journal article·2022-10Open access

Hydrogen-enhanced grain boundary vacancy stockpiling causes transgranular to intergranular fracture transition

Yu Ding, Haiyang Yu, Meichao Lin, Kai Zhao, Senbo Xiao, Alexey Vinogradov, Lijie Qiao, Michael Ortiz, Jianying He, Zhiliang Zhang

Acta Materialia· Volume 239

Abstract

The attention to hydrogen embrittlement (HE) has been intensified recently in the light of hydrogen as a carbon-free energy carrier. Despite worldwide research, the multifaceted HE mechanism remains a matter of debate. Here we report an atomistic study of the coupled effect of hydrogen and deformation temperature on the pathway to intergranular fracture of nickel. Uniaxial straining is applied to nickel Σ5(210)[001] and Σ9(1-10)[22-1] grain boundaries with or without pre-charged hydrogen at various temperatures. Without hydrogen, vacancy generation at grain boundary is limited and transgranular fracture mode dominates. When charged, hydrogen as a booster can enhance strain-induced vacancy generation by up to ten times. This leads to the superabundant vacancy stockpiling at the grain boundary, which agglomerates and nucleates intergranular nanovoids eventually causing intergranular fracture. While hydrogen tends to persistently enhance vacancy concentration, temperature plays an intriguing dual role as either an enhancer or an inhibitor for vacancy stockpiling. These results show good agreement with recent positron annihilation spectroscopy experiments. An S-shaped quantitative correlation between the proportion of intergranular fracture and vacancy concentration was for the first time derived, highlighting the existence of a critical vacancy concentration, beyond which fracture mode will be completely intergranular.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (75)

Show source-provided references
1. On some remarkable changes produced in iron and steel by the action of hydrogen and acids10.1098/rspl.1874.0024 ↗
2. Gangloff · 2012
3. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
4. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation. I. Theoretical background10.1016/j.actamat.2007.05.047 ↗
5. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
6. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
7. A mechanistic theory of hydrogen embrittlement of steels10.1002/bbpc.19720760864 ↗
8. A quantum-mechanically informed continuum model of hydrogen embrittlement10.1016/j.jmps.2004.02.010 ↗
9. Atomic mechanism and prediction of hydrogen embrittlement in iron10.1038/nmat3479 ↗
10. A decohesion pathway for hydrogen embrittlement in nickel: mechanism and quantitative prediction10.1016/j.actamat.2019.11.062 ↗
11. A predictive model unifying hydrogen enhanced plasticity and decohesion10.1016/j.scriptamat.2022.114707 ↗
12. Hydrogen-enhanced fatigue crack growth in a single-edge notched tensile specimen under in-situ hydrogen charging inside an environmental scanning electron microscope10.1016/j.actamat.2019.03.032 ↗
13. Strain localisation and failure at twin-boundary complexions in nickel-based superalloys
14. Hydrogen-enhanced localized plasticity - a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
15. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
16. Mechanisms of hydrogen-enhanced localized plasticity: an atomistic study using alpha-Fe as a model system10.1016/j.actamat.2014.01.008 ↗
17. Hydrogenated vacancies lock dislocations in aluminium10.1038/ncomms13341 ↗
18. Effect of electrochemical charging on the hydrogen embrittlement susceptibility of alloy 71810.1016/j.actamat.2019.08.020 ↗
19. Hydrogen-induced transgranular to intergranular fracture transition in bi-crystalline nickel10.1016/j.scriptamat.2021.114122 ↗
20. Effect of hydrogen environment on the separation of Fe grain boundaries10.1016/j.actamat.2016.01.067 ↗
21. Atomistic study of hydrogen embrittlement of grain boundaries in nickel: I. Fracture10.1016/j.jmps.2017.01.020 ↗
22. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
23. Formation of superabundant vacancies in M–H alloys and some of its consequences: a review10.1016/S0925-8388(02)01269-0 ↗
24. Hydrogen related failure of steels - a new aspect10.1179/026708304225019687 ↗
25. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: overview10.1016/j.actamat.2018.12.013 ↗
26. The interaction of dislocations and hydrogen-vacancy complexes and its importance for deformation-induced proto nano-voids formation in alpha-Fe10.1016/j.ijplas.2015.05.017 ↗
27. Study on interactions of an edge dislocation with vacancy-H complex by atomistic modelling10.1016/j.ijplas.2017.03.003 ↗
28. Effects of grain size and deformation temperature on hydrogen-enhanced vacancy formation in Ni alloys10.1016/j.actamat.2017.02.016 ↗
29. Elucidating the contribution of mobile hydrogen-deformation interactions to hydrogen-induced intergranular cracking in polycrystalline nickel10.1016/j.actamat.2018.07.043 ↗
30. Criteria for hydrogen-assisted crack initiation in Ni-based superalloy 71810.1016/j.actamat.2022.117789 ↗
31. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
32. Hydrogen trapping and embrittlement in high-strength Al alloys10.1038/s41586-021-04343-z ↗
33. Hydrogen embrittlement controlled by reaction of dislocation with grain boundary in alpha-iron10.1016/j.ijplas.2018.08.013 ↗
34. The role of atomistic simulations in probing hydrogen effects on plasticity and embrittlement in metals10.1016/j.engfracmech.2019.106502 ↗
35. Hydrogen embrittlement in metallic nanowires10.1038/s41467-019-10035-0 ↗
36. First-principles calculations of hydrogen solution and diffusion in tungsten: temperature and defect-trapping effects10.1016/j.actamat.2014.10.039 ↗
37. Hydrogen bubble nucleation in α-iron10.1016/j.scriptamat.2017.03.006 ↗
38. Predictive model of hydrogen trapping and bubbling in nanovoids in bcc metals10.1038/s41563-019-0422-4 ↗
39. Atomistic study of hydrogen distribution and diffusion around a {1 1 2}< 1 1 1>edge dislocation in alpha iron10.1016/j.actamat.2008.04.011 ↗
40. Hydrogen-enhanced local plasticity at dilute bulk H concentrations: the role of H–H interactions and the formation of local hydrides10.1016/j.actamat.2011.01.037 ↗
41. The key role played by dislocation core radius and energy in hydrogen interaction with dislocations10.1016/j.actamat.2019.12.033 ↗
42. Atomistic studies of hydrogen effects on grain boundary structure and deformation response in FCC Ni10.1016/j.commatsci.2016.05.014 ↗
43. Atomistic investigation of the role of grain boundary structure on hydrogen segregation and embrittlement in alpha-Fe10.1007/s11661-012-1430-z ↗
44. Atomistic investigation of hydrogen induced decohesion of Ni grain boundaries10.1016/j.mechmat.2020.103586 ↗
45. Atomistic simulations of hydrogen embrittlement10.1016/j.ijhydene.2009.09.052 ↗
46. Mechanisms of hydrogen-enhanced localized plasticity: an atomistic study using α-Fe as a model system10.1016/j.actamat.2014.01.008 ↗
47. Atomistic study of hydrogen embrittlement of grain boundaries in nickel: II. Decohesion, modelling and simulation in
48. Trapping of hydrogen to lattice-defects in nickel10.1088/0965-0393/3/3/001 ↗
49. Rapid estimation of elastic constants by molecular dynamics simulation under constant stress10.1103/PhysRevB.69.134103 ↗
50. Hydrogen effects on nanovoid nucleation in face-centered cubic single-crystals10.1016/j.actamat.2007.09.012 ↗
51. Origin of micrometer-scale dislocation motion during hydrogen desorption10.1126/sciadv.aaz1187 ↗
52. Fast parallel algorithms for short-range molecular-dynamics10.1006/jcph.1995.1039 ↗
53. Grand canonical ensemble monte-carlo for a lennard-jones fluid10.1080/00268977500100221 ↗
54. General formulation of pressure and stress tensor for arbitrary many-body interaction potentials under periodic boundary conditions10.1063/1.3245303 ↗
55. Dislocation nucleation and defect structure during surface indentation10.1103/PhysRevB.58.11085 ↗
56. Softening of nanocrystalline metals at very small grain sizes10.1038/35328 ↗
57. Visualization and analysis of atomistic simulation data with OVITO–the open visualization tool10.1088/0965-0393/18/1/015012 ↗
58. First-principles investigation of hydrogen trapping and diffusion at grain boundaries in nickel10.1016/j.actamat.2015.07.031 ↗
59. Amorphization associated with crack propagation in hydrogen-charged steel10.1016/S1359-6462(03)00469-X ↗
60. Amorphization under fracture surface in hydrogen-charged and low-temperature tensile-tested austenitic stainless steel10.1080/09500839.2020.1841915 ↗
61. Hydrogen induced amorphization of LaMgNi4 phase in metal hydride alloys10.1016/j.ijhydene.2015.05.017 ↗
62. Hydrogen induced amorphization behaviors of multiphase La0. 8Mg0. 2Ni3. 5 alloy10.1016/j.ijhydene.2015.02.047 ↗
63. Hydrogen embrittlement of ferritic steels: Observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
64. Thermodynamic model for solid-state amorphization in binary systems at interfaces and grain boundaries10.1103/PhysRevB.54.9109 ↗
65. Disclinations, amorphization and microcrack generation at grain boundary junctions in polycrystalline solids10.1080/01418619408242248 ↗
66. Hydrogen induced vacancy clustering and void formation mechanisms at grain boundaries in palladium10.1016/j.actamat.2020.06.007 ↗
67. Stability of vacancy-hydrogen clusters in nickel from first-principles calculations10.1016/j.actamat.2014.06.021 ↗
68. Hydrogen diffusion and vacancies formation in tungsten: density functional theory calculations and statistical models10.1016/j.actamat.2015.04.052 ↗
69. Grain size and grain-boundary effects on diffusion and trapping of hydrogen in pure nickel10.1016/j.actamat.2012.09.004 ↗
70. Temperature dependence of grain boundary excess free volume10.1016/j.scriptamat.2019.10.046 ↗
71. Formation and time dynamics of hydrogen-induced vacancies in nickel10.1016/j.actamat.2021.117264 ↗
72. Quantities and distribution of strain-induced vacancies and dislocations enhanced by hydrogen in iron10.1016/j.actamat.2021.116663 ↗
73. An investigation of micro-mechanisms in hydrogen induced cracking in nickel-based superalloy 71810.1016/j.jallcom.2016.01.033 ↗
74. The effect of hydrogen on the fracture of alloy X-75010.1007/BF02647750 ↗
75. Cracking process in delayed fracture of high-strength steel after long atmospheric exposure10.2355/isijinternational.ISIJINT-2021-238 ↗