Abstract

Abstract A Monte-Carlo simulation of microstructural development under forced convection is presented. The model takes into account both diffusive and forced fluid flow, kinetics of atomic attachment at the solid–liquid interface and structural modification under the influence of capillary forces. It has been shown that the nature of fluid flow has a very significant influence on the morphology of the solidification structure. A laminar type flow is shown to destabilize the solid–liquid interface promoting dendritic growth for solid growing from fixed substrate. Particle rotation under streamlined flow, or a periodic change in the fluid flow direction around the growing solid is, however, shown to produce the rosette type solidification morphology. A turbulent type flow penetrating into the interdendritic region produces fine and compact solidification structures with or without liquid entrapment.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Solidification and crystal growth phenomena · Aluminum Alloy Microstructure Properties · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Flemings, M. C., Metall. Trans. A, 1991;22A:957.10.1007/BF02661090 ↗
2. Kirkwood · Int. Mater. Rev. · 1994 · 39 · 17310.1179/imr.1994.39.5.173 ↗
3. Spencer · Metall Trans. · 1972 · 3 · 192510.1007/BF02642580 ↗
4. Flemings · Mater. Sci. Engng · 1976 · 25 · 10310.1016/0025-5416(76)90057-4 ↗
5. Fan Z, Bevis MJ, Ji S. WIPO PCT Patent, WO 01/21343 A1, 1999.
6. Ji · Mater. Sci. Engng · 2001 · A299 · 999
7. Vogel · J. Cryst. Growth · 1977 · 37 · 30910.1016/0022-0248(77)90125-7 ↗
8. Doherty · Mater. Sci. Engng · 1984 · 65 · 18110.1016/0025-5416(84)90211-8 ↗
9. Mullis · Acta Mater. · 1999 · 47 · 178310.1016/S1359-6454(99)00052-X ↗
10. Witten · Phys. Rev. Lett. · 1981 · 47 · 140010.1103/PhysRevLett.47.1400 ↗
11. Kumar · Acta Metall. Mater. · 1994 · 42 · 359510.1016/0956-7151(94)90426-X ↗
12. Martin · Acta Metall. Mater. · 1994 · 42 · 360310.1016/0956-7151(94)90427-8 ↗
13. Das · Metall. Mater. Trans. A · 2000 · 31A · 204910.1007/s11661-000-0232-x ↗
14. Das · Philos. Mag. A · 2001 · 81 · 272510.1080/01418610108216666 ↗
15. Binder · 1986 · 3
16. Haemers · Modelling Simul. Mater. Sci. Engng · 1999 · 35 · 23310.1088/0965-0393/7/2/007 ↗
17. Cantor · J. Cryst. Growth · 1977 · 41 · 10910.1016/0022-0248(77)90104-X ↗
18. Vogel A. D. Phil thesis, University of Sussex, 1977.
19. Vogel A, Doherty RD, Cantor B. Proc Conf on Solidification and Casting of Metals, Sheffield. Metals Society, London, 1979. p. 518.
20. Apaydin · Mater. Sci. Engng · 1980 · 46 · 14510.1016/0025-5416(80)90170-6 ↗
21. Lee · 1983 · 119
22. Hellawell A. Conf Prof on Semisolid Processing of Alloys and Composites, Sheffield, 1996. p. 60.
23. Molenaar · J. Mater. Sci. · 1985 · 20 · 433510.1007/BF00559322 ↗
24. Molenaar · J. Mater. Sci. · 1986 · 21 · 38910.1007/BF01145499 ↗
25. Vogel A. Metal Sci. 1978;576.10.1179/msc.1978.12.12.576 ↗
26. Ji S, Fan Z.Metall. Mater. Trans. A, submitted.
27. Ryoo · 1994 · 95