Photoelectrochemical Analysis of the Dyed TiO2/Electrolyte Interface in Long-Term Stability of Dye-Sensitized Solar Cells
Source abstract
Abstract
The interface structure induced by electrolyte cations was found to play a significant role in determining the performance and stability of dye-sensitized solar cells. The trap state density in the nanostructure TiO 2 electrodes was affected by the adsorbed 1,2-dimethyl-3-propylimidazolium cation (DMPI + ) or alkali cations, such as Li +, Na +, K +, and Cs +, on the dyed TiO 2 electrode and was found to increase with the order of decreasing cation radius DMPI + < Cs + < K + < Na + < Li + . The change in interface structure resulted from the accumulation of the adsorbed cations to increase trap states in the nanostructure TiO 2 electrodes during long-term accelerated aging tests. The size effect of electrolyte cations on the cell performance suggested that the reduced surface cations, when small cations penetrated into titania lattice, resulted in a negative shift of the TiO 2 conduction band edge and a weaker interaction of Li + with dyes to obtain the decline in photocurrent and efficiency. The overall efficiency of dye-sensitized solar cells with large DMPI + in the electrolyte retained over 110% of its initial value after 2100 h. Also, no obvious differences in the efficiency for dye-sensitized solar cells with electrolyte cations, such as Li +, Cs +, and DMPI +, were observed after 1270 h under one sun light soaking in our experiment. The results suggested that large DMPI + chemisorbed on TiO 2 surface could not intercalate into the TiO 2 lattice for the enhanced stability of dye-sensitized solar cells in practical application.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: TiO2 Photocatalysis and Solar Cells · Advanced Photocatalysis Techniques · Advanced Nanomaterials in Catalysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Key Laboratory of Novel Thin Film Solar Cells, Institute of Plasma Physics, Chinese Academy of Sciences, P.O. Box 1126, Hefei, Anhui 230031, People’s Republic of China
School of Materials Science and Technology, Harbin Institute of Technology, Harbin, Heilongjiang 150001, People’s Republic of China
References (32)
Show source-provided references
1. O’Regan B. · Nature · 1991 · 353 · 73710.1038/353737a0 ↗
2. Nazeeruddin M. K. · J. Am. Chem. Soc. · 2005 · 127 · 1683510.1021/ja052467l ↗
3. Yum J. · Nano Today · 2010 · 5 · 9110.1016/j.nantod.2010.02.003 ↗
4. Hagfeldt A. · Chem. Rev. · 2010 · 110 · 659510.1021/cr900356p ↗
5. Asghar M. I. · Energy Environ. Sci. · 2010 · 3 · 41810.1039/b922801b ↗
6. Yella A. · Science · 2011 · 334 · 62910.1126/science.1209688 ↗
7. Watson D. F. · Coord. Chem. Rev. · 2004 · 248 · 139110.1016/j.ccr.2004.02.015 ↗
8. Li R. · Energy Environ. Sci. · 2010 · 3 · 176510.1039/c0ee00223b ↗
9. Zhang C. · J. Photochem. Photobiol., A: Chem. · 2010 · 213 · 8710.1016/j.jphotochem.2010.05.004 ↗
10. Fredin K. · J. Electroanal. Chem. · 2007 · 609 · 5510.1016/j.jelechem.2007.05.013 ↗
11. Kopidakis N. · J. Phys. Chem. B · 2006 · 110 · 1248510.1021/jp0607364 ↗
12. Jennings J. R. · J. Phys. Chem. C · 2010 · 114 · 171510.1021/jp9104129 ↗
13. Bai Y. · Langmuir · 2011 · 27 · 474910.1021/la200156m ↗
14. Kato N. · Sol. Energy Mater. Sol. Cells · 2009 · 93 · 89310.1016/j.solmat.2008.10.022 ↗
15. Gregg B. A. · Coord. Chem. Rev. · 2004 · 248 · 121510.1016/j.ccr.2004.02.009 ↗
16. Nakade S. · Langmuir · 2005 · 21 · 1141410.1021/la051483t ↗
17. Zhang C. · Electrochim. Acta · 2008 · 53 · 550310.1016/j.electacta.2008.03.016 ↗
18. Zhang C. · J. Phys. Chem. C · 2009 · 113 · 2177910.1021/jp909732f ↗
19. Kato N. · Sol. Energy Mater. Sol. Cells · 2009 · 93 · 89310.1016/j.solmat.2008.10.022 ↗
20. Nguyen P. T. · Sol. Energy Mater. Sol. Cells · 2010 · 94 · 158210.1016/j.solmat.2010.04.076 ↗
21. Alarcon H. · J. Phys. Chem. C · 2007 · 111 · 1327610.1021/jp072641n ↗
22. Zhang C. · J. Phys. Chem. C · 2011 · 115 · 1641810.1021/jp2024318 ↗
23. Liu W. · J. Phys. Chem. C · 2010 · 114 · 996510.1021/jp1003903 ↗
24. Schlichthorl G. · J. Phys. Chem. B · 1997 · 101 · 814110.1021/jp9714126 ↗
25. Liu Y. · Sol. Energy Mater. Sol. Cells · 1998 · 55 · 26710.1016/S0927-0248(98)00111-1 ↗
26. Shi Y. · Phys. Chem. Chem. Phys. · 2011 · 13 · 1459010.1039/c1cp21020c ↗
27. Bisquert J. · J. Phys. Chem. B · 2002 · 106 · 877410.1021/jp026058c ↗
28. Bisquert J. · J. Phys. Chem. B · 2004 · 108 · 231310.1021/jp035395y ↗
29. Harima Y. · Appl. Phys. Lett. · 2007 · 90 · 10351710.1063/1.2711659 ↗
30. Jennings J. R. · J. Phys. Chem. C · 2010 · 114 · 171510.1021/jp9104129 ↗
31. Hara K. · Sol. Energy Mater. Sol. Cells · 2005 · 85 · 21
32. Furube A. · J. Phys. Chem. B · 2005 · 109 · 1640610.1021/jp0513263 ↗