Growth rate of lithium filaments in ceramic electrolytes
Source abstract
Abstract
© 2020 Lithium-ion batteries with single ion-conductor ceramic electrolytes short-circuit when subjected to charging currents above a critical current density. Here, we analyse the rate at which a lithium (Li) filament (sometimes referred to as a dendrite) will grow from the cathode towards the anode during charging of such batteries. The filament is modelled as a climbing edge dislocation with its growth occurring by Li+ flux from the electrolyte into the filament tip at constant chemical potential. The growth rate is set by a balance between the reduction of free-energy at the filament tip and energy dissipation associated with the resistance to the flux of Li+ through the filament tip. For charging currents above the critical current density, the filament growth rate increases with decreasing filament tip resistance. Imperfections, such as voids in the Li cathode along the electrolyte/cathode interface, decrease the critical current density but filament growth rates are also lower in these cases as filament growth rates scale with the charging currents. The predictions of the model are in excellent quantitative agreement with measurements and confirm that above the critical current density a filament can traverse the electrolyte in minutes or less. This suggests that initiation of filament growth is the critical step to prevent short-circuiting of the battery.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Progress and prospective of solid-state lithium batteries10.1016/j.actamat.2012.10.034 ↗
2. All-solid-state batteries10.1016/0378-7753(84)80064-6 ↗
3. Lithium metal stripping/plating mechanisms studies: a metallurgical approach10.1016/j.elecom.2006.07.037 ↗
4. Detection of subsurface structures underneath dendrites formed on cycled lithium metal electrodes10.1038/nmat3793 ↗
5. Electrochemical deposition and stripping behavior of lithium metal across a rigid block copolymer electrolyte membrane10.1149/2.0321514jes ↗
6. Characterizing the Li–Li7La3Zr2O12 interface stability and kinetics as a function of temperature and current density10.1016/j.jpowsour.2015.10.053 ↗
7. In-situ, non-destructive acoustic characterization of solid state electrolyte cells10.1016/j.jpowsour.2016.05.062 ↗
8. Surface chemistry mechanism of ultra-low interfacial resistance in the solid-state electrolyte Li7La3Zr2O1210.1021/acs.chemmater.7b03002 ↗
9. Controlling and correlating the effect of grain size with the mechanical and electrochemical properties of Li7La3Zr2O12 solid-state electrolyte10.1039/C7TA06790A ↗
10. The role of the solid electrolyte interphase layer in preventing Li dendrite growth in solid-state batteries10.1039/C8EE00540K ↗
11. Intergranular Li metal propagation through polycrystalline Li6.25Al0.25La3Zr2O12 ceramic electrolyte10.1016/j.electacta.2016.12.018 ↗
12. Slow degradation and electron conduction in sodium/beta-aluminas10.1007/BF02402796 ↗
13. Li penetration in ceramic solid electrolytes: operando microscopy analysis of morphology, propagation, and reversibility10.1016/j.matt.2020.02.008 ↗
14. Initiation of mode I degradation in sodium-beta alumina electrolytes10.1007/BF00591486 ↗
15. Mechanism of lithium metal penetration through inorganic solid electrolytes10.1002/aenm.201701003 ↗
16. Dendritic cracking in solid electrolytes driven by lithium insertion
17. Analysis of solid-state electrodeposition-inducedmetal plastic flow and predictions of stress states in solid ionic conductor defects
18. Dendrites as climbing dislocations in ceramic electrolytes: initiation of growth10.1016/j.jpowsour.2020.227989 ↗
19. Critical stripping current leads to dendrite formation on plating in lithium anode solid electrolyte cells10.1038/s41563-019-0438-9 ↗
20. Mechanical properties of metallic lithium: from nano to bulk scales10.1016/j.actamat.2019.12.036 ↗
21. Real-time 3D imaging of microstructure growth in battery cells using indirect MRI10.1073/pnas.1607903113 ↗
22. Defect parameters of bcc metals: group-specific trends10.1016/0921-5093(91)90766-G ↗
23. Synthesis, crystal chemistry, and electrochemical properties of Li7–2xLa3Zr2–xMoxO12 (x = 0.1–0.4): stabilization of the cubic garnet polymorph via substitution of Zr4+ by Mo6+10.1021/acs.inorgchem.5b01895 ↗
24. Room temperature elastic moduli and Vickers hardness of hot-pressed LLZO cubic garnet10.1007/s10853-012-6687-5 ↗
25. Abaqus2Matlab: a suitable tool for finite element post-processing10.1016/j.advengsoft.2017.01.006 ↗