Modifications and Growth Mechanisms of Ultrathin Aluminum Oxide Films on NiAl in Water

Vincent Maurice, Inès Bennour, Sandrine Zanna, Lorena H. Klein, Philippe Marcus

The Journal of Physical Chemistry C· Volume 114· Issue 15
Publisher page

Abstract

X-ray photoelectron spectroscopy (XPS) and atomic force microscopy (AFM) have been combined to study the modifications and growth of alumina thin films on NiAl(001) induced by exposure to water vapor at low pressure (10 −6 mbar) and by immersion in ultrapure liquid water at room temperature. The film thickness and stoichiometry, as well as the alloy composition changes, were analyzed by angle-resolved XPS measurements. Ultrathin (∼0.7 nm) hydroxylated native oxide films were compared to thicker (∼4 nm) anhydrous and oxygen-deficient thermal oxide films grown at 900 °C under low air pressure (10 −4 mbar). The results show that immersion in liquid water causes the formation of one to two equivalent additional monolayers of aluminum oxide at the interface between the native oxide film and the alloy, suggesting anion transport along the oxide/alloy interface after entry at intergranular oxide sites. The hydroxylated oxide surface remains unchanged. In contrast, immersion of the thicker thermal oxide films in liquid water causes the formation of ∼3 equivalent additional aluminum oxide monolayers at the oxide/water interface, indicating cation transport through the film. AFM suggests a preferential growth at the boundaries between the oxide grains due to faster ion transport. The ∼4 nm thick thermal oxide film is inert when exposed to water at low vapor pressure (10 −6 mbar) confirming the pressure gap for the water-induced modifications of transitional alumina films. Exposure to ambient air partially annihilates the oxygen deficiency observed after formation as shown by the variation of the O−Al stoichiometry and core level shift effects.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Laboratoire de Physico-Chimie des Surfaces, CNRS (UMR 7045), Ecole Nationale Supérieure de Chimie de Paris (Chimie ParisTech), Université Pierre et Marie Curie, 11 rue Pierre et Marie Curie, 75005 Paris, France

References (48)

Show source-provided references
1. Padture N. P. · Science · 2002 · 296 · 28010.1126/science.1068609 ↗
2. Chambers S. A. · Science · 2002 · 297 · 82710.1126/science.1073404 ↗
3. Kelber J. · Surf. Sci. Rep. · 2007 · 62 · 27110.1016/j.surfrep.2006.12.003 ↗
4. Elam J. W. · J. Phys. Chem. B · 1998 · 102 · 700810.1021/jp981070j ↗
5. Liu P. · Surf. Sci. · 1998 · 417 · 5310.1016/S0039-6028(98)00661-X ↗
6. Niu C. · Surf. Sci. · 2000 · 465 · 16310.1016/S0039-6028(00)00728-7 ↗
7. Garza M. · Surf. Sci. · 2002 · 519 · 25910.1016/S0039-6028(02)02214-8 ↗
8. Libuda J. · Surf. Sci. · 1997 · 384 · 10610.1016/S0039-6028(97)00170-2 ↗
9. Tzvetkov G. · Surf. Sci. · 2003 · 543 · 13110.1016/S0039-6028(03)01029-X ↗
10. Ozensoy E. H. · J. Phys. Chem. B · 2005 · 109 · 343110.1021/jp0449206 ↗
11. Eng P. J. · Science · 2000 · 288 · 102910.1126/science.288.5468.1029 ↗
12. Hass K. C. · Science · 1998 · 282 · 26510.1126/science.282.5387.265 ↗
13. Qin F. · Surf. Sci. Lett. · 2004 · 565 · L27710.1016/j.susc.2004.06.203 ↗
14. Qin F. · Mater. High Temp. · 2004 · 21 · 19310.3184/096034004782748684 ↗
15. Kelber J. A. · Surf. Sci. · 2007 · 601 · 346410.1016/j.susc.2007.06.036 ↗
16. Maurice V. · Surf. Sci. · 2005 · 581 · 8810.1016/j.susc.2005.02.034 ↗
17. Cabrera N. · Rep. Prog. Phys. · 1949 · 12 · 16310.1088/0034-4885/12/1/308 ↗
18. Fehlner F. P. · Oxid. Met. · 1970 · 2 · 5910.1007/BF00603582 ↗
19. Maurice V. · Surf. Sci. · 2005 · 596 · 6110.1016/j.susc.2005.09.011 ↗
20. Maurice V. · Acta Materialia · 2007 · 55 · 331510.1016/j.actamat.2007.01.030 ↗
21. Doychak J. · Oxid. Met. · 1989 · 31 · 43110.1007/BF00666466 ↗
22. Presscott R. · Corros. Sci. · 1995 · 37 · 134110.1016/0010-938X(95)00034-H ↗
23. Pint B. A. · Solid State Ionics · 1995 · 78 · 9910.1016/0167-2738(95)00013-V ↗
24. Pint B. A. · Oxid. Met. · 1997 · 48 · 30310.1007/BF01670505 ↗
25. Grabke H. J. · Intermetallics · 1999 · 7 · 115310.1016/S0966-9795(99)00037-0 ↗
26. Rivoaland L. · Oxid. Met. · 2003 · 60 · 15910.1023/A:1024625615544 ↗
27. Hou P. · J. Am. Ceram. Soc. · 2003 · 86 · 66010.1111/j.1151-2916.2003.tb03355.x ↗
28. Światowska-Mrowiecka J. · Electrochim. Acta · 2007 · 52 · 564410.1016/j.electacta.2006.12.050 ↗
29. Tanuma S. · Surf. Interface Anal. · 1993 · 21 · 16510.1002/sia.740210302 ↗
30. Alexander M. R. · Surf. Interface Anal. · 2000 · 29 · 46810.1002/1096-9918(200007)29:7<468::AID-SIA890>3.0.CO;2-V ↗
31. Rotole J. A. · Surf. Sci. Spec. · 1998 · 5 · 1810.1116/1.1247852 ↗
32. Theo Kloprogge J. · J. Colloid Interface Sci. · 2006 · 296 · 57210.1016/j.jcis.2005.09.054 ↗
33. Venezia A. M. · Surf. Sci. · 1988 · 194 · 13610.1016/0039-6028(94)91250-5 ↗
34. Fremy N. · Surf. Interface Anal. · 2002 · 34 · 51910.1002/sia.1351 ↗
35. Fremy N. · J. Am. Ceram. Soc. · 2003 · 86 · 66910.1111/j.1151-2916.2003.tb03356.x ↗
36. Fremy, N.Study of the initial stages of oxidation of NiAl(001): growth of ultra-thin films of alumina and reactivity towards water vapor. Ph.D. Thesis, University Pierre et Marie Curie, Paris, 2004.
37. Gassmann P. · Surf. Sci. · 1994 · 319 · 9510.1016/0039-6028(94)90572-X ↗
38. Baümer M. · Prog. Surf. Sci. · 1999 · 61 · 12710.1016/S0079-6816(99)00012-X ↗
39. Franchy R. · Surf. Sci. Rep. · 2000 · 38 · 19510.1016/S0167-5729(99)00013-8 ↗
40. Stierle A. · Surf. Sci. · 2000 · 467 · 8510.1016/S0039-6028(00)00719-6 ↗
41. Ivey M. M. · J. Phys. Chem. B · 2003 · 107 · 639110.1021/jp022177g ↗
42. Hancock G. F. · Phys. Status Solidi A · 1971 · 4 · 14310.1002/pssa.2210040115 ↗
43. Lutze Birk A. · Scr. Metall. · 1975 · 9 · 76110.1016/0036-9748(75)90236-7 ↗
44. Song W. · Thin Solid Films · 2004 · 464 · 5210.1016/j.tsf.2004.06.017 ↗
45. Wu Y. · Surf. Sci. · 1996 · 365 · 33710.1016/0039-6028(96)00699-1 ↗
46. Giordiano L. · Phys. Rev. Lett. · 2008 · 101 · 02610210.1103/PhysRevLett.101.026102 ↗
47. Marcus P. · Corros. Sci. · 2008 · 50 · 269810.1016/j.corsci.2008.06.047 ↗
48. Seyeux A. · Electrochem. Solid State Lett. · 2009 · 12 · C2510.1149/1.3186644 ↗