Selective Formation and SHG Intensity of Noncentrosymmetric and Centrosymmetric 1,1,2,2-Tetramethyl-1-(4-(N,N-dimethylamino)phenyl)-2-(2′-cyanophenyl)disilane Crystals under External Stimuli

Masaki Nishio, Masaki Shimada, Kenichiro Omoto, Toyotaka Nakae, Hiroaki Maeda, Mariko Miyachi, Yoshinori Yamanoi, Eiji Nishibori, Naofumi Nakayama, Hitoshi Goto, Tomonori Matsushita, Takashi Kondo, Mineyuki Hattori, Keiko Jimura, Shigenobu Hayashi, Hiroshi Nishihara

The Journal of Physical Chemistry C· Volume 124· Issue 32
Publisher page

Abstract

In this paper, selective formation of noncentrosymmetric ( Cc; α-crystal) and centrosymmetric ( P 2 1 / c; β-crystal) 1,1,2,2-tetramethyl-1-(4-( N, N -dimethylamino)phenyl)-2-(2′-cyanophenyl)disilane ( 1 ) was reported and both crystals were characterized by single-crystal X-ray diffraction (XRD) analysis, indicating multiple CH−π interactions created the crystal packing. The second harmonic generation (SHG) activity was attributed to the crystal packing and the orientation of dipole moment. Noncentrosymmetric crystal packing in a parallel manner exhibited SHG activity (intensity: 2.1 times vs urea). On the contrary, centrosymmetric structure in an antiparallel form showed no SHG activity (intensity: 0.0 times vs urea). As the calculated crystal energies of two polymorphs were very close to each other, the regulation of α- and β-crystals is succeeded through supercooled liquid-to-crystal and crystal-to-crystal phase transitions, controlling the SHG activity. Powder XRD and solid-state 13 C NMR spectroscopy were applied for the qualitative analysis of α- or β-polymorphs.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Crystallography and molecular interactions · Solid-state spectroscopy and crystallography · Nonlinear Optical Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemistry, School of Science, The University of Tokyo, 7-3-1 Hongo, Bunkyo-ku, Tokyo 113-0033, Japan

Division of Physics, Faculty of Pure and Applied Sciences, Tsukuba Research Center for Energy Materials Science (TREMS), University of Tsukuba, 1-1-1, Tennodai, Tsukuba, Ibaraki 305-8571, Japan

CONFLEX Corporation, 3-23-17 Takanawa, Minato-ku, Tokyo 108-0074, Japan

Department of Computer Science and Engineering, Toyohashi University of Technology, 1-1 Tempaku-cho, Toyohashi, Aichi 441-8580, Japan

Research Center for Advanced Science and Technology, The University of Tokyo, Tokyo 1153-8904, Japan

National Institute of Advanced Industrial Science and Technology (AIST), AIST Central 5, 1-1-1 Higashi, Tsukuba, Ibaraki 305-8565, Japan

Funding

Institute for Fermentation, Osaka · Ministry of Education, Culture, Sports, Science and Technology · MIKIYA Science and Technology Foundation · Core Research for Evolutional Science and Technology · Naohiko Fukuoka Memorial Foundation · Tonen General Sekiyu Research/ Development Encouragement & Scholarship Foundation · Yashima Environment Technology Foundation

References (69)

Show source-provided references
1. Bernstein J. · 2002
2. McCrone, W. C. Physics and Chemistry of the Organic Solid State, Fox, D.; Labes, M. M.; Weissberger, A., Eds. Wiley-Interscience: New York, 1965; Vol. 2, pp 725–767.
3. 10.1039/c3ra41559g10.1039/c3ra41559g ↗
4. 10.1002/chem.20180564110.1002/chem.201805641 ↗
5. Scheschkewitz D. · 201410.1007/978-3-319-03620-5 ↗
6. 10.1016/j.jphotochemrev.2008.06.00110.1016/j.jphotochemrev.2008.06.001 ↗
7. 10.1021/om040090710.1021/om0400907 ↗
8. 10.1246/cl.2006.102210.1246/cl.2006.1022 ↗
9. 10.1016/j.jphotochem.2010.12.02110.1016/j.jphotochem.2010.12.021 ↗
10. 10.1021/om300551t10.1021/om300551t ↗
11. 10.1039/C9DT03058A10.1039/C9DT03058A ↗
12. 10.1039/C8CC04962A10.1039/C8CC04962A ↗
13. 10.1039/C8DT00256H10.1039/C8DT00256H ↗
14. 10.1002/asia.20100054310.1002/asia.201000543 ↗
15. 10.1021/acs.jpcc.9b1071810.1021/acs.jpcc.9b10718 ↗
16. 10.3390/molecules2403052110.3390/molecules24030521 ↗
17. 10.1021/acsami.7b1480210.1021/acsami.7b14802 ↗
18. 10.1021/jacs.7b0567110.1021/jacs.7b05671 ↗
19. 10.1002/anie.20150938010.1002/anie.201509380 ↗
20. 10.1021/jo500029f10.1021/jo500029f ↗
21. 10.1039/c0cc00352b10.1039/c0cc00352b ↗
22. 10.1021/ja511177e10.1021/ja511177e ↗
23. Williams D. J. · 1983 · 233
24. Zyss J. · 1987
25. Zyss J. · 1994
26. Nalwa H. S. · 1996
27. 10.1246/bcsj.2014026410.1246/bcsj.20140264 ↗
28. Prasad P. N. · 1991
29. 10.1021/acs.cgd.7b0156010.1021/acs.cgd.7b01560 ↗
30. 10.1039/B712869J10.1039/B712869J ↗
31. 10.1021/cg025529h10.1021/cg025529h ↗
32. 10.1063/1.9771610.1063/1.97716 ↗
33. 10.1016/0022-0248(86)90549-X10.1016/0022-0248(86)90549-X ↗
34. 10.1021/cg400712s10.1021/cg400712s ↗
35. 10.1021/acs.cgd.7b0035310.1021/acs.cgd.7b00353 ↗
36. 10.5059/yukigoseikyokaishi.74.109810.5059/yukigoseikyokaishi.74.1098 ↗
37. 10.1063/1.165685710.1063/1.1656857 ↗
38. 10.1063/1.45092510.1063/1.450925 ↗
39. Previously, the crystal recrystallized from CHCl3 had non-centrosymmetric Pa packing (see reference (22)). Pa and Cc have almost similar packing patterns and cannot be distinguished by powder X-ray analysis.
40. CCDC 1030759 (α-form) and 1993486 ( β-form), contain the supplementary crystallographic data for this paper. These data can be obtained free of charge from the Cambridge crystallographic Data Center.
41. Sheldrick W. S. · 1989
42. 10.1021/ja00517a06310.1021/ja00517a063 ↗
43. 10.1021/ja056577410.1021/ja0565774 ↗
44. 10.1139/cjc-2014-055910.1139/cjc-2014-0559 ↗
45. 10.1021/ja512053t10.1021/ja512053t ↗
46. 10.1016/S0040-4020(01)89185-710.1016/S0040-4020(01)89185-7 ↗
47. 10.1039/b902318f10.1039/b902318f ↗
48. Myerson A. S. · 201910.1017/9781139026949 ↗
49. Goto, H.; Obata, S.; Nakayama, N.; Ohta, K. CONFLEX 8; CONFLEX Corporation: Tokyo, Japan, 2017.
50. 10.2477/jccj.H201610.2477/jccj.H2016 ↗
51. 10.2751/jcac.9.810.2751/jcac.9.8 ↗
52. 10.1063/1.491355710.1063/1.4913557 ↗
53. 10.1002/(SICI)1096-987X(199604)17:5/6<490::AID-JCC1>3.0.CO;2-P10.1002/(SICI)1096-987X(199604)17:5/6<490::AID-JCC1>3.0.CO;2-P ↗
54. 10.1002/(SICI)1096-987X(199604)17:5/6<520::AID-JCC2>3.0.CO;2-W10.1002/(SICI)1096-987X(199604)17:5/6<520::AID-JCC2>3.0.CO;2-W ↗
55. 10.1002/(SICI)1096-987X(199604)17:5/6<553::AID-JCC3>3.0.CO;2-T10.1002/(SICI)1096-987X(199604)17:5/6<553::AID-JCC3>3.0.CO;2-T ↗
56. 10.1002/(SICI)1096-987X(199604)17:5/6<587::AID-JCC4>3.0.CO;2-Q10.1002/(SICI)1096-987X(199604)17:5/6<587::AID-JCC4>3.0.CO;2-Q ↗
57. 10.1002/(SICI)1096-987X(199604)17:5/6<616::AID-JCC5>3.0.CO;2-X10.1002/(SICI)1096-987X(199604)17:5/6<616::AID-JCC5>3.0.CO;2-X ↗
58. 10.1002/(SICI)1096-987X(199905)20:7<720::AID-JCC7>3.0.CO;2-X10.1002/(SICI)1096-987X(199905)20:7<720::AID-JCC7>3.0.CO;2-X ↗
59. 10.1002/(SICI)1096-987X(199905)20:7<730::AID-JCC8>3.0.CO;2-T10.1002/(SICI)1096-987X(199905)20:7<730::AID-JCC8>3.0.CO;2-T ↗
60. Previously, we reported SHG intensity of α-crystal was 2.9 times vs urea (see: reference (22)). We measured the SHG intensity several times with an error of ca. ±0.5 (times vs urea).
61. 10.1021/cg500184210.1021/cg5001842 ↗
62. 10.1021/acs.jpcb.6b0409510.1021/acs.jpcb.6b04095 ↗
63. 10.1039/C8SC02723D10.1039/C8SC02723D ↗
64. 10.1021/acscentsci.5b0009110.1021/acscentsci.5b00091 ↗
65. 10.1002/(SICI)1521-3773(19991203)38:23<3440::AID-ANIE3440>3.0.CO;2-#10.1002/(SICI)1521-3773(19991203)38:23<3440::AID-ANIE3440>3.0.CO;2-# ↗
66. 10.1002/chem.20050141710.1002/chem.200501417 ↗
67. Methylene chloride, acetone, and pentane were tried as solvent of vapor diffusion instead of MeOH. In these solvents, the solvent is adsorbed and resulted in a solution state.
68. 10.1021/acs.cgd.8b0142510.1021/acs.cgd.8b01425 ↗
69. 10.1021/cg049766r10.1021/cg049766r ↗