Rumpling induced by thermal cycling of an overlay coating: the effect of coating thickness
Source abstract
Abstract
Abstract Initially flat NiAl-based overlay coatings on a Ni-base superalloy substrate develop surface undulations when cyclically oxidized at high-temperatures. The effect of the coating thickness on the amplitude and wavelength of the undulations is described. The amplitude, after 100 one-hour cycles to 1150 °C in air, appears to have a maximum at intermediate thicknesses between 100 and 150 μm whereas the effective wavelength increases with the coating thickness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Combustion and flame dynamics · nanoparticles nucleation surface interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. Surface instability of platinum modified aluminide coatings during 1100 °C cyclic testing10.1116/1.574197 ↗
2. Mechanical degradation of coating systems in high-temperature cyclic oxidation10.1016/0257-8972(95)02551-0 ↗
3. Tolpygo VK, Clarke DR. Acta Mater, submitted for publication
4. Surface rumpling of a (Ni,Pt)Al bond coat induced by cyclic oxidation10.1016/S1359-6454(00)00156-7 ↗
5. Characterization of a cyclic displacement instability for a thermally grown oxide in a thermal barrier system10.1016/S1359-6454(01)00071-4 ↗
6. Bond coat surface rumpling in thermal barrier coatings10.1016/S1359-6454(02)00395-6 ↗
7. The ratcheting of compressed thermally grown thin films on ductile substrates10.1016/S1359-6454(00)00053-7 ↗
8. Mechanisms controlling the durability of thermal barrier coatings10.1016/S0079-6425(00)00020-7 ↗