journal article·2019-10

The effect of Zr substitution on saturation magnetization in (Sm1-xZrx)(Fe0.8Co0.2)12 compound with the ThMn12 structure

P. Tozman, Y.K. Takahashi, H. Sepehri-Amin, D. Ogawa, S. Hirosawa, K. Hono

Acta Materialia· Volume 178
Publisher page

Abstract

Abstract Zr is one of the essential elements to stabilize the ThMn12 structure in rare earth (R) transition metal (M) hard magnetic compounds, RM12. In this work, the effects of Zr on the intrinsic hard magnetic properties of (Sm1-x Zrx)(Fe0.8Co0.2)12 compounds are investigated using epitaxially grown thin films. The increase of Zr substitution for Sm from x = 0 to 0.26 for (Sm1-x Zrx)(Fe0.8Co0.2)12 increases saturation magnetization (μ0Ms) from 1.78 T to 1.90 T, the highest value reported for hard magnetic compounds. The largest μ0Ha and Tc for Zr-doped samples were found to be 9.8 T and 671 K for x = 0.18 which is superior to those for Nd2Fe14B. Sm-rich Sm1.30Zr0.27(Fe0.8Co0.2)12, obtained as sub-μm thick films, has remanence, μ0Mr of 1 T, which appears to be useful for near-field applications such as micro-electro-machines and magnetic recording media if microstructure can be optimized to obtain a sufficient coercivity.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic Properties and Applications · Magnetic properties of thin films

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. New material for permanent magnets on a base of Nd and Fe10.1063/1.333572 ↗
2. Magnetic properties of Fe-rich rare-earth intermetallic compounds with a ThMn12 structure10.1063/1.342235 ↗
3. Intrinsic magnetic properties of the iron-rich ThMn12-structure alloys R(Fe11Ti); R= Y, Nd, Sm, Gd, Tb, Dy, Ho, Er, Tm and Lu10.1088/0953-8984/1/4/009 ↗
4. Structure and magnetic properties of nanocrystalline Sm(Fe1− xCox)11Ti (x<∼ 2)10.1103/PhysRevB.63.054412 ↗
5. Permanent magnet materials based on tetragonal rare earth compounds of the type RFe12− xMx10.1016/0304-8853(91)90813-P ↗
6. (Sm, Zr)(Fe,Co)11.0-11.5Ti1. 0-0.5 compounds as new permanent magnet materials10.1063/1.4943051 ↗
7. Intrinsic magnetic properties of Sm(Fe1-xCox)11Ti and Zr-substituted Sm1-yZry(Fe0. 8Co0. 2)11.5Ti0. 5 compounds with ThMn12 structure toward the development of permanent magnets10.1016/j.actamat.2018.05.008 ↗
8. Magnetic and structural properties of SmTiFe11-xCox alloys10.1016/0304-8853(88)90039-X ↗
9. Electronic structure and magnetism of transition-metal-stabilized YFe12− xMx intermetallic compounds10.1103/PhysRevB.41.11790 ↗
10. First-principles study of magnetocrystalline anisotropy and magnetization in NdFe12, NdFe11Ti, and NdFe11TiN10.7566/JPSJ.83.043702 ↗
11. Theoretical screening of intermetallic ThMn12-type phases for new hard-magnetic compounds with low rare earth content10.1038/srep24686 ↗
12. Intrinsic hard magnetic properties of Sm(Fe1-xCox)12 compounds with the ThMn12 structure10.1016/j.scriptamat.2017.05.029 ↗
13. Enhanced energy product in Y-Co-Fe magnets intermediate between Nd-Fe-B and ferrite10.1063/1.4927306 ↗
14. Permanent magnets beyond Nd-Dy-Fe-B10.1109/TMAG.2018.2863737 ↗
15. Attractive-domain-wall-pinning controlled Sm-Co magnets overcome the coercivity-remanence trade-off10.1016/j.actamat.2018.10.046 ↗
16. Development of ultra-fine grain sized SmFe12-based powders using hydrogenation disproportionation desorption recombination process10.1016/j.actamat.2018.11.065 ↗
17. Shape of temperature dependence of spontaneous magnetization of ferromagnets: quantitative analysis
18. Novel torque magnetometry for uniaxial anisotropy constants of thin films and its application to FePt granular thin films
19. Crystal-field splittings in rare-earth-based hard magnets: an ab initio approach10.1103/PhysRevB.96.155132 ↗
20. Magnetization and magnetic anisotropy of R2Fe14B measured on single crystals10.1063/1.336611 ↗
21. First-principles study of intersite magnetic couplings and Curie temperature in RFe12− x Crx (R= Y, Nd, Sm)10.7566/JPSJ.87.044706 ↗
22. First-principles study of spin-wave dispersion in Sm (Fe1− xCox)1210.1016/j.jmmm.2018.08.071 ↗
23. On the limits of coercivity in permanent magnets10.1063/1.4999315 ↗
24. Observation of intermultiplet transitions in SmFe11Ti by inelastic magnetic neutron scattering10.1103/PhysRevB.42.1940 ↗
25. High field magnetization measurements of SmFe11Ti and SmFe11TiH1− δ10.1063/1.361852 ↗
26. Magnetic phase transitions, magnetocrystalline anisotropy, and crystal-field interactions in the R Fe 11 Ti series (where R= Y, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, or Tm)10.1103/PhysRevB.47.3231 ↗
27. Theory of first order magnetization processes: uniaxial anisotropy10.1016/0304-8853(80)90522-3 ↗
28. D. Ogawa , T. Yoshioka, X.D. Xu, Y. K. Takahashi, H. Tsuchiura, T. Ohkubo, S. Hirosawa, K. Hono, Will Be Published.
29. Strategy for high-coercivity Nd–Fe–B magnet10.1016/j.scriptamat.2012.06.038 ↗