journal article·2009-02-05

Impact of Stoichiometry on the Hydrogen Storage Properties of LiNH2−LiBH4−MgH2 Ternary Composites

Andrea Sudik, Jun Yang, Donald J. Siegel, C. Wolverton, Roscoe O. Carter, A. R. Drews

Publisher page

Abstract

We recently reported (Yang, J.; et al. Angew. Chem., Int. Ed. 2008, 47, 882) a novel hydrogen storage composite involving a 2:1:1 LiNH 2:LiBH 4:MgH 2 ratio. On the basis of in-depth experimental and computational analysis, this composite was found to release hydrogen via a complex multistep reaction cascade, which seeded the products of a subsequent reversible hydrogen storage reaction. This so-called autocatalytic reaction sequence was found to result in favorable kinetics, ammonia attenuation, and partial low-temperature reversibility. Here, we extend our original study by examining the effects of reactant stoichiometry on the ensuing hydrogen storage desorption pathway and properties. In particular, we examine four (LiNH 2 ) X −(LiBH 4 ) Y −(MgH 2 ) Z composites, where X:Y:Z = 2:1:2, 1:1:1, 2:0.5:1, and 2:1:1 (original stoichiometry). For each sample, we characterize the postmilled mixtures using powder X-ray diffraction (PXRD) and infrared spectroscopy (IR) analyses and observe differences in the relative extent of two spontaneous milling-induced reactions. Variable-temperature hydrogen desorption data subsequently reveal that all composites exhibit a hydrogen release event at rather low temperature, liberating between 2.3 (1:1:1) and 3.6 (2:0.5:1) wt % by 200 °C. At higher temperatures (200−370 °C), the hydrogen release profiles differ considerably between composites and release a total of 5.7 (1:1:1) to 8.6 (2:0.5:1) wt %. Utilizing variable-temperature IR and PXRD data coupled with first-principles calculations, we propose a reaction pathway that is consistent with the observed phase progression and hydrogen desorption properties. From these data, we conclude that premilled reactant stoichiometry has a profound impact on reaction kinetics and high-temperature reaction evolution because of reactant availability. From this enhanced understanding of the desorption process, we recommend and test a stoichiometrically optimal ratio (3:1:1.5) which releases a total of 9.1 wt % hydrogen. Finally, we assess the reversibility (at 180 °C) of the four primary composites over two desorption cycles and find that only the 2:1:1 and 2:0.5:1 are reversible (3.5 wt % for 2:0.5:1).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen Storage and Materials · Hybrid Renewable Energy Systems · Ammonia Synthesis and Nitrogen Reduction

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Ford Motor Company, Research and Advanced Engineering, MD1170/RIC, P.O. Box 2053, Dearborn, Michigan 48121, and Materials Science and Engineering Department, Northwestern University, 2220 Campus Drive, Evanston, Illinois 60208

References (41)

Show source-provided references
1. Crabtree G. W. · Phys. Today · 2004 · 57 · 3910.1063/1.1878333 ↗
2. Targets for On-Board Hydrogen Storage Systems, 2007.U.S. Department of Energy Web site.http://www1.eere.energy.gov/hydrogenandfuelcells/storage/pdfs/targets_onboard_hydro_storage.pdf(accessed, July 11, 2008).
3. Züttel A. · J. Alloys Compd. · 2003 · 356 · 51510.1016/S0925-8388(02)01253-7 ↗
4. Züttel A. · J. Power Sources · 2003 · 118 · 110.1016/S0378-7753(03)00054-5 ↗
5. Nakamori Y. · Mater. Trans. · 2006 · 47 · 189810.2320/matertrans.47.1898 ↗
6. Bogdanović B. · J. Alloys Compd. · 1997 · 253 · 110.1016/S0925-8388(96)03049-6 ↗
7. Orimo S. · Chem. Rev. · 2007 · 107 · 411110.1021/cr0501846 ↗
8. Vajo J. J. · J. Phys. Chem. B · 2005 · 109 · 371910.1021/jp040769o ↗
9. Reilly J. J. · Inorg. Chem. · 1968 · 7 · 225410.1021/ic50069a016 ↗
10. Siegel D. J. · Phys. Rev. B · 2007 · 76 · 13410210.1103/PhysRevB.76.134102 ↗
11. Yang J. · J. Phys. Chem. C · 2007 · 111 · 1913410.1021/jp076434z ↗
12. Sun D. · J. Phys. Chem. B · 2003 · 107 · 1017610.1021/jp030637f ↗
13. Pinkerton F. E. · J. Alloys Compd. · 2007 · 433 · 28210.1016/j.jallcom.2006.06.108 ↗
14. Pinkerton F. E. · J. Phys. Chem. B · 2005 · 109 · 610.1021/jp0455475 ↗
15. Aoki M. · Appl. Phys. A: Mater. Sci. Process. · 2005 · 80 · 140910.1007/s00339-004-3194-9 ↗
16. Chater P. A. · J. Alloys Compd. · 2007 · 446 · 35010.1016/j.jallcom.2007.01.114 ↗
17. Luo W. · J. Alloys Compd. · 2004 · 381 · 28410.1016/j.jallcom.2004.03.119 ↗
18. Wu G. · Inorg. Chem. · 2007 · 46 · 51710.1021/ic060769y ↗
19. Yang J. · Angew. Chem., Int. Ed. · 2008 · 47 · 88210.1002/anie.200703756 ↗
20. Sudik A. · J. Phys. Chem. C · 2008 · 112 · 438410.1021/jp711393k ↗
21. Hu J. · Chem. Mater. · 2008 · 20 · 439810.1021/cm800584x ↗
22. Lewis G. J. · J. Alloys Compd. · 2007 · 446 · 35510.1016/j.jallcom.2007.04.028 ↗
23. Kresse G. · Phys. Rev. B · 1996 · 54 · 1116910.1103/PhysRevB.54.11169 ↗
24. Blöchl P. E. · Phys. Rev. B · 1994 · 50 · 1795310.1103/PhysRevB.50.17953 ↗
25. Perdew J. P. · Phys. Rev. B · 1992 · 46 · 667110.1103/PhysRevB.46.6671 ↗
26. Sorby M. H. · J. Alloys Compd. · 2007 · 428 · 29710.1016/j.jallcom.2006.03.037 ↗
27. Partin D. E. · J. Solid State Chem. · 1997 · 132 · 5610.1006/jssc.1997.7407 ↗
28. Rijssenbeek J. · J. Alloys Compd. · 2008 · 454 · 23310.1016/j.jallcom.2006.12.008 ↗
29. Siegel D. J. · Phys. Rev. B · 2007 · 75 · 01410110.1103/PhysRevB.75.014101 ↗
30. Wolverton C. · J. Phys.: Condens. Matter · 2008 · 20 · 064228
31. Chater P. A. · Chem. Commun. · 2006 · 243910.1039/b518243c ↗
32. Luo W. · J. Alloys Compd. · 2006 · 407 · 27410.1016/j.jallcom.2005.06.046 ↗
33. Yang J. · J. Alloys Compd. · 2007 · 430 · 33410.1016/j.jallcom.2006.05.039 ↗
34. While not performed, it is anticipated that if the 2:1:1 and 2:0.5:1 composites were held at <110°C for a longer period of time, reaction2would occur to completion, leaving no residual Li4BN3H10.
35. The disparity in temperature between kinetic desorption (Figure3, top) and TPD-MS (Figure3, bottom) data can be attributed to the pressure difference during data acquisition, 1 bar static for kinetic desorption and 100 sccm flowing Ar for TPD-MS experiments.
36. Chen P. · J. Phys. Chem. B · 2006 · 110 · 1422110.1021/jp061496v ↗
37. Meisner G. P. · J. Phys. Chem. B · 2006 · 110 · 418610.1021/jp056019b ↗
38. Luo W. · J. Alloys Compd. · 2007 · 440 · 35710.1016/j.jallcom.2006.09.057 ↗
39. Goubeau V. J. · Z. Anorg. Allg. Chem. · 1961 · 310 · 24810.1002/zaac.19613100410 ↗
40. Xiong Z. · Adv. Mater. · 2004 · 16 · 152210.1002/adma.200400571 ↗
41. Sudik A. · J. Phys. Chem. C · 2007 · 111 · 656810.1021/jp0683465 ↗