journal article·2025-10

Temperature dependence of hydrogen embrittlement behavior in a medium-entropy alloy

Jingjing Zhou, Huijie Cheng, Ning Yao, Tiwen Lu, Xu Lu, Fenghua Lu, Wei Li, Binhan Sun, Xian-Cheng Zhang, Shan-Tung Tu

Acta Materialia· Volume 298
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High Entropy Alloys Studies · Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (83)

Show source-provided references
1. Current challenges in the utilization of hydrogen energy-a focused review on the issue of hydrogen-induced damage and embrittlement10.1016/j.adapen.2024.100168 ↗
2. Liquid hydrogen: a review on liquefaction, storage, transportation, and safety10.3390/en14185917 ↗
3. The influence of L12 ordered precipitates on hydrogen embrittlement behavior in CoCrNi-based medium entropy alloys10.1016/j.actamat.2023.119328 ↗
4. In-depth understanding in the effect of hydrogen on microstructural evolution, mechanical properties and fracture micro-mechanisms of advanced high-strength steels welded joints10.1016/j.corsci.2024.112112 ↗
5. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
6. Influence of 70 MPa hydrogen gas on SUS 630 from 77 K to 373 K by simple testing method
7. C. Qiu, Numerical and experimental study on a tube-in-tube heat exchanger working at liquid-hydrogen temperature with a large temperature span, (2023).10.1016/j.ijheatmasstransfer.2023.124089 ↗
8. Development advances in liquid rocket engines turbopump: a review10.4028/p-AF49pz ↗
9. High-entropy alloys: a review of mechanical properties and deformation mechanisms at cryogenic temperatures10.1007/s10853-022-07066-2 ↗
10. Effects of cryogenic temperature on tensile and impact properties in a medium-entropy VCoNi alloy10.1016/j.jmst.2021.02.034 ↗
11. Effects of grain size and cryogenic temperature on the strain hardening behavior of VCoNi medium-entropy alloys10.1007/s40195-023-01520-z ↗
12. Strong resistance to hydrogen embrittlement of high-entropy alloy10.1016/j.msea.2018.08.101 ↗
13. Current challenges and opportunities toward understanding hydrogen embrittlement mechanisms in advanced high-strength steels: a review
14. Hydrogen embrittlement and failure mechanisms of multi-principal element alloys: a review10.1016/j.jmst.2022.01.008 ↗
15. Chemical heterogeneity enhances hydrogen resistance in high-strength steels10.1038/s41563-021-01050-y ↗
16. Atomic mechanism and prediction of hydrogen embrittlement in iron10.1038/nmat3479 ↗
17. Hydrogen solubility and diffusivity in defective and amorphous metals10.1016/0079-6425(88)90010-2 ↗
18. Hydrogen embrittlement of metals10.1016/0025-5416(72)90109-7 ↗
19. Hydrogen embrittlement of α titanium: in situ TEM studies10.1016/0001-6160(88)90032-6 ↗
20. Hydrogenated vacancies lock dislocations in aluminium10.1038/ncomms13341 ↗
21. Semiempirical, quantum mechanical calculation of hydrogen embrittlement in metals10.1103/PhysRevLett.50.1285 ↗
22. Hydrogen embrittlement in different materials: a review10.1016/j.ijhydene.2018.09.201 ↗
23. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
24. Hydrogen-induced intergranular fracture of steels10.1016/S0013-7944(00)00124-7 ↗
25. Hydrogen-enhanced localized plasticity—A mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
26. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
27. Raja · 2011
28. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: overview10.1016/j.actamat.2018.12.013 ↗
29. The role of hydrogen and other interstitials in the mechanical behavior of metals: (1959 Edward De Mille Campbell Memorial Lecture)10.1007/s13632-016-0319-4 ↗
30. A mechanistic theory of hydrogen embrittlement of steels10.1002/bbpc.19720760864 ↗
31. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(01)00011-X ↗
32. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
33. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
34. Role of hydrogen and temperature in hydrogen embrittlement of equimolar CoCrFeMnNi high-entropy alloy10.1007/s12540-020-00752-3 ↗
35. Sluggish hydrogen diffusion and hydrogen decreasing stacking fault energy in a high-entropy alloy
36. Internal reversible hydrogen embrittlement of austenitic stainless steels based on type 316 at low temperatures10.2355/isijinternational.52.240 ↗
37. Hydrogen environment embrittlement on austenitic stainless steels from room temperature to low temperatures10.1088/1757-899X/102/1/012005 ↗
38. Dependence of hydrogen-induced lattice defects and hydrogen embrittlement of cold-drawn pearlitic steels on hydrogen trap state, temperature, strain rate and hydrogen content10.1016/j.actamat.2014.07.008 ↗
39. Heterogeneous precipitation behavior and stacking-fault-mediated deformation in a CoCrNi-based medium-entropy alloy10.1016/j.actamat.2017.07.029 ↗
40. Tuning the degree of chemical ordering in the solid solution of a complex concentrated alloy and its impact on mechanical properties10.1016/j.actamat.2021.116938 ↗
41. Quantifying the hydrogen embrittlement of pipeline steels for safety considerations10.1016/j.ijhydene.2012.05.143 ↗
42. Hydrogen embrittlement of industrial components: prediction, prevention, and models10.5006/1958 ↗
43. Effect of electrochemical charging on the hydrogen embrittlement susceptibility of alloy 71810.1016/j.actamat.2019.08.020 ↗
44. Effect of alloying elements on the hydrogen diffusion and trapping in high entropy alloys10.1016/j.scriptamat.2021.113957 ↗
45. A strong and ductile medium-entropy alloy resists hydrogen embrittlement and corrosion10.1038/s41467-020-16791-8 ↗
46. Ductile fracture: experiments and computations10.1016/j.ijplas.2010.04.001 ↗
47. Hydrogen induced microstructure, mechanical properties and cracking evolution in a novel CoCrNiMo medium-entropy alloy10.1016/j.jallcom.2023.168790 ↗
48. Exploring the hydrogen embrittlement behavior in nickel-economized austenitic stainless steel: investigating the role of manganese in modifying hydrogen-induced crack mechanisms10.1016/j.corsci.2023.111691 ↗
49. Ultrastrong medium-entropy single-phase alloys designed via severe lattice distortion10.1002/adma.201807142 ↗
50. Strain hardening by dynamic slip band refinement in a high-Mn lightweight steel10.1016/j.actamat.2016.06.037 ↗
51. Stacking fault energies of face-centered cubic concentrated solid solution alloys10.1016/j.actamat.2017.05.001 ↗
52. A critical review of the mechanical properties of CoCrNi-based medium-entropy alloys
53. Comparative study of hydrogen-induced intergranular fracture behavior in Ni and Cu–Ni alloy at ambient and cryogenic temperatures10.1016/j.msea.2019.138349 ↗
54. Effect of hydrogen and low temperature on fatigue crack growth of pipeline steels10.1016/j.engfracmech.2012.09.023 ↗
55. Hydrogen-assisted decohesion associated with nanosized grain boundary κ-carbides in a high-Mn lightweight steel10.1016/j.actamat.2022.118392 ↗
56. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
57. Dependence of hydrogen embrittlement mechanisms on microstructure-driven hydrogen distribution in medium Mn steels10.1016/j.actamat.2019.11.029 ↗
58. Dislocation modeling and acoustic emission observation of alternating ductile/brittle events in Fe-3wt%Si crystals10.1016/0956-7151(90)90255-F ↗
59. Revealing fracture mechanisms of medium manganese steels with and without delta-ferrite10.1016/j.actamat.2018.11.029 ↗
60. Hydrogen interactions with defects in crystalline solids10.1103/RevModPhys.64.559 ↗
61. Atomistic simulations of hydrogen embrittlement10.1016/j.ijhydene.2009.09.052 ↗
62. Hydrogen-enhanced compatibility constraint for intergranular failure in FCC FeNiCoCrMn high-entropy alloy10.1016/j.corsci.2021.109407 ↗
63. Hydrogen effects on plasticity10.1016/S1572-4859(09)01504-6 ↗
64. Hydrogen effects on the character of dislocations in high-purity aluminum10.1016/S1359-6454(99)00156-1 ↗
65. In situ electrochemical nanoindentation: a technique for local examination of hydrogen embrittlement10.1016/j.corsci.2007.05.026 ↗
66. Cross-slip process in fcc nickel with hydrogen in a stacking fault: an atomistic study using the embedded-atom method10.1103/PhysRevB.75.144110 ↗
67. In-situ investigation of the interaction between hydrogen and stacking faults in a bulk austenitic steel10.1016/j.actamat.2023.119441 ↗
68. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗
69. Mechanism of hydrogen embrittlement in a gamma-prime phase strengthened Fe–Ni based austenitic alloy10.1016/j.msea.2012.06.036 ↗
70. In-situ observation of hydrogen induced crack initiation in a nickel-based superalloy10.1016/j.scriptamat.2017.07.006 ↗
71. Hydrogen assisted crack initiation and propagation in a nickel-based superalloy10.1016/j.actamat.2016.05.003 ↗
72. Mechanisms of formation of ductile fatigue striations
73. On the formation of fatigue striations10.1007/BF00185199 ↗
74. The phenomena of rupture and flow in solids
75. Dislocation nucleation from a crack tip: an analysis based on the Peierls concept10.1016/S0022-5096(05)80012-2 ↗
76. Mechanism and prediction of hydrogen embrittlement in fcc stainless steels and high entropy alloys10.1103/PhysRevLett.127.175501 ↗
77. Dislocation emission from crack tips10.1080/01418619108204596 ↗
78. Internal hydrogen embrittlement of ultrahigh-strength AERMET 100 steel10.1007/s11661-003-0334-3 ↗
79. Quantitative tests revealing hydrogen-enhanced dislocation motion in α-iron10.1038/s41563-023-01537-w ↗
80. Temperature dependence of the flow stress of Fe–18Mn–0.6C–xAl twinning-induced plasticity steel10.1016/j.actamat.2013.07.042 ↗
81. A constitutive description of the deformation of copper based on the use of the mechanical threshold stress as an internal state variable10.1016/0001-6160(88)90030-2 ↗
82. Anomalous strain rate dependence of the serrated flow in Ni-H and Ni-C-H alloys10.1016/0956-7151(90)90206-V ↗
83. A model for the Portevin-Le Chatelier effect in substitutional alloys10.1016/0001-6160(72)90028-4 ↗