Abstract

To investigate the effects of hydrogen (H) on the mechanical properties of 316L austenitic stainless steel (316L) additively manufactured using laser-powder bed fusion (L-PBF), tensile, nanoindentation, and micropillar compression tests were performed on samples in both the as-built (AB) and H-charged (HC) conditions. Microstructural characterization revealed that the electrochemical H charging exerted marginal effects on grains, phases, and overall dislocation densities of L-PBF 316L. However, the dislocation networks inherent to L-PBF 316L appear to disentangle upon H charging and are distributed more homogeneously through the matrix. Mechanical test results showed that H charging results in a marginal reduction in hardness and strength, indicating H-induced softening, possibly due to the elastic shielding effects of H that weaken the interactions between dislocations. The elastic shielding effect and the enhanced slip planarity, facilitate the H accumulation along slip bands and twins, promote H-enhanced localized plasticity, resulting cracking when a critical H concentration is reached. This, in turn, aids in H embrittlement mechanism that results in a significant loss in ductility upon H charging. A detailed discussion of all these micromechanisms is presented.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (99)

Show source-provided references
1. The hydrogen embrittlement of metals10.1016/0079-6425(61)90005-6 ↗
2. Hydrogen embrittlement in different materials: a review10.1016/j.ijhydene.2018.09.201 ↗
3. Resistance of CoCrFeMnNi high-entropy alloy to gaseous hydrogen embrittlement10.1016/j.scriptamat.2017.03.029 ↗
4. Influence of plastic deformation on hydrogen diffusion and permeation in stainless steels10.1016/0001-6160(89)90211-3 ↗
5. Effect of strain-induced martensite on tensile properties and hydrogen embrittlement of 304 stainless steel10.1007/s11661-015-3198-4 ↗
6. Effect of strain-induced martensite on hydrogen environment embrittlement of sensitized austenitic stainless steels at low temperatures10.1016/S1359-6454(98)00136-0 ↗
7. A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)10.1007/BF02642048 ↗
8. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
9. Hydrogen-enhanced localization of plasticity in an austenitic stainless steel10.1007/BF02669644 ↗
10. The synergistic action of HELP and HEDE mechanisms of hydrogen embrittlement in steels
11. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
12. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
13. Directed energy deposition of metals: processing, microstructures, and mechanical properties10.1080/09506608.2022.2097411 ↗
14. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
15. Mesostructure engineering in additive manufacturing of alloys10.1016/j.scriptamat.2023.115429 ↗
16. Additively manufactured hierarchical stainless steels with high strength and ductility10.1038/nmat5021 ↗
17. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
18. Superior resistance to hydrogen damage for selective laser melted 316L stainless steel in a proton exchange membrane fuel cell environment10.1016/j.corsci.2019.108425 ↗
19. Effect of additive manufacturing and subsequent heat and/or surface treatment on the hydrogen embrittlement sensitivity of 316L austenitic stainless steel10.1016/j.ijhydene.2023.05.215 ↗
20. The dependence of hydrogen embrittlement on hydrogen transport in selective laser melted 304L stainless steel10.1016/j.ijhydene.2021.02.035 ↗
21. A micropillar compression investigation into the plastic flow properties of additively manufactured alloys10.1016/j.actamat.2022.118290 ↗
22. Selective laser melting of stainless steel 316L with low porosity and high build rates10.1016/j.matdes.2016.05.035 ↗
23. Hydrogen-related phase transformations in austenitic stainless steels10.1007/BF02642872 ↗
24. Effects of Ni/Cu replacement on improvement of tensile and hydrogen-embrittlement properties in austenitic stainless steels10.1016/j.actamat.2022.118093 ↗
25. The origin of high-density dislocations in additively manufactured metals10.1080/21663831.2020.1751739 ↗
26. Mechanical behavior of selective laser melted 316L stainless steel10.1016/j.msea.2017.04.058 ↗
27. Mechanical properties and corrosion behavior of selective laser melted 316L stainless steel after different heat treatment processes10.1016/j.jmst.2019.03.003 ↗
28. Comparative study of hydrogen embrittlement resistance between additively and conventionally manufactured 304L austenitic stainless steels10.1016/j.msea.2020.140499 ↗
29. Hydrogen-induced softening in nanocrystalline Ni investigated by nanoindentation10.1080/14786435.2016.1159743 ↗
30. Rate-dependent mechanical behavior of single-, bi-, twinned-, and poly-crystals of CoCrFeNi high-entropy alloy10.1016/j.jmst.2021.12.025 ↗
31. Small-volume aluminum alloys with native oxide shell deliver unprecedented strength and toughness10.1016/j.actamat.2016.12.055 ↗
32. Interpreting the stress–strain response of Al micropillars through gradient plasticity10.1016/j.msea.2013.10.082 ↗
33. Influence of bulk pre-straining on the size effect in nickel compression pillars10.1016/j.msea.2012.08.055 ↗
34. Hydrogen effects on dislocation activity in austenitic stainless steel10.1016/j.actamat.2006.02.007 ↗
35. In-situ study of initiation and extension of nano-thick defect-free channels in irradiated nickel10.1016/j.jmst.2020.03.057 ↗
36. Hydrogen effects on the character of dislocations in high-purity aluminum10.1016/S1359-6454(99)00156-1 ↗
37. An Fe–Ni–Cr–H interatomic potential and predictions of hydrogen-affected stacking fault energies in austenitic stainless steels10.1016/j.ijhydene.2021.09.261 ↗
38. Hydrogen-induced ductilization in a novel austenitic lightweight TWIP steel10.1016/j.scriptamat.2022.114629 ↗
39. Hydrogen-assisted failure in Inconel 718 fabricated by laser powder bed fusion: the role of solidification substructure in the embrittlement10.1016/j.scriptamat.2021.114308 ↗
40. Effect of hydrogen-induced surface steps on the nanomechanical behavior of a CoCrFeMnNi high-entropy alloy revealed by in-situ electrochemical nanoindentation10.1016/j.intermet.2019.106605 ↗
41. A modified electrochemical nanoindentation setup for probing hydrogen-material interaction demonstrated on a nickel-based alloy10.1007/s11837-020-04104-9 ↗
42. Direct observation of hydrogen-enhanced plasticity in super duplex stainless steel by means of in situ electrochemical methods10.1016/j.scriptamat.2009.11.007 ↗
43. The role of hydrogen in hardening/softening steel: influence of the charging process10.1016/j.scriptamat.2015.05.017 ↗
44. Influences of hydrogen charging method on the hydrogen distribution and nanomechanical properties of face-centered cubic high-entropy alloy: a comparative study10.1016/j.scriptamat.2019.04.025 ↗
45. Crank · 1979
46. X-ray diffraction measurement of the stacking fault energy reduction induced by hydrogen in an AISI 304 steel10.1016/S1359-6462(97)00332-1 ↗
47. Phase relations in the hydrogen-austenite system10.1016/0956-7151(93)90393-7 ↗
48. Porosity control in 316L stainless steel using cold and hot isostatic pressing10.1016/j.matdes.2017.10.025 ↗
49. Effect of dislocation cell walls on hydrogen adsorption, hydrogen trapping and hydrogen embrittlement resistance10.1016/j.corsci.2020.108428 ↗
50. Effects of alloy composition and strain hardening on tensile fracture of hydrogen-precharged type 316 stainless steels10.1016/j.ijhydene.2007.10.046 ↗
51. Hydrogen embrittlement of additively manufactured austenitic stainless steel 316L10.1016/j.corsci.2021.109790 ↗
52. Interaction of hydrogen with dislocation pile-ups and hydrogen induced softening of pure iron10.1016/S1359-6462(00)00398-5 ↗
53. Solid solution softening and hardening by mobile solute atoms with special focus on hydrogen10.1016/j.scriptamat.2012.07.022 ↗
54. Stress-dependent hardening-to-softening transition of hydrogen effects in nanoindentation of a linepipe steel10.1016/j.ijhydene.2013.11.060 ↗
55. Hydrogen effect against hydrogen embrittlement10.1007/s11661-010-0275-6 ↗
56. A possible explanation for the contradictory results of hydrogen effects on macroscopic deformation10.1016/j.ijpvp.2012.08.001 ↗
57. The effect of residual hydrogen on hydrogenation behavior of titanium thin films10.1016/j.scriptamat.2010.01.037 ↗
58. The effect of hydrogen atoms on the screw dislocation mobility in bcc iron: a first-principles study10.1016/j.actamat.2013.07.064 ↗
59. Mechanism of hydrogen-induced softening and hardening in iron
60. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
61. Hydrogen-enhanced local plasticity in aluminum: an ab initio study10.1103/PhysRevLett.87.095501 ↗
62. Hydrogen embrittlement I. Analysis of hydrogen-enhanced localized plasticity: effect of hydrogen on the velocity of screw dislocations in α-Fe
63. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
64. Mechanism of hardening and damage initiation in oxygen embrittlement of body-centred-cubic niobium10.1016/j.actamat.2019.02.030 ↗
65. Ab initio investigation of the screw dislocation-hydrogen interaction in bcc tungsten and iron10.1016/j.actamat.2022.118048 ↗
66. Hydrogen induced dislocation core reconstruction in bcc tungsten10.1016/j.actamat.2022.117622 ↗
67. Quantitative tests revealing hydrogen-enhanced dislocation motion in α-iron10.1038/s41563-023-01537-w ↗
68. Numerical simulations of hydrogen–dislocation interactions in fcc stainless steels.: part II: hydrogen effects on crack tip plasticity at a stress corrosion crack10.1016/S1359-6454(02)00009-5 ↗
69. Effects of strain rate and temperature on tensile behavior of hydrogen-charged SA508 Cl. 3 pressure vessel steel10.1016/S0921-5093(02)00737-2 ↗
70. Antagonist softening and hardening effects of hydrogen investigated using nanoindentation on cyclically pre-strained nickel single crystal10.1016/j.msea.2020.140480 ↗
71. Investigation of hydrogen-deformation interactions in β-21S titanium alloy using thermal desorption spectroscopy10.1016/j.jallcom.2006.10.026 ↗
72. Activation volume and density of mobile dislocations in hydrogen-charged iron10.1016/j.actamat.2013.05.007 ↗
73. A comparative study of additive manufactured and wrought SS316L: pre-existing dislocations and grain boundary characteristics10.1016/j.msea.2021.142546 ↗
74. Mechanism of high yield strength and yield ratio of 316 L stainless steel by additive manufacturing10.1016/j.msea.2018.12.092 ↗
75. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray debye-scherrer spectrum10.1080/14786435608238074 ↗
76. Constitutive modeling of cellular-structured metals produced by additive manufacturing10.1016/j.actamat.2022.118421 ↗
77. Strengthening and hardening mechanisms of additively manufactured stainless steels: the role of cell sizes10.1016/j.scriptamat.2019.10.005 ↗
78. Hydrogen uptake in 316L stainless steel: consequences on the tensile properties10.1016/j.corsci.2005.11.004 ↗
79. Hydrogen uptake and its influence in selective laser melted austenitic stainless steel: a nanoindentation study10.1016/j.scriptamat.2020.113718 ↗
80. Effect of cell wall on hydrogen response in CoCrFeMnNi high-entropy alloy additively manufactured by selective laser melting10.1016/j.jallcom.2022.166735 ↗
81. Improving the hydrogen embrittlement resistance of a selective laser melted high-entropy alloy via modifying the cellular structures10.1016/j.corsci.2021.109695 ↗
82. Hydrogen embrittlement behavior of selective laser-melted Inconel 718 alloy10.1016/j.jmrt.2022.12.196 ↗
83. Hydrogen trapping and micromechanical behavior in additively manufactured CoCrFeNi high-entropy alloy in as-built and pre-strained conditions10.1016/j.actamat.2024.119886 ↗
84. Crystallographic-orientation-dependent tensile behaviours of stainless steel 316L fabricated by laser powder bed fusion10.1016/j.msea.2019.138395 ↗
85. Micropillar compression investigation on the mechanical behavior of Ni manufactured using laser powder bed fusion10.1016/j.msea.2023.145269 ↗
86. Role of the solidification cells on the yield strength of the Al-Si-Mg alloy manufactured using laser powder bed fusion: a micropillar compression study10.1016/j.scriptamat.2023.115566 ↗
87. Effect of initial dislocation density on the plastic deformation response of 316L stainless steel manufactured by directed energy deposition10.1016/j.msea.2022.143591 ↗
88. Hydrogen transport by dislocations10.1007/BF02644079 ↗
89. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(01)00011-X ↗
90. The effect of hydrogen on the slip character of nickel10.1016/0001-6160(80)90105-4 ↗
91. Dislocation network in additive manufactured steel breaks strength–ductility trade-off10.1016/j.mattod.2017.11.004 ↗
92. The stress field of an array of parallel dislocation pile-ups: implications for grain boundary hardening and excess dislocation distributions10.1016/j.actamat.2010.04.026 ↗
93. Distinct effects of in-situ and ex-situ hydrogen charging methods on the mechanical behavior of CoCrFeNi high-entropy alloy fabricated by laser-powder bed fusion10.1016/j.jallcom.2023.168858 ↗
94. Recent advances on hydrogen embrittlement of structural materials10.1007/s10704-015-0068-4 ↗
95. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage” fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
96. Hydrogen embrittlement of low carbon structural steel10.1016/j.mspro.2014.06.190 ↗
97. Strain-induced twins and martensite: effects on hydrogen embrittlement of selective laser melted (SLM) 316L stainless steel10.1016/j.corsci.2022.110669 ↗
98. Hydrogen embrittlement of catholically hydrogen-precharged 304L austenitic stainless steel: effect of plastic pre-strain10.1016/j.ijhydene.2014.04.122 ↗
99. A novel methodology to estimate hydrogen diffusivity and its applications in revealing hydrogen effects in CoCrNi medium-entropy alloy versus 316L stainless steel10.1016/j.ijplas.2023.103737 ↗