journal article·2013-02-07

A Versatile Material for a Symmetrical Electric Energy Storage Device: A Composite of the Polymer of the Ferrocene Adduct of C60 and Single-Wall Carbon Nanotubes Exhibiting Redox Conductivity at Both Positive and Negative Potentials

Piotr Pieta, Ievgen Obraztsov, Janusz W. Sobczak, Olga Chernyayeva, Sushanta K. Das, Francis D’Souza, Wlodzimierz Kutner

Publisher page

Abstract

A (carbon nanotube)–(fullerene–ferrocene dyad polymer) composite, pyr-SWCNTs/(C 60 Fc-Pd), was devised and tested as an active material of a symmetrical device for electric energy storage. The composite was redox conducting at both positive and negative potentials due to the Fc/Fc + and C 60 – /C 60 electrode process of the ferrocene and fullerene moiety of the dyad, respectively. The composite was prepared, first, by electrophoretic deposition of a film of noncovalently modified with 1-pyrenebutyric acid stacked single-wall carbon nanotubes (pyr-SWCNTs). Then, this film was coated, by potentiodynamic electropolymerization, with a film of the palladium-doped polymer of 2′-ferrocenylfulleropyrrolidine (C 60 Fc-Pd). The AFM imaging showed that the C 60 Fc-Pd film was uniformly built of 40–150 nm diameter globules of C 60 Fc-Pd while the film formed a tangle of pyr-SWCNTs bundles wrapped with clusters of ∼45 nm diameter globules of C 60 Fc-Pd. The XPS measurements identified interactions between the Pd and C 60 moieties in C 60 Fc-Pd. The electrochemical and viscoelastic properties of the pyr-SWCNTs/(C 60 Fc-Pd) film in a blank acetonitrile solution of tetra- n -butylammonium perchlorate favorably compared to those of the C 60 Fc-Pd film as disclosed by simultaneous cyclic voltammetry (CV) and piezoelectric microgravimetry (PM) measurements. Specific capacitance ( C s ) of the pyr-SWCNTs/(C 60 Fc-Pd) film was higher than that of the C 60 Fc-Pd film and for positive charging its maximum value was C s,max ≅ 300 F g –1 . The EIS measurements revealed capacitive and mixed capacitive and pseudocapacitive behavior of the composite over the narrow and wide range of the applied potentials, respectively. Alternate galvanostatic +0.72 mA cm –2 charging and −0.72 mA cm –2 discharging and then opposite polarity charging of a device constructed of two identical composite film electrodes was reversible only for low (+0.6 and −0.6 V) voltage of charging and discharging. After multiple charging and discharging (1000 cycles), the capacity increased by ∼5%, but it decreased by ∼18% for the high (+1.2 and −1.2 V) voltage. Importantly, the average power of the device was ∼7.3 times higher for the latter.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Conducting polymers and applications · Supercapacitor Materials and Fabrication · Carbon Nanotubes in Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Physical Chemistry of Supramolecular Complexes, Institute of Physical Chemistry, Polish Academy of Sciences, Kasprzaka 44/52, 01-224 Warsaw, Poland

Department of Chemistry, University of North Texas, 1155 Union Circle, #305070, Denton, Texas 76203-5017, United States

Faculty of Mathematics and Natural Sciences, School of Science, Cardinal Stefan Wyszynski University in Warsaw, Woycickiego 1/3, 01-938 Warsaw, Poland

References (58)

Show source-provided references
1. Pieta P. · 2011 · 2 · 69310.1142/9789814327824_0021 ↗
2. Frackowiak E. · J. Power Sources · 2006 · 153 · 41310.1016/j.jpowsour.2005.05.030 ↗
3. Zhang Y. · Int. J. Hydrogen Energy · 2009 · 34 · 488910.1016/j.ijhydene.2009.04.005 ↗
4. Wang J. · Compos. Sci. Technol. · 2007 · 67 · 298110.1016/j.compscitech.2007.05.015 ↗
5. Honda Y. · J. Electrochem. Soc. · 2008 · 155 · 93010.1149/1.2988743 ↗
6. Peng C. · Prog. Nat. Sci. · 2008 · 18 · 77710.1016/j.pnsc.2008.03.002 ↗
7. Zhou C. · Chem. Mater. · 2005 · 17 · 199710.1021/cm047882b ↗
8. Jurewicz K. · Chem. Phys. Lett. · 2001 · 347 · 3610.1016/S0009-2614(01)01037-5 ↗
9. Wu M. · J. Mater. Chem. · 2005 · 15 · 229710.1039/b418835g ↗
10. Pieta P. · J. Phys. Chem. B · 2009 · 113 · 668210.1021/jp810173c ↗
11. Pieta P. · J. Phys. Chem. C · 2010 · 114 · 815010.1021/jp912033q ↗
12. Pieta P. · J. Phys. Chem. C · 2009 · 113 · 1404610.1021/jp903891v ↗
13. Harris P. J. F. · 2009
14. Meitl M. A. · Nano Lett. · 2004 · 4 · 164310.1021/nl0491935 ↗
15. Sreekumar T. V. · Chem. Mater. · 2003 · 15 · 17510.1021/cm020367y ↗
16. Kim J. H. · Carbon · 2006 · 44 · 196310.1016/j.carbon.2006.02.002 ↗
17. Wu Z. · Science · 2004 · 305 · 127310.1126/science.1101243 ↗
18. Simmons T. J. · J. Am. Chem. Soc. · 2007 · 129 · 1008810.1021/ja073745e ↗
19. Kordás K. · Small · 2006 · 2 · 102110.1002/smll.200600061 ↗
20. Li X. · J. Am. Chem. Soc. · 2007 · 129 · 489010.1021/ja071114e ↗
21. Lee S. W. · J. Am. Chem. Soc. · 2008 · 131 · 67110.1021/ja807059k ↗
22. Ren Z. F. · Science · 1998 · 282 · 110510.1126/science.282.5391.1105 ↗
23. Huang Z. P. · Appl. Phys. Lett. · 1998 · 73 · 384510.1063/1.122912 ↗
24. Ren Z. F. · Appl. Phys. Lett. · 1999 · 75 · 108610.1063/1.124605 ↗
25. Chen J. H. · Synth. Met. · 2002 · 125 · 28910.1016/S0379-6779(01)00404-0 ↗
26. Xiao Q. · Electrochim. Acta · 2003 · 48 · 57510.1016/S0013-4686(02)00727-2 ↗
27. Valentini L. · Appl. Phys. Lett. · 2003 · 82 · 96110.1063/1.1545166 ↗
28. Hughes M. · Adv. Mater. · 2002 · 14 · 38210.1002/1521-4095(20020304)14:5<382::AID-ADMA382>3.0.CO;2-Y ↗
29. Kamat P. V. · J. Am. Chem. Soc. · 2004 · 126 · 1075710.1021/ja0479888 ↗
30. Kim J. Y. · J. Power Sources · 2008 · 176 · 39610.1016/j.jpowsour.2007.09.117 ↗
31. Frackowiak E. · Phys. Chem. Chem. Phys. · 2007 · 9 · 177410.1039/b618139m ↗
32. Khomenko V. · Electrochim. Acta · 2005 · 50 · 249910.1016/j.electacta.2004.10.078 ↗
33. Khomenko V. · Appl. Phys. A: Mater. Sci. Process. · 2006 · 82 · 56710.1007/s00339-005-3397-8 ↗
34. Pieta P. · Phys. Status Solidi B · 2008 · 245 · 229210.1002/pssb.200879633 ↗
35. Grodzka E. · Electrochim. Acta · 2009 · 54 · 562110.1016/j.electacta.2009.04.066 ↗
36. Pieta, P.; Obraztsov, I.; Sobczak, J.; Winkler, K.; Balch, A. L.; Das, S.; D’Souza, F.; Kutner, W.“Composite Material, Especially for Constructing Electrochemical Capacitors and Electrochemical Capacitor”, Polish Pat. Appl. No. P-393956 of 18 February, 2011.
37. Winkler K. · J. Mater. Chem. · 2007 · 17 · 57210.1039/B611932H ↗
38. Plonska M. E. · Mater. Chem. · 2003 · 15 · 412210.1021/cm034364c ↗
39. Prato M. · Tetrahedron · 1996 · 52 · 522110.1016/0040-4020(96)00126-3 ↗
40. D’Souza F. · J. Phys. Chem. A · 2002 · 106 · 64910.1021/jp0136415 ↗
41. Thompson M. · Analyst · 1991 · 116 · 88110.1039/AN9911600881 ↗
42. Thompson B. C. · Angew. Chem., Int. Ed. · 2008 · 47 · 5810.1002/anie.200702506 ↗
43. Zhang Y. Y. · J. Colloid Interface Sci. · 2001 · 236 · 28210.1006/jcis.2000.7397 ↗
44. Muramatsu H. · Anal. Chem. · 1988 · 60 · 214210.1021/ac00170a032 ↗
45. Shirley A. D. · Phys. Rev. B · 1972 · 5 · 470910.1103/PhysRevB.5.4709 ↗
46. Winkler K. · J. Solid State Electrochem. · 2006 · 10 · 76110.1007/s10008-006-0171-6 ↗
47. Winkler K. · J. Electrochem. Soc. · 2000 · 147 · 259710.1149/1.1393574 ↗
48. Winkler K. · J. Mater. Chem. · 2003 · 13 · 51810.1039/b208481n ↗
49. Marx K. A. · Biomacromolecules · 2003 · 4 · 109910.1021/bm020116i ↗
50. Muramatsu H. · J. Electroanal. Chem. · 1995 · 388 · 8910.1016/0022-0728(95)03881-G ↗
51. Balch A. L. · J. Am. Chem. Soc. · 1998 · 120 · 961410.1021/ja9805526 ↗
52. Kutner W. · Chem. Mater. · 2005 · 17 · 563510.1021/cm050829i ↗
53. Datta A. · Chem. Commun. · 1996 · 85110.1039/CC9960000851 ↗
54. Dresselhaus, M. S.; Dresselhaus, G.; Eklund, P. C.Vibrational Modes. InScience of Fullerenes and Carbon Nanotubes;Academic Press, Inc.:San Diego, CA, 1996; pp329–412.10.1016/B978-012221820-0/50011-3 ↗
55. Woodbridge C. M. · J. Phys. Chem. B · 2008 · 104 · 308510.1021/jp993235+ ↗
56. Weaver J. H. · Phys. Rev. Lett. · 1991 · 66 · 174110.1103/PhysRevLett.66.1741 ↗
57. Lang G. · Electrochim. Acta · 1991 · 36 · 84710.1016/0013-4686(91)85284-E ↗
58. Bard A. J. · 2001