Effects of prestrain on the ductile-to-brittle transition of ice

Scott A. Snyder, Erland M. Schulson, Carl E. Renshaw

Acta Materialia· Volume 108

Abstract

The ductile-to-brittle transition was investigated in prestrained columnar ice at −10 °C. Laboratory-grown specimens of freshwater and saline ice were prestrained under uniaxial across-column compression (to levels from εp = 0.003 to εp = 0.20, at constant strain rates in the ductile regime) and likewise reloaded (at rates from 1 × 10−6s−1 to 3 × 10−2s−1). Prestrain caused solid-state recrystallization as well as damage in the form of non-propagating microcracks. The ductile-to-brittle transition strain rate ε˙D/B increased by a factor of 3–10 after prestrain of εp = 0.035 in both freshwater and saline ice, compared to that of initially undamaged ice of the same type. Additional prestrain had little further effect on ε˙D/B. The results are interpreted within the framework of a model (proposed by Schulson, 1990, and Renshaw and Schulson, 2001) that predicts the transition strain rate based on the micromechanical boundary between creep and fracture processes. Model parameters primarily affected by prestrain were the power-law creep coefficient B (more so than the creep exponent n), Young's modulus E and, by extension, the fracture toughness KIc.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Cryospheric studies and observations · Climate change and permafrost · Arctic and Antarctic ice dynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Brittle compressive fracture of ice10.1016/0956-7151(90)90308-4 ↗
2. Universal behaviour in compressive failure of brittle materials10.1038/35091045 ↗
3. Schulson · 2009
4. The effect of temperature on the ductile-to-brittle transition in columnar ice
5. The ductile-to-brittle transition and ductile failure envelopes of orthotropic ice under biaxial compression10.1016/0956-7151(95)90149-3 ↗
6. On the ductile-to-brittle transition in ice under compression10.1016/0956-7151(93)90391-5 ↗
7. Crack-enhanced creep in polycrystalline material: strain-rate sensitive strength and deformation of ice10.1007/BF00551940 ↗
8. Creep behaviour of damaged ice under uniaxial compression
9. Effect of microcracking on the deformation of ice10.1139/t92-015 ↗
10. The ductile behaviour of damaged ice under compression
11. Damage of isotropic polycrystalline ice under moderate confining pressures
12. The effects of prestrain on the compressive ductile-to-brittle transition in ice
13. Classification of river and lake ice10.1139/t71-004 ↗
14. Plastic faulting: brittle-like failure under high confinement10.1029/2003JB002945 ↗
15. The effects of compressive and tensile prestrain on ductile fracture initiation in steels10.1016/j.engfracmech.2004.07.012 ↗
16. The influence of pre-compression on the creep deformation and failure behaviour of Type 316h stainless steel10.1016/j.engfracmech.2013.08.006 ↗
18. Ductile saline ice10.3189/S0022143000012454 ↗
19. Effects of surface condition on the mechanical properties of ice crystals
20. Rheology of columnar-grained ice10.1007/BF02324282 ↗
21. The friction and creep of polycrystalline ice
22. Uniaxial compressive strength of first-year and multi-year sea ice10.1139/l84-010 ↗
23. Langway · 1958
24. Snyder · 2015
25. Hobbs · 1974
26. The role of damage and recrystallization in the elastic properties of columnar ice10.3189/2015JoG14J225 ↗
27. Transition in brittle failure mode in ice under low confinement10.1016/j.actamat.2008.09.021 ↗
28. Observations of anisotropy in damage and elastic properties of columnar ice containing cracks
29. Transition from brittle fracture to ductile flow in solenhofen limestone as a function of temperature, confining pressure, and interstitial fluid pressure10.1130/MEM79-p193 ↗
30. Elastic solids with many cracks and related problems
31. The friction of ice on ice at low sliding velocities10.1080/01418610008212103 ↗
32. Friction of ice on ice10.1029/2012JB009219 ↗
33. The effects of anisotropy and microcracks on the fracture toughness (KIc) of freshwater ice
34. Deformation and failure of ice under constant stress or constant strain-rate10.1016/0165-232X(82)90015-5 ↗
35. Uniaxial constant compressive stress creep tests on sea ice10.1115/1.2827235 ↗
36. Rate-controlling processes in the creep of polycrystalline ice10.1021/j100244a014 ↗
37. Statistical characteristics for the strain-dependent density and the spatial position for deformation-induced cracks in columnar-grain ice10.3189/002214399793377158 ↗
38. On the initiation of shear faults during brittle compressive failure: a new mechanism10.1029/1998JB900017 ↗
39. Brittle failure of ice10.1016/S0013-7944(01)00037-6 ↗
40. Tensile cracks in creeping solids
41. The plasticity of polycrystalline ice10.1080/01418618108240401 ↗
42. Buck · 1994
43. Failure envelopes and the ductile to brittle transition in S2 columnar freshwater and saline ice under biaxial compression