Abstract

This article investigates the dehydrogenation behavior of the LiBH 4 –YH 3 composite under various early-stage Ar back-pressure conditions. It is clearly observed that a minute change in early-stage atmosphere greatly affects the overall dehydrogenation reaction of the composite. Free boron and Li 2 B 12 H 12 start to form in turn as the partial dehydrogenation products around 400 °C under static vacuum or low Ar back pressure. The formation of Li 2 B 12 H 12 greatly increases the activation energy for the dehydrogenation reaction between LiBH 4 and YH 3 into LiH and YB 4, hence significantly retarding the reaction. The formation of B just slightly increases the incubation period of the reaction. The formation of Li 2 B 12 H 12 is effectively suppressed by initially applying Ar back pressure above 0.1 MPa.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen Storage and Materials · Superconductivity in MgB2 and Alloys · Superconducting Materials and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

High Temperature Energy Materials Research Center, Korea Institute of Science and Technology, Seoul 136-791, Republic of Korea

Department of Materials Science and Engineering, Seoul National University, Seoul 151-742, Republic of Korea

References (18)

Show source-provided references
1. Züttel A. · J. Power Sources · 2003 · 118 · 110.1016/S0378-7753(03)00054-5 ↗
2. Orimo S. · J. Alloys Compd. · 2005 · 404 · 42710.1016/j.jallcom.2004.10.091 ↗
3. Mauron P. · J. Phys. Chem. B · 2008 · 112 · 90610.1021/jp077572r ↗
4. Barkhordarian G. · J. Alloys Compd. · 2007 · 440 · L1810.1016/j.jallcom.2006.09.048 ↗
5. Vajo J. J. · J. Phys. Chem. B · 2005 · 109 · 371910.1021/jp040769o ↗
6. Cho Y. W. · CALPHAD · 2006 · 30 · 6510.1016/j.calphad.2005.10.002 ↗
7. Shim J. -H. · J. Phys. Chem. Lett. · 2010 · 1 · 5910.1021/jz900012n ↗
8. Kim K. -B. · Chem. Commun. · 2011 · 47 · 983110.1039/c1cc14072h ↗
9. Shim J. -H. · J. Alloys Compd. · 2012 · 510 · L910.1016/j.jallcom.2011.09.005 ↗
10. Nakagawa T. · J. Alloys Compd. · 2007 · 446 · 30610.1016/j.jallcom.2007.02.097 ↗
11. Pinkerton F. E. · J. Phys. Chem. C · 2007 · 111 · 1288110.1021/jp0742867 ↗
12. Bösenberg U. · J. Phys. Chem. C · 2010 · 114 · 1521210.1021/jp104814u ↗
13. Yan Y. · J. Phys. Chem. C · 2011 · 115 · 1941910.1021/jp205450c ↗
14. Ohba N. · Phys. Rev. B · 2006 · 74 · 075110–110.1103/PhysRevB.74.075110 ↗
15. Hwang S. -J. · J. Phys. Chem. C · 2008 · 112 · 316410.1021/jp710894t ↗
16. Kostka J. · J. Phys. Chem. C · 2007 · 111 · 1402610.1021/jp073783k ↗
17. Friedrichs O. · Chem. Mater. · 2010 · 22 · 326510.1021/cm100536a ↗
18. Kissinger H. E. · Anal. Chem. · 1957 · 29 · 170210.1021/ac60131a045 ↗