journal article·2020-12

Hydrogen clustering in bcc metals: Atomic origin and strong stress anisotropy

Jie Hou, Xiang-Shan Kong, C.S. Liu, Jun Song

Acta Materialia· Volume 201
Publisher page

Abstract

Hydrogen (H) induced damage in metals has been a long-standing woe for many industrial applications. One form of such damage is linked to H clustering, for which the atomic origin remains contended, particularly for non-hydride forming metals. In this work, we systematically studied H clustering behavior in bcc metals represented by W, Fe, Mo, and Cr, combining first-principles calculations, atomistic and Monte Carlo simulations. H clustering has been shown to be energetically favorable, and can be strongly facilitated by anisotropic stress field, dominated by the tensile component along one of the <001> crystalline directions. We showed that the stress effect can be well predicted by the continuum model based on H formation volume tensor, and that H clustering is thermodynamically possible at edge dislocations, evidenced by nanohydride formation at rather low levels of H concentration. Moreover, anisotropy in the stress effect is well reflected in nanohydride morphology around dislocations, with nanohydride growth occurring in the form of thin platelet structures that maximize one <001> tension. In particular, the <001> type edge dislocation, with the <001> tensile component maximized, has been shown to be highly effective in facilitating H aggregation, thus expected to play an important role in H clustering in bcc metals, in close agreement with recent experimental observations. This work explicitly and quantitatively clarifies the anisotropic nature of stress effect on H energetics and H clustering behaviors, offering mechanistic insights critical towards understanding H-induced damages in metals.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. On some remarkable changes produced in iron and steel by the action of hydrogen and acids10.1038/011393a0 ↗
2. Hydrogen assisted crack initiation and propagation in a nickel-based superalloy10.1016/j.actamat.2016.05.003 ↗
3. Hydrogen-enhanced fatigue crack growth in a single-edge notched tensile specimen under in-situ hydrogen charging inside an environmental scanning electron microscope10.1016/j.actamat.2019.03.032 ↗
4. Atomic mechanism and prediction of hydrogen embrittlement in iron10.1038/nmat3479 ↗
5. In situ study of the initiation of hydrogen bubbles at the aluminium metal/oxide interface10.1038/nmat4336 ↗
6. Crack and blister initiation and growth in purified iron due to hydrogen loading10.1016/j.actamat.2016.05.034 ↗
7. <001>edge dislocation nucleation mechanism of surface blistering in tungsten exposed to deuterium plasma10.1088/1741-4326/aaf32e ↗
8. Hydrogen blistering under extreme radiation conditions
9. Effect of hydrogen on the integrity of aluminium-oxide interface at elevated temperatures10.1038/ncomms14564 ↗
10. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
11. Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel10.1126/science.aal2418 ↗
12. The role of hydrogen and other interstitials in the mechanical behavior of metals
13. The efect of hydrogen on dislocation dynamics10.1016/S0013-7944(01)00011-X ↗
14. Hydrogen-enhanced localized plasticity—A mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
15. A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)10.1007/BF02642048 ↗
16. Effects of grain size and deformation temperature on hydrogen-enhanced vacancy formation in Ni alloys10.1016/j.actamat.2017.02.016 ↗
17. Formation of superabundant vacancies in M–H alloys and some of its consequences: a review10.1016/S0925-8388(02)01269-0 ↗
18. The role of atomistic simulations in probing hydrogen effects on plasticity and embrittlement in metals10.1016/j.engfracmech.2019.106502 ↗
19. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
20. Hydrogen-induced interactions in vanadium from first-principles calculations10.1103/PhysRevB.83.045111 ↗
21. Hydrogen-vacancy interactions in Fe-C Alloys10.1103/PhysRevLett.103.085501 ↗
22. Hydrogen-enhanced local plasticity at dilute bulk H concentrations: the role of H–H interactions and the formation of local hydrides10.1016/j.actamat.2011.01.037 ↗
23. First-principles calculations of transition metal solute interactions with hydrogen in tungsten10.1088/0029-5515/56/2/026004 ↗
24. Difference in formation of hydrogen and helium clusters in tungsten10.1063/1.2103390 ↗
25. A density functional theory assessment of the clustering behaviour of He and H in tungsten10.1016/j.jnucmat.2008.12.085 ↗
26. Hydrogen bubble nucleation in α-iron10.1016/j.scriptamat.2017.03.006 ↗
27. Predictive model of hydrogen trapping and bubbling in nanovoids in bcc metals10.1038/s41563-019-0422-4 ↗
28. Chemomechanical origin of hydrogen trapping at grain boundaries in fcc metals10.1103/PhysRevLett.116.075502 ↗
29. Influence of grain boundaries on the radiation-induced defects and hydrogen in nanostructured and coarse-grained tungsten10.1016/j.actamat.2016.10.007 ↗
30. Effect of plastic deformation on deuterium retention and release in tungsten10.1063/1.4913478 ↗
31. Depth distribution of deuterium in single- and polycrystalline tungsten up to depths of several micrometers10.1016/j.jnucmat.2004.10.082 ↗
32. Temperature dependence of surface morphology and deuterium retention in polycrystalline ITER-grade tungsten exposed to low-energy, high-flux D plasma10.1016/j.jnucmat.2011.11.003 ↗
33. Blister bursting and deuterium bursting release from tungsten exposed to high fluences of high flux and low energy deuterium plasma10.1088/0029-5515/47/3/006 ↗
34. Incident energy dependence of blistering at tungsten irradiated by low energy high flux deuterium plasma beams10.1016/j.jnucmat.2005.07.014 ↗
35. Hydrogen bubble nucleation by self-clustering: density functional theory and statistical model studies using tungsten as a model system10.1088/1741-4326/aacdb6 ↗
36. First-principles study of hydrogen diffusion and self-clustering below tungsten surfaces10.1063/1.5092595 ↗
37. Stress-induced hydrogen self-trapping in tungsten10.1088/1741-4326/aae2c7 ↗
38. Embedded-atom method potential for modeling hydrogen and hydrogen-defect interaction in tungsten
39. Multiscale description of dislocation induced nano-hydrides10.1016/j.actamat.2015.01.057 ↗
40. A nanoscale mechanism of hydrogen embrittlement in metals10.1016/j.actamat.2010.11.019 ↗
41. An electron-optical study of β-hydride and hydrogen embrittlement of vanadium10.1016/0001-6160(74)90166-7 ↗
42. The kinetics and micromechanics of hydrogen assisted cracking in Fe-3 pct Si single crystals10.1007/BF03350949 ↗
43. Evidence of stress-induced hydrogen ordering in zirconium hydrides10.1016/j.actamat.2008.08.061 ↗
44. Combined effects of oxygen and hydrogen on tensile properties of a Nb-10 At. Pct V Alloy10.1007/BF02670253 ↗
45. Anisotropic strain enhanced hydrogen solubility in bcc metals: the independence on the sign of strain10.1103/PhysRevLett.109.135502 ↗
46. Universality of point defect structure in body-centered cubic metals
47. Effect of uniaxial strain on the site occupancy of hydrogen in vanadium from density-functional calculations10.1038/srep10301 ↗
48. Hydrogen diffusion behavior in tungsten under anisotropic strain
49. Multiscale modelling of the interaction of hydrogen with interstitial defects and dislocations in BCC tungsten10.1088/1741-4326/aa8e0c ↗
50. Hydrogen accumulation around dislocation loops and edge dislocations: from atomistic to mesoscopic scales in BCC tungsten10.1088/1402-4896/aa9400 ↗
51. Ab initio molecular dynamics for open-shell transition metals10.1103/PhysRevB.48.13115 ↗
52. Ab initio molecular dynamics for liquid metals10.1103/PhysRevB.47.558 ↗
53. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
54. Atoms, molecules, solids, and surfaces: applications of the generalized gradient approximation for exchange and correlation10.1103/PhysRevB.46.6671 ↗
55. High-precision sampling for Brillouin-zone integration in metals10.1103/PhysRevB.40.3616 ↗
56. The code for structure relaxation under a specific stress tensor using VASPis available online at:https://github.com/jiehou93/VASP_fixpressure.
57. Fast parallel algorithms for short-range molecular dynamics10.1006/jcph.1995.1039 ↗
58. Visualization and analysis of atomistic simulation data with OVITO–the Open Visualization Tool10.1088/0965-0393/18/1/015012 ↗
59. Interatomic potentials for hydrogen in α–iron based on density functional theory10.1103/PhysRevB.79.174101 ↗
60. Methods of conjugate gradients for solving linear systems10.6028/jres.049.044 ↗
61. Grand canonical ensemble Monte Carlo for a Lennard-Jones fluid10.1080/00268977500100221 ↗
62. Material laws and properties
63. First-principles study of the stability and electronic structure of metal hydrides10.1103/PhysRevB.66.144107 ↗
64. First-principles calculations of hydrogen solution and diffusion in tungsten: temperature and defect-trapping effects10.1016/j.actamat.2014.10.039 ↗
65. Dissolving, trapping and detrapping mechanisms of hydrogen in bcc and fcc transition metals10.1063/1.4789547 ↗
66. Interplay between hydrogen and vacancies in α-Fe10.1103/PhysRevB.87.174103 ↗
67. An X-ray study of hydrides formed in austenitic stainless steels10.2355/isijinternational1966.18.485 ↗
68. Phase transformation and cracking during aging of an electrolytically charged Fe18Cr12Ni alloy at room temperature10.1016/0956-716X(93)90085-7 ↗
69. Hydride phases in austenitic stainless steels10.5006/0010-9312-35.10.461 ↗
70. Formation of iron hydride in α-Fe under dislocation strain field and its effect on dislocation interaction10.1016/j.commatsci.2017.09.032 ↗
71. The continuum elastic and atomistic viewpoints on the formation volume and strain energy of a point defect10.1016/j.jmps.2006.02.007 ↗
72. Elastic modeling of point-defects and their interaction10.1016/j.commatsci.2018.01.053 ↗
73. The key role played by dislocation core radius and energy in hydrogen interaction with dislocations10.1016/j.actamat.2019.12.033 ↗
74. Atomistic study of hydrogen distribution and diffusion around a {112}<111>edge dislocation in alpha iron10.1016/j.actamat.2008.04.011 ↗
75. Influence of shear strain on the hydrogen trapped in bcc-Fe: a first-principles-based study10.1016/j.scriptamat.2008.12.009 ↗
76. Ab initio parametrized model of strain-dependent solubility of H in α-iron10.1088/0965-0393/20/3/035011 ↗