journal article·2024-01

In-situ investigation of the interaction between hydrogen and stacking faults in a bulk austenitic steel

Hao Shi, Supriya Nandy, Huijie Cheng, Binhan Sun, Dirk Ponge

Acta Materialia· Volume 262
Publisher page

Abstract

The interaction between hydrogen (H) atoms and various microstructural defects remains a key to understand the H-induced damage and the subsequent premature failure of high-strength metallic materials. Previous studies on this subject are mainly focused on the in-situ probing of dislocations in a thin foil placed in an environmental transmission electron microscopy (TEM) cell. Here, a three-point bending test coupled with electron channeling contrast imaging (ECCI) has been applied to investigate the interaction of H with stacking faults (SFs) in a bulk high Mn austenitic steel. The expansion of some SFs, in terms of one partial dislocation movement within a partial dislocation pair, was observed on the H pre-charged sample when kept at a constant loading (i.e., a continuous H migration and likely build-up close to the pre-prepared notch tip). A temporal-resolved cross-correlation EBSD (CC-EBSD) measurement shows that the migration of H towards the notch tip region has a minor effect on the internal stress evolution. However, the local shear modulus (μ) and stacking fault energy (γSF) can be reduced by a local H segregation. Further theoretical calculation of SF ribbon width indicates that the reduction of μ by H results in the shrinkage of SF, while the H-induced reduction of γSF results in SF expansion at a lower resolved shear stress. The observed expansion of SF ribbons can be interrupted by a combined reduction of both μ and γSF due to H.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Hydrogen energy, economy and storage: review and recommendation10.1016/j.ijhydene.2019.04.068 ↗
2. Hydrogen energy systems: a critical review of technologies, applications, trends and challenges10.1016/j.rser.2021.111180 ↗
3. The production and application of hydrogen in steel industry10.1016/j.ijhydene.2020.12.123 ↗
4. Strategies for improving the sustainability of structural metals10.1038/s41586-019-1702-5 ↗
5. Hydrogen embrittlement mechanisms in advanced high strength steel10.1016/j.actamat.2021.117488 ↗
6. Effects of residual stress and plastic strain on hydrogen embrittlement of a stretch-formed TRIP-aided martensitic steel sheet10.1016/j.corsci.2020.108957 ↗
7. Overview of hydrogen embrittlement in high-Mn steels10.1016/j.ijhydene.2017.02.214 ↗
8. Dependence of hydrogen embrittlement mechanisms on microstructure-driven hydrogen distribution in medium Mn steels10.1016/j.actamat.2019.11.029 ↗
9. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
10. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation. I. Theoretical background10.1016/j.actamat.2007.05.047 ↗
11. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation: II. Experimental evidence and consequences10.1016/j.actamat.2007.05.033 ↗
12. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
13. A review on hydride precipitation in zirconium alloys10.1016/j.jnucmat.2015.07.014 ↗
14. Direct observation of hydrogen-enhanced plasticity in super duplex stainless steel by means of in situ electrochemical methods10.1016/j.scriptamat.2009.11.007 ↗
15. Mechanics of the hydrogendashdislocationdashimpurity interactions-I. Increasing shear modulus10.1016/0022-5096(94)00056-B ↗
16. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
17. Formation of shear bands and strain-induced martensite during plastic deformation of metastable austenitic stainless steels10.1016/j.actamat.2007.07.015 ↗
18. The influence of manganese content on the stacking fault and austenite/e-martensite interfacial energies in Fe–Mn–(Al–Si) steels investigated by experiment and theory10.1016/j.actamat.2014.01.001 ↗
19. Dislocation and twin substructure evolution during strain hardening of an Fe–22 wt.% Mn–0.6 wt.% C TWIP steel observed by electron channeling contrast imaging10.1016/j.actamat.2011.07.009 ↗
20. The influence of stacking fault energy on the microstructural and strain-hardening evolution of Fe–Mn–Al–Si steels during tensile deformation10.1016/j.actamat.2015.08.030 ↗
21. High Mn TWIP steel and medium Mn steel
22. Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
23. Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels10.1016/j.msea.2010.12.085 ↗
24. Effect of strain rate on hydrogen embrittlement susceptibility of twinning-induced plasticity steel pre-charged with high-pressure hydrogen gas10.1016/j.ijhydene.2016.06.259 ↗
25. Ferreira · 1997
26. Unravelling the effect of hydrogen on microstructure evolution under low-cycle fatigue in a high-manganese austenitic TWIP steel10.1016/j.ijplas.2019.11.004 ↗
27. Atomistic simulations of hydrogen effect on dissociation of screw dislocations in nickel10.1016/j.scriptamat.2005.01.044 ↗
28. Cross-slip process in fcc nickel with hydrogen in a stacking fault: An atomistic study using the embedded-atom method10.1103/PhysRevB.75.144110 ↗
29. Recent developments in the study of hydrogen embrittlement: Hydrogen effect on dislocation nucleation10.1016/j.actamat.2010.05.057 ↗
30. Atomistic simulations of the interactions of hydrogen with dislocations in fcc metals10.1103/PhysRevB.86.174102 ↗
31. Effect of hydrogen on the ideal shear strength in metals and its implications on plasticity: A first-principles study10.1016/j.ijhydene.2021.05.068 ↗
32. The key role played by dislocation core radius and energy in hydrogen interaction with dislocations10.1016/j.actamat.2019.12.033 ↗
33. A decohesion pathway for hydrogen embrittlement in nickel: Mechanism and quantitative prediction10.1016/j.actamat.2019.11.062 ↗
34. In situ transmission electron microscopy studies in gas/liquid environment
35. Discussion of some recent literature on hydrogen-embrittlement mechanisms: addressing common misunderstandings10.1515/corrrev-2019-0017 ↗
36. Theory and application of electron channelling contrast imaging under controlled diffraction conditions10.1016/j.actamat.2014.04.018 ↗
37. Origin of micrometer-scale dislocation motion during hydrogen desorption10.1126/sciadv.aaz1187 ↗
38. Observation of the hydrogen-dislocation interactions in a high-manganese steel after hydrogen adsorption and desorption
39. Numerical analysis of hydrogen transport near a blunting crack tip10.1016/0022-5096(89)90002-1 ↗
40. A general mechanism of martensitic nucleation: Part I. General concepts and the FCC→ HCP transformation
41. Effect of high-pressure torsion processing and annealing on hydrogen embrittlement of type 304 metastable austenitic stainless steel10.1007/s11661-010-0394-0 ↗
42. Correlating the five parameter grain boundary character distribution and the intergranular corrosion behaviour of a stainless steel using 3D orientation microscopy based on mechanical polishing serial sectioning10.1016/j.actamat.2018.06.044 ↗
43. High resolution mapping of strains and rotations using electron backscatter diffraction10.1179/174328406X130966 ↗
44. On the relationship between uniaxial yield strength and resolved shear stress in polycrystalline materials10.1016/S0022-3115(00)00378-0 ↗
45. Enhanced hydrogen concentrations ahead of rounded notches and cracks—competition between plastic strain and hydrostatic stress10.1016/S1359-6454(97)00364-9 ↗
46. The forces exerted on dislocations and the stress fields produced by them10.1103/PhysRev.80.436 ↗
47. On the stress dependence of partial dislocation separation and deformation microstructure in austenitic stainless steels10.1016/S1359-6454(03)00117-4 ↗
48. Effects of hydrogen and carbon on thermally activated deformation in nickel10.1016/0956-7151(92)90438-K ↗
49. Hydrogen effects on dislocation activity in austenitic stainless steel10.1016/j.actamat.2006.02.007 ↗
50. Atomistic study of the effect of hydrogen on dislocation emission from a mode II crack tip in alpha iron10.1016/j.ijmecsci.2009.09.042 ↗
51. Change in the electron structure caused by C, N and H atoms in iron and its effect on their interaction with dislocations10.1016/j.actamat.2005.07.028 ↗
52. The Peierls dislocation: Line energy, line tension, dissociation and deviation10.1016/S1359-6454(96)00340-0 ↗
53. Correlation between lattice distortion and friction stress in Ni-based equiatomic alloys10.1016/j.intermet.2017.03.011 ↗
54. The Peierls stress of dislocations: an analytic formula10.1103/PhysRevLett.78.266 ↗
55. Decoupling between Shockley partials and stacking faults strengthens multiprincipal element alloys10.1073/pnas.2114167118 ↗
56. Effect of hydrogen on shear modulus of polycrystalline α iron10.1016/0001-6160(77)90149-3 ↗
57. Twinning-induced plasticity (TWIP) steels10.1016/j.actamat.2017.06.046 ↗
58. Influence of hydrogen on the stacking-fault energy of an austenitic stainless steel10.4028/b-il4xtN ↗
59. Effect of hydrogen charging on dislocation behavior in Ni-Cr and Ni2Cr alloys10.1007/s11661-003-0235-5 ↗
60. Effect of hydrogen atom and hydrogen filled vacancies on stacking fault energy in γ-Fe by first-principles calculations10.1016/j.ijhydene.2019.04.229 ↗
61. An Fe–Ni–Cr–H interatomic potential and predictions of hydrogen-affected stacking fault energies in austenitic stainless steels10.1016/j.ijhydene.2021.09.261 ↗
62. Hull · 2001
63. The influence of L12 ordered precipitates on hydrogen embrittlement behavior in CoCrNi-based medium entropy alloys10.1016/j.actamat.2023.119328 ↗
64. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
65. Role of copper and aluminum additions on the hydrogen embrittlement susceptibility of austenitic Fe–Mn–C TWIP steels10.1016/j.corsci.2014.01.022 ↗