteries10.1149/1.2139955 ↗
25. Investigation on the fire-induced hazards of Li-ion battery cells by fire calorimetry10.1039/C1EE02218K ↗
26. Thermal hazard evaluation by an accelerating rate calorimeter10.1016/0040-6031(80)85001-5 ↗
27. ASTM E 1354–09 · 1990
28. 2011
29. Incropera · 2007
30. NIST-JANAF thermochemical tables, fourth edition
31. Measuring stored chemical energy in lithium ion batteries using a bomb calorimeter