journal article·2018-06

Influence of quasicrystal I-phase on twinning of extruded Mg-Zn-Y alloys under compression

G. Garces, J. Medina, P. Pérez, K. Máthis, K. Horváth, A. Stark, N. Schell, P. Adeva

Acta Materialia· Volume 151
Publisher page

Abstract

The interaction of the I-phase with twins during compression has been studied in a Mg-6Zn-1Y (wt.%) alloy using the combination of Synchrotron Radiation Diffraction and Acoustic Emission experiments during compression tests. The I-phase occurs as coarse particles at grain boundaries and nanosized precipitates within magnesium grains. Their interaction with twins depends on their shape and size. The presence of coarse I-phase particles with higher Young Modulus requires an additional stress for the activation of twinning since they induce tensile residual stresses in the magnesium matrix. Besides twinning, the basal and non-basal slip systems are also activated. Non-basal slip is observed after macroscopic yield stress within twins. The fine I-phase precipitates within grains interacts with the dislocations and the twins. In the latter case a back-stress arises, which acts against the compressive applied stress. This back stress hinders the twin growth more than the effect of the coarse particles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Microstructure and mechanical properties · Quasicrystal Structures and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Deformation behavior of Mg-Zn-Y alloys reinforced by icosahedral quasicrystalline particles10.1016/S1359-6454(02)00067-8 ↗
2. Application of quasicrystalline particles as a strengthening phase in Mg-Zn-Y alloys10.1016/S0925-8388(02)00273-6 ↗
3. Quasicrystal strengthened Mg – Zn – Y alloys by extrusion10.1016/S1359-6462(03)00305-1 ↗
4. Microstructure and strength of quasicrystal containing extruded Mg – Zn – Y alloys for elevated temperature application10.1016/S0921-5093(04)00903-7 ↗
5. High temperature processing of Mg – Zn – Y alloys containing quasicrystal phase for high strength10.1016/j.msea.2011.05.001 ↗
6. Grain refinement of Mg-Zn-Y alloy reinforced by an icosahedral quasicrystalline phase by severe hot rolling10.1016/j.jallcom.2006.10.006 ↗
7. High-strength Mg-Zn-Y alloys produced by powder metallurgy10.1016/j.scriptamat.2009.01.012 ↗
8. Ultra-fine grain size and isotropic very high strength by direct extrusion of chill-cast Mg-Zn-Y alloys containing quasicrystal phase10.1016/j.scriptamat.2010.12.016 ↗
9. In-situ neutron diffraction of a quasicrystal-containing Mg alloy interpreted using a new polycrystal plasticity model of hardening due to {10.2} tensile twinning10.1016/j.ijplas.2017.09.005 ↗
10. Effect of particles on the formation of deformation twins in a magnesium-based alloy10.1016/j.msea.2009.04.001 ↗
11. Effect of particles in promoting twin nucleation in a Mg–5wt.% Zn alloy10.1016/j.scriptamat.2010.06.026 ↗
12. Effect of precipitate shape on slip and twinning in magnesium alloys10.1016/j.actamat.2010.11.060 ↗
13. {101¯2} Twinning in magnesium-based lamellar microstructures10.1016/j.scriptamat.2012.06.035 ↗
14. Effect of plate-shaped particle distributions on the deformation behaviour of magnesium alloy AZ91 in tension and compression10.1016/j.actamat.2011.10.001 ↗
15. In-situ X-ray diffraction studies of slip and twinning in the presence of precipitates in AZ91 alloy10.1016/j.actamat.2016.08.022 ↗
16. Reducing the tension–compression yield asymmetry in a Mg–8Al–0.5Zn alloy via precipitation10.1016/j.scriptamat.2009.11.024 ↗
17. Precipitation strengthening and reversed yield stress asymmetry in Mg alloys containing rare-earth elements: a quantitative study10.1016/j.actamat.2016.11.019 ↗
18. Evolution of internal strain during plastic deformation in magnesium matrix composites10.1016/j.msea.2009.06.026 ↗
19. Influence of SiC particles on compressive deformation of magnesium matrix composites10.1016/j.msea.2011.10.103 ↗
20. Effect of reinforcing shape on twinning in extruded magnesium matrix composites10.1016/j.msea.2016.04.028 ↗
21. EBSD analysis of deformation modes in Mg–3Al–1Zn10.1016/j.scriptamat.2006.07.036 ↗
22. Hammersley · 1997
23. A real-time approach to acoustic emission clustering10.1016/j.ymssp.2013.03.017 ↗
24. Microstructural changes in an extruded Mg-Zn-Y alloy reinforced by quasicrystalline I-phase by small additions of calcium, manganese and cerium-rich mischmetal10.1016/j.matchar.2016.05.019 ↗
25. Effects of calcium, manganese and cerium-rich mischmetal additions on the mechanical properties of extruded Mg-Zn-Y alloy reinforced by quasicrystalline I-phase10.1016/j.matchar.2017.04.033 ↗
26. Highly ordered structure of icosahedral quasicrystal in Zn-Mg-RE(RE=rare earth metals) systems10.1080/09500839408240971 ↗
27. Quasicrystal-crystal transformation in Zn-Mg-Rare-Earth alloys10.1103/PhysRevLett.83.753 ↗
28. Study of the mechanical properties of Mg-7.7at.% Al by in-situ neutron diffraction10.1080/01418619908210386 ↗
29. Validating a polycrystal model for the elastoplastic response of magnesium alloy AZ31 using in situ neutron diffraction10.1016/j.actamat.2006.06.020 ↗
30. Internal strain and texture evolution during deformation twinning in magnesium10.1016/j.msea.2005.02.016 ↗
31. Evolution of twinning in extruded AZ31 with bimodal grain structure10.1016/j.matchar.2017.02.017 ↗
32. Hutchinson · 1977 · vol. 8 · 1465
33. Smithells Metals Reference Book Edited E.A. Brandes, G.B. Brooks Sections 15-2 Butterworth-Heinemann.
34. S. Takeuchi, K. Edagawa Elastic and plastic properties of quasicrystals (Chapter 8) 267–311, in Quasicrystal Editors T. Fujiwara and Y. Ishii Elsevier.10.1016/S1570-002X(08)80023-7 ↗
35. Variance method for the evaluation of particle size and dislocation density from x-ray Bragg peaks
36. Acoustic emission as a tool for exploring deformation mechanisms in magnesium and its alloys in situ10.1007/s11837-016-1966-2 ↗
37. Effect of the loading mode on the evolution of the deformation mechanisms in randomly textured magnesium polycrystals - Comparison of experimental and modeling results10.1016/j.ijplas.2015.05.009 ↗
38. Temperature dependency of slip and twinning in plane strain compressed magnesium single crystals10.1016/j.actamat.2010.11.064 ↗
39. In situ neutron diffraction and polycrystal plasticity modeling of a Mg–Y–Nd–Zr alloy: effects of precipitation on individual deformation mechanisms10.1016/j.actamat.2013.03.010 ↗
40. Reorientation and stress relaxation due to twinning: modeling and experimental characterization for Mg10.1016/j.actamat.2008.01.057 ↗
41. Wu · 2008 · vol. 56 · 3699
42. Ultra-fine grain size and isotropic very high strength by direct extrusion of chill-cast Mg–Zn–Y alloys containing quasicrystal phase10.1016/j.scriptamat.2010.12.016 ↗
43. Rare-earth free wrought-processed magnesium alloy with dispersion of quasicrystal phase10.1016/j.scriptamat.2009.06.008 ↗
44. Deformation behavior of ultra-fine-grained Mg-0.3 at% Al alloy in compression10.1016/j.jallcom.2017.08.032 ↗
45. Plasticity analysis by synchrotron radiation in a Mg97Y2Zn1 alloy with bimodal grain structure and containing LPSO phase10.1016/j.actamat.2015.04.048 ↗
46. A crystal plasticity theory for latent hardening by glide twinning through dislocation transmutation and twin accommodation effects10.1016/j.jmps.2009.12.004 ↗
47. Electron microscope observation in and around {11¯02}twins in magnesium10.2320/matertrans1960.17.158 ↗
48. Deformation of twins in a magnesium alloy under tension at room temperature10.1016/j.jallcom.2014.01.100 ↗
49. Prism stacking faults observed contiguous to a {10-12} twin in a Mg-Y alloy10.1016/j.scriptamat.2013.12.015 ↗
50. On the role of twinning and stacking faults on the crystal plasticity and grain refinement in magnesium alloys10.1016/j.actamat.2017.11.004 ↗
51. Thermal expansion of icosahedral Al-Pd-Mn and decagonal Al-Cu-Co quasicrystals10.1080/095008300176452 ↗
52. Clyne · 1993
53. Stress Measurements in Composites using Neutron Diffraction in: measurement of residual and applied stress using neutron diffraction
54. Deformation twinning10.1016/0079-6425(94)00007-7 ↗
55. Nanoprecipitates of icosahedral phase in quasicrystal-strengthened Mg-Zn-Y alloys10.1080/09500830310001597027 ↗
56. Twinning and the orientation relationships of icosahedral phase with the magnesium matrix10.1016/j.actamat.2005.06.026 ↗
57. Surface energy of icosahedral quasicrystals
58. The work-hardening of copper-silica I. A model based on internal stresses, with no plastic relaxation10.1080/14786437108217405 ↗
59. Effect of precipitates shape on slip and twinning in magnesium alloys10.1016/j.actamat.2010.11.060 ↗
60. Novel hexagonal structure and ultrahigh strength of magnesium solid solution in the Mg-Zn-Y system
61. Effect of multimodal microstructure evolution on mechanical properties of Mg–Zn–Y extruded alloy10.1016/j.actamat.2011.02.038 ↗
62. Effects of stacking sequence and short-range ordering of solute atoms on elastic properties of Mg–Zn–Y alloys with long-period stacking ordered structures10.1016/j.actamat.2015.06.005 ↗
63. Thermal expansion behaviour of Long-period stacking ordered (LPSO) phase
64. The role of extrusion texture on strength and its anisotropy in a Mg-base alloy composed of the Long-Period-Structural-Order phase10.1016/j.intermet.2014.07.015 ↗