Abstract

We present a new concept for strengthening ceamics by utilizing a graded structure with a low elastic modulus at both top and bottom surfaces sandwiching a high-modulus interior. Closed-form equations have been developed for stress analysis of simply supported graded sandwich beams subject to transverse center loads. Theory predicts that suitable modulus gradients at the ceramic surface can effectively reduce and spread the maximum bending stress from the surface into the interior. The magnitude of such stress dissipation is governed by the thickness ratio of the beam to the graded layers. We test our concept by infiltrating both top and bottom surfaces of a strong class of zirconia ceramic with an in-house prepared glass of similar coefficient of thermal expansion and Poisson's ratio to zirconia, producing a controlled modulus gradient at the surface without significant long-range residual stresses. The resultant graded glass/zirconia/glass composite exhibits significantly higher load-bearing capacity than homogeneous zirconia.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Tribology and Wear Analysis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Green · Science · 1999 · 283 · 129510.1126/science.283.5406.1295 ↗
2. Green · J Am Ceram Soc · 1983 · 66 · 17810.1111/j.1151-2916.1983.tb10543.x ↗
3. Balakrishnan · J Mater Res · 2007 · 22 · 255010.1557/jmr.2007.0325 ↗
4. Chu · Mater Sci Eng A · 2007 · 452–453 · 11010.1016/j.msea.2006.10.102 ↗
5. Suresh · Science · 2001 · 292 · 244710.1126/science.1059716 ↗
6. Jitcharoen · J Am Ceram Soc · 1998 · 81 · 230110.1111/j.1151-2916.1998.tb02625.x ↗
7. Pender · Acta Mater · 2001 · 49 · 325510.1016/S1359-6454(01)00200-2 ↗
8. Suresh · Acta Mater · 1999 · 47 · 391510.1016/S1359-6454(99)00205-0 ↗
9. Koizumi · Ceram Trans · 1993 · 34 · 3
10. Sankar · Compos Sci Technol · 2001 · 61 · 68910.1016/S0266-3538(01)00007-0 ↗
11. Kapuria · Compos Struct · 2008 · 82 · 39010.1016/j.compstruct.2007.01.019 ↗
12. Kashtalyan · Eur J Mec A/Solids · 2004 · 23 · 85310.1016/j.euromechsol.2004.04.002 ↗
13. Kashtalyan · Compos Struct · 2009 · 87 · 3610.1016/j.compstruct.2007.12.003 ↗
14. Zhang Y, Kim JW. Dent Mater. Published online: February 1, 2009. doi: 10.1016/j.dental.2009.01.002.10.1016/j.dental.2009.01.002 ↗
15. Gere · 1997
16. Oliver · J Mater Res · 1992 · 7 · 156410.1557/JMR.1992.1564 ↗
17. Oliver · J Mater Res · 2004 · 19 · 310.1557/jmr.2004.19.1.3 ↗
18. ISO International Standard, Dental ceramics, vol. 6872. ISO; 1995.
19. Kassir · Int J Fract Mech · 1972 · 8 · 32510.1007/BF00186131 ↗
20. Tilbrook · Compos Sci Technol · 2005 · 65 · 20110.1016/j.compscitech.2004.07.004 ↗
21. Parameswaran · Mech Mater · 1999 · 31 · 57910.1016/S0167-6636(99)00025-3 ↗
22. Lawn · 1993
23. Chantikul · J Am Ceram Soc · 1979 · 62 · 55110.1111/j.1151-2916.1979.tb12728.x ↗
24. Flaitz · J Am Ceram Soc · 1987 · 70 · 44910.1111/j.1151-2916.1987.tb05674.x ↗