The low temperature performance of Li-ion batteries

S.S. Zhang, K. Xu, T.R. Jow

Journal of Power Sources· Volume 115· Issue 1
Publisher page

Abstract

Abstract A symmetric cell was adopted to analyze low temperature performance of Li-ion battery. Results showed that impedances of both Li-ion and symmetric cells are mainly composed of bulk resistance (Rb), surface layer resistance (Rsl) and charge-transfer resistance (Rct). Among these three components, the Rct is most significantly increased and becomes predominant as the temperature falls to below −10 °C. Therefore, we may ascribe the poor low temperature performance of Li-ion battery to the substantially high Rct of the graphite and cathode. Comparing impedance spectra of the symmetric cells, we found that at −30 °C the delithiated graphite and lithiated cathode, both of which correspond to a discharged state in a Li-ion battery, have a much higher Rct than when charged. This means that the Li-ion battery in the discharged state suffers a higher polarization. This result explains the phenomenon that at low temperatures, charging of a discharged Li-ion battery is more difficult than discharging of a charged battery.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Battery Technologies Research · Advancements in Battery Materials · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Smart · J. Electrochem. Soc. · 1999 · 146 · 48610.1149/1.1391633 ↗
2. Huang · J. Electrochem. Soc. · 2000 · 147 · 289310.1149/1.1393622 ↗
3. Plichta · J. Power Sources · 2000 · 88 · 19210.1016/S0378-7753(00)00367-0 ↗
4. Lin · Electrochem. Solid-State Lett. · 2001 · 4 · A7110.1149/1.1368736 ↗
5. Ratnakumar · J. Power Sources · 2001 · 97–98 · 13710.1016/S0378-7753(01)00682-6 ↗
6. Nagasubramanian · J. Appl. Electrochem. · 2001 · 31 · 9910.1023/A:1004113825283 ↗
7. Wang · J. Electrochem. Soc. · 2002 · 149 · A75410.1149/1.1474427 ↗
8. Zhang · J. Power Sources · 2002 · 110 · 217
9. Zhang · Electrochim. Acta · 2002 · 48 · 24110.1016/S0013-4686(02)00620-5 ↗
10. Zhang · Electrochem. Commun. · 2002 · 4 · 92810.1016/S1388-2481(02)00490-3 ↗
11. Mohamedi · Electrochim. Acta · 2002 · 47 · 348310.1016/S0013-4686(02)00285-2 ↗
12. Ma · J. Appl. Electrochem. · 2002 · 32 · 6510.1023/A:1014242112512 ↗
13. Zhang · Electrochem. Solid-State Lett. · 2001 · 4 · A20610.1149/1.1414946 ↗