journal article·2023-08-24

Deterioration Analysis of Si Composite Anodes for All-Solid-State Batteries during Charge–Discharge by Auger Electron Spectroscopy and Scanning Electron Microscopy with Energy Dispersive Spectroscopy

Reiko Matsuda, Akihiro Tanaka, Kota Yanagihara, Yoshikazu Sasaki, Kazuhiro Hikima, Hiroyuki Muto, Atsunori Matsuda

The Journal of Physical Chemistry C· Volume 127· Issue 33
Publisher page

Abstract

Silicon (Si) is a promising anode material for lithium-ion batteries owing to its large capacity. Herein, all-solid-state full cells using Si composite anodes and sulfide solid electrolytes were fabricated and their charge–discharge performances were evaluated. From Auger electron spectroscopy and scanning electron microscopy with energy dispersive spectroscopy analyses of the cross section of the full cells, the presence of Li 2 O in the Si composite anodes was confirmed after the 50th charge–discharge cycle. Further, the relation between the capacity deterioration mechanism of the cells using the Si composite anodes and the generation of Li 2 O was studied.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Toyohashi University of Technology, 1-1 Hibarigaoka, Tempaku-cho, Toyohashi, Aichi 441-8580, Japan

JEOL Ltd., 3-1-2 Musashino, Akishima, Tokyo 196-8558, Japan

Funding

Advanced Low Carbon Technology Research and Development Program

References (24)

Show source-provided references
1. 10.1149/1.137902810.1149/1.1379028 ↗
2. 10.1021/ja508723m10.1021/ja508723m ↗
3. Hayashi, A.; Minami, K.; Ujiie, S.; Tatsumisago, M. Crystal structure of a superionic conductor, Li7P3S11–z glass-ceramic electrolytes. 2010, 356, 44–49, 2670–2673.10.1016/j.jnoncrysol.2010.04.048 ↗
4. 10.1038/srep0226110.1038/srep02261 ↗
5. 10.1021/acsaem.1c0316610.1021/acsaem.1c03166 ↗
6. 10.1016/j.est.2022.10654710.1016/j.est.2022.106547 ↗
7. 10.1039/c2jm16802b10.1039/c2jm16802b ↗
8. 10.1016/j.electacta.2022.14114910.1016/j.electacta.2022.141149 ↗
9. 10.1016/j.jpowsour.2019.04.02810.1016/j.jpowsour.2019.04.028 ↗
10. 10.1016/j.jpowsour.2014.08.10910.1016/j.jpowsour.2014.08.109 ↗
11. 10.1039/C0EE00281J10.1039/C0EE00281J ↗
12. 10.1016/j.nantod.2012.08.00410.1016/j.nantod.2012.08.004 ↗
13. 10.1016/j.jpowsour.2020.22859510.1016/j.jpowsour.2020.228595 ↗
14. 10.1021/acsenergylett.8b0199710.1021/acsenergylett.8b01997 ↗
15. 10.1021/acsami.1c2156110.1021/acsami.1c21561 ↗
16. 10.1016/j.jpowsour.2017.08.06510.1016/j.jpowsour.2017.08.065 ↗
17. 10.1016/j.ssi.2019.11504010.1016/j.ssi.2019.115040 ↗
18. Nishiguchi K. · Yousetsugakkai Ronbunsyu · 1991 · 9 · 537
19. 10.1016/j.jnucmat.2018.02.01010.1016/j.jnucmat.2018.02.010 ↗
20. 10.1016/j.ssi.2010.10.01310.1016/j.ssi.2010.10.013 ↗
21. 10.1016/j.apmt.2020.10091810.1016/j.apmt.2020.100918 ↗
22. 10.1016/j.ssi.2019.11518410.1016/j.ssi.2019.115184 ↗
23. 10.1016/j.jpowsour.2022.23108510.1016/j.jpowsour.2022.231085 ↗
24. 10.1021/acs.chemmater.9b0155010.1021/acs.chemmater.9b01550 ↗