Small-Molecule (CO, H2) Electro-Oxidation as an Electrochemical Tool for Characterization of Ni@Pt/C with Different Pt Coverages
Source abstract
Abstract
The electrochemical oxidation processes of CO and H 2 have been used as probes to assess the surface states of carbon-supported Ni@Pt core-shell catalysts (Ni@Pt/C) with different Pt coverages in electrochemical environments. The CO-stripping cyclic voltammograms (CVs) of Ni@Pt/C catalysts present split double peaks representing two different states of Pt atoms on Ni-core particles. The current peaks in the CO-stripping CVs of Ni@Pt/C catalysts under relatively more positive potentials are consistent with that of Pt/C (a single peak), which indicates that some of the Pt atoms on Ni-core particles behave like pure Pt as isolated Pt atoms. The shoulder peaks shift toward more negative potentials, which may be because these Pt atoms on Ni-core particles assemble Pt–Pt bonds, resulting in Pt lattice constriction. The more positive current peaks in the CO-stripping CVs of Ni@Pt/C catalysts are predominant with lower Pt coverage, and with increasing Pt surface coverage, the more negative current peaks become prominent, which illustrates the integrity of Pt–Pt ensembles with neighboring Pt atoms. This phenomenon can be demonstrated by the schematic diagram of changes in the morphologies of Ni@Pt/C catalysts with increasing Pt coverage. HOR measurements further exhibit clearly regular patterns; here, the exchange current density ( j 0 ) values of Ni@Pt/C catalysts decrease with increasing Pt coverage and correspond to that of Pt/C at high Pt coverage. This result can be explained by the existence of nickel hydroxides and hydrogen spillover.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · CO2 Reduction Techniques and Catalysts · Electrochemical Analysis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Chemistry, Henan Polytechnic University, Jiaozuo 454000, China
College of Chemistry and molecular Science, Wuhan University, Wuhan 430072, China
Funding
Ministry of Science and Technology of the People's Republic of China · Education Department Henan Province
References (47)
Show source-provided references
1. Wang J. X. · J. Am. Chem. Soc. · 2009 · 131 · 1729810.1021/ja9067645 ↗
2. Zhou W. P. · J. Am. Chem. Soc. · 2009 · 131 · 1275510.1021/ja9039746 ↗
3. Shao M. · J. Am. Chem. Soc. · 2010 · 132 · 925310.1021/ja101966a ↗
4. Wang X. · J. Am. Chem. Soc. · 2013 · 135 · 593810.1021/ja312382h ↗
5. Xing Y. · J. Phys. Chem. Lett. · 2010 · 1 · 323810.1021/jz101297r ↗
6. Chol S. · ACS Nano · 2014 · 8 · 1036310.1021/nn5036894 ↗
7. Chen Y. · J. Phys. Chem. C · 2008 · 112 · 164510.1021/jp709886y ↗
8. Chen Y. · J. Phys. Chem. C · 2011 · 115 · 2407310.1021/jp207828n ↗
9. Lin R. · J. Power Sources · 2013 · 223 · 19010.1016/j.jpowsour.2012.09.073 ↗
10. Li Z. S. · Int. J. Hydrogen Energy · 2012 · 37 · 1415210.1016/j.ijhydene.2012.07.100 ↗
11. Henry J. B. · ACS Catal. · 2012 · 2 · 145710.1021/cs300165t ↗
12. Neergat M. · J. Electrochem. Soc. · 2012 · 159 · 23410.1149/2.039207jes ↗
13. Yang L. J. · J. Phys. Chem. C · 2013 · 117 · 174810.1021/jp309990e ↗
14. Koenigsmann C. · J. Am. Chem. Soc. · 2011 · 133 · 978310.1021/ja111130t ↗
15. Huang R. · J. Phys. Chem. C · 2012 · 116 · 866410.1021/jp3015639 ↗
16. Cochell T. · J. Phys. Chem. C · 2013 · 117 · 386510.1021/jp3126522 ↗
17. Zhang J. · Angew. Chem., Int. Ed. · 2005 · 44 · 213210.1002/anie.200462335 ↗
18. He C. Y. · Nano Energy · 2014 · 8 · 5210.1016/j.nanoen.2014.05.016 ↗
19. Oezaslan M. · J. Phys. Chem. Lett. · 2013 · 4 · 327310.1021/jz4014135 ↗
20. Wang X. M. · J. Am. Chem. Soc. · 2013 · 135 · 593810.1021/ja312382h ↗
21. An W. · J. Phys. Chem. C · 2013 · 117 · 1614410.1021/jp4057785 ↗
22. Callejas-Tovar R. · J. Phys. Chem. C · 2012 · 116 · 1441410.1021/jp303135j ↗
23. Kettner M. · J. Phys. Chem. C · 2012 · 116 · 1543210.1021/jp303773y ↗
24. Nagamatsu S. · J. Phys. Chem. C · 2013 · 117 · 1309410.1021/jp402438e ↗
25. Cuesta A. · J. Electroanal. Chem. · 2006 · 586 · 18410.1016/j.jelechem.2005.10.006 ↗
26. Vidakovic T. · Electrochim. Acta · 2007 · 52 · 560610.1016/j.electacta.2006.12.057 ↗
27. Chatenet M. · Electrochim. Acta · 2007 · 53 · 36910.1016/j.electacta.2007.01.029 ↗
28. Ochal P. · J. Electronanl. Chem. · 2011 · 655 · 40
29. Park I. S. · Catal. Today · 2013 · 202 · 17510.1016/j.cattod.2012.05.045 ↗
30. Reshetenko T. V. · J. Power Sources · 2014 · 269 · 34410.1016/j.jpowsour.2014.06.146 ↗
31. Kadyk T. · Electrochim. Acta · 2011 · 56 · 1059310.1016/j.electacta.2011.05.005 ↗
32. Cui G. F. · J. Power Sources · 2011 · 196 · 612510.1016/j.jpowsour.2011.03.042 ↗
33. Muthuswamy N. · Int. J. Hydrogen Energy · 2013 · 38 · 1663110.1016/j.ijhydene.2013.02.056 ↗
34. Lopez-Cudero A. · J. Electroanal. Chem. · 2006 · 586 · 20410.1016/j.jelechem.2005.10.003 ↗
35. Yu Y. · J. Phys. Chem. C · 2012 · 116 · 385110.1021/jp210851b ↗
36. Dai Y. · Electrochim. Acta · 2013 · 89 · 74410.1016/j.electacta.2012.11.011 ↗
37. Shao M. · J. Power Sources · 2011 · 196 · 243310.1016/j.jpowsour.2010.10.093 ↗
38. Kumar S. M. S. · Int. J. Hydrogen Energy · 2011 · 36 · 545310.1016/j.ijhydene.2011.01.124 ↗
39. Hu Y. · J. Electroanal. Chem. · 2014 · 726 · 5510.1016/j.jelechem.2014.05.012 ↗
40. Du B. C. · J. Phys. Chem. B · 2005 · 109 · 1777510.1021/jp0537310 ↗
41. van der Vliet D. F. · Angew. Chem., Int. Ed. · 2012 · 51 · 313910.1002/anie.201107668 ↗
42. Wang C. · Nano Lett. · 2011 · 11 · 91910.1021/nl102369k ↗
43. Wang C. · J. Am. Chem. Soc. · 2011 · 133 · 1439610.1021/ja2047655 ↗
44. Sun Y. · Phys. Chem. Chem. Phys. · 2012 · 14 · 227810.1039/c2cp22761d ↗
45. Chen S. L. · J. Phys. Chem. B · 2004 · 108 · 1398410.1021/jp048641u ↗
46. Park K. W. · J. Phys. Chem. B · 2002 · 106 · 186910.1021/jp013168v ↗
47. Liang Y. M. · J. Phys. Chem. B · 2006 · 118 · 782810.1021/jp0602732 ↗